Abstract AITranslate
Surface oxidation is a major defect of drawn tungsten wire.Based on a comprehensive analysis of the formation rules and mechanisms of the surface oxidation of tungsten wire, this paper builds structural models and quality evaluation indexes of the tungsten wire surface layer, and correspondingly proposes improvement measures.The surface oxidation morphology of tungsten wire can be mainly divided into two types: surface grooves and graphite emulsion layer shedding, which are formed as a result of the non-uniformity and non-integrity of the surface carbon layer.To improve the surface quality of the tungsten wire, the key is to form a uniform and integral carbon layer and increase the effective carbon content of the surface layer.By controlling the granularity and viscosity of the graphite emulsion and setting the reasonable pass compression ratio, coating layers of the graphite emulsion, processing temperature and other processing parameters, it can effectively prevent the damage of the lubricating layer, build an ideal surface layer for the tungsten wire, and thus improve its surface quality.
KeyWords AITranslate
1董金翔.钽丝表面沟槽产生和修复机理[J].稀有金属与硬质合金,1992,20(4):11-13. 被引量:3
2涂启建.拉拔钼丝表面微缺陷的形成及控制[J].中国钼业,2020,44(3):49-52. 被引量:1
3刘文辉.粗钨丝拉丝石墨乳的运用研究和选用[J].山东工业技术,2018(17):19-19. 被引量:2
4李渝.钨钼丝拉拔润滑机理:第Ⅱ部分:表面条件对润滑和润滑膜形成的影响[J].钨钼材料,1993(1):88-93. 被引量:1
1叶铭海,李世明,方毅金.逆氢蓝钨工艺对掺杂钨丝高温性能的影响[J].中国钨业,2023,38(1):51-57.
1杨培元,霍庆辉,陈卓,周伟,汪宏斌.露点对DP590双相钢表面氧化行为的影响[J].金属热处理,2021,46(11):97-102. 被引量:1
2雷杰华,陈西玲,方庆明.MRI可量化指标诊断肩峰下撞击综合征患者肩功能和临床症状的价值[J].深圳中西医结合杂志,2022,32(16):41-44.
3徐丽云.宋代赣州文化繁盛的现代价值研究[J].文化产业,2022(33):76-78.
4徐正林,刘克勤.追而不迷:地方本科院校转型发展中对大学排行榜的态度初探[J].丽水学院学报,2022,44(6):66-73.
5黄来源.基于流域形态特征分析的北京北山泥石流易发性评价因子研究[J].城市地质,2022,17(4):385-393. 被引量:2
6朱曦,王丽娟,王晓理,蒋婧.双层中空玻璃隔声性能仿真研究[J].噪声与振动控制,2022,42(6):256-262.
7周芃,李可然,胡飞,时天骄,龚攀.添加Be对CoCrFeNi高熵合金组织和性能影响的研究[J].精密成形工程,2022,14(12):41-49.
8袁小蝶,赵霞,林园,苏朝晖.左氧氟沙星负载的小尺寸聚多巴胺纳米粒子用于光热/抗生素联合细菌治疗[J].分析化学,2022,50(12):1889-1898.
9陈伟龙,郭榕榕,仝钰申,刘莉莉,周圣岚,林金海.亚禁带光照对CdZnTe晶体中晶界电场分布的影响[J].物理学报,2022,71(22):212-219.
10闫超群(译).一种多H键扩链聚氨酯制备的高韧性、热熔粘合、3D打印手指矫形器[J].聚合物与助剂,2022(5):14-23.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]
Citation Information:
Surface oxidation is a major defect of drawn tungsten wire.Based on a comprehensive analysis of the formation rules and mechanisms of the surface oxidation of tungsten wire, this paper builds structural models and quality evaluation indexes of the tungsten wire surface layer, and correspondingly proposes improvement measures.The surface oxidation morphology of tungsten wire can be mainly divided into two types: surface grooves and graphite emulsion layer shedding, which are formed as a result of the non-uniformity and non-integrity of the surface carbon layer.To improve the surface quality of the tungsten wire, the key is to form a uniform and integral carbon layer and increase the effective carbon content of the surface layer.By controlling the granularity and viscosity of the graphite emulsion and setting the reasonable pass compression ratio, coating layers of the graphite emulsion, processing temperature and other processing parameters, it can effectively prevent the damage of the lubricating layer, build an ideal surface layer for the tungsten wire, and thus improve its surface quality.
quote
| GB/T 7714-2015 | [1] HUANG Can-xin. Research on Oxidation Behavior of Tungsten Wire Surface and Improvement Measures[J]. Rare Metals and Cemented Carbides, 2022(5): 40-46. |
| MLA | [1] HUANG Can-xin. "Research on Oxidation Behavior of Tungsten Wire Surface and Improvement Measures." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 40-46. |
| APA | [1] HUANG Can-xin. (2022). Research on Oxidation Behavior of Tungsten Wire Surface and Improvement Measures. Rare Metals and Cemented Carbides(5), 40-46. |
| IEEE | [1] HUANG Can-xin, "Research on Oxidation Behavior of Tungsten Wire Surface and Improvement Measures," Rare Metals and Cemented Carbides, no. 5, pp. 40-46, 2022. keywords: {tungsten wire;surface oxidation;surface groove;graphite emulsion;lubricating layer;quantifiable indicator;improvement measure} |