Study on the Anti-Na Poisoning Performance of Nb Modified V-Mo/Ti Denitration Catalyst AITranslate
Abstract AITranslate
V-Mo/Ti and V-Mo-Nb/Ti denitration catalysts were prepared,and the denitration activity and resistance to Na poisoning of the two catalysts were investigated and compared.XRD,BET,NH3-TPD,H2-TPR and XPS were used to characterize the catalysts.The results show that the addition of Nb can effectively inhibit the decrease in acidity and reducibility of the catalyst caused by Na poisoning,and the decrease of chemisorbed oxygen on surface of the Na-poisoned catalyst.Thus,V-Mo-Nb/Ti-Na catalyst exhibits better denitration activity than V-Mo/Ti-Na catalyst.
KeyWords AITranslate
1朱崇兵,金保升,仲兆平,李锋,翟俊霞.WO3对于V2O5/TiO2脱硝催化剂的抗中毒作用[J].锅炉技术,2009,40(1):63-67. 被引量:16
2曹俊,姚小江,杨复沫,陈丽,傅敏,汤常金,董林.Ce^(4+),Zr^(4+)共掺杂提高V_2O_5-WO_3/TiO_2催化剂脱硝性能及抗K中毒能力(英文)[J].催化学报(英文),2019,40(1):95-104. 被引量:11
3何杰,范以宁,邱金恒,陈懿.Nb_2O_5/TiO_2催化剂表面铌氧物种的分散状态和催化性能[J].化学学报,2004,62(14):1311-1317. 被引量:20
4贾勇,周军,柏家串,李睦,王烨,钟秦.砷、钾复合中毒选择性催化还原脱硝催化剂的再生[J].硅酸盐学报,2016,44(7):1025-1032. 被引量:11
5陈昶名,吴晓东,尉文超,高宇曦,翁端,石磊,耿春雷.氧化钛负载脱硝催化剂的碱中毒过程:氧化钒的保留和氧化钨的牺牲(英文)[J].催化学报(英文),2015,36(8):1287-1294. 被引量:6
6晁晶迪,何洪,宋丽云,房玉娇,梁全明,张桂臻,邱文革,张然.Pr掺杂对V2O5-MoO3/TiO2催化剂NH3-SCR反应活性的影响[J].高等学校化学学报,2015,36(3):523-530. 被引量:30
7冯静,张明森,罗国庆.铌对V_2O_5/TiO_2催化剂性能的影响[J].石油化工,2001,30(9):665-668. 被引量:10
8贾勇,柏家串,李睦,周军,王烨,钟秦.乙二酸再生钾中毒催化剂V_2O_5-WO_3/TiO_2的实验研究[J].中国电机工程学报,2016,36(4):1009-1015. 被引量:5
9沈伯雄,熊丽仙,刘亭,王静,田晓娟.纳米负载型V_2O_5-WO_3/TiO_2催化剂碱中毒及再生研究[J].燃料化学学报,2010,38(1):85-90. 被引量:52
1常峥峰,黄力,姚晔,王虎,纵宇浩,高义博,于洋.钕铌共掺杂对V-Mo/Ti脱硝催化剂性能的影响[J].有色金属工程,2022,12(6):144-150. 被引量:1
2赵晋涛,张晓凯,吕瑞亮.谈脱硝技术在燃煤锅炉烟气处理中的应用现状[J].区域供热,2022(4):73-80. 被引量:1
3兰馨,赵玲.SCR催化剂抗碱(土)金属中毒及再生研究进展[J].环境化学,2022,41(11):3778-3788. 被引量:1
1陈璐,张文之,侯雨薇,沈庆峰,李永刚,俞小花.SiO_(2)模板法制备LaMnO_(3)及其催化性能[J].有色金属工程,2023,13(4):7-12.
2黄纪荣,仲超.燃煤锅炉烟气脱硝技术研究[J].清洗世界,2023,39(4):4-6.
3何川,吴国勋,李昂,张发捷,卞子君,卢承政,王丽朋,赵民.垃圾焚烧脱硝催化剂钙镁失活与活性恢复特性[J].化工进展,2023,42(5):2413-2420.
1李柯志,罗河,赵冉,韩帅,任靖,张新军,孟凡立.具焙烧服役史钛白粉对新制脱硝催化剂活性影响机制研究[J].分子催化,2020,34(5):415-424. 被引量:9
2李丹,王慧,陈留平,朱娜.一种无定形有序的Ce⁃Ti催化膜用于同时去除粉尘和氮氧化物[J].无机化学学报,2020,36(11):2189-2196.
3王川,李新宇,于涛.离线淬火工艺对NM400耐磨钢组织与性能的影响[J].山东冶金,2020,42(4):43-45. 被引量:3
4宋唯一,朱宝忠,孙运兰,谢超越.煅烧气氛对柠檬酸溶胶凝胶铁氧化物催化剂低温SCR脱硝性能的影响[J].洁净煤技术,2020,26(5):56-63.
5赵重阳,李国波,眭华军,刘初明,王玲,张亚平.砷中毒商业V2O5-WO3/TiO2催化剂再生研究[J].分子催化,2020,34(5):407-414. 被引量:2
6李娜,张胜寒,李华,王晶晶,张凯,武文斐.水热法合成氟碳铈矿的反应条件和脱硝性能研究[J].稀有金属与硬质合金,2020,48(5):48-54. 被引量:1
7廖广,何立模,胡松,陈小芳,任强强,向军.镍基催化甲苯分解过程中无定形碳与石墨型碳生成及转化特性[J].太阳能学报,2020,41(10):347-354.
8刘双,卜龙利,宁珂,张婷婷,刘嘉栋.整体式分子筛基催化剂制备及其微波催化燃烧VOCs[J].中国环境科学,2020,40(11):4688-4696. 被引量:7
9王馨瑶,徐禄禄,张维萍.四丙基氢氧化铵改性Mo/HZSM-5催化甲烷甲醇共芳构化反应性能[J].分子催化,2020,34(5):425-435. 被引量:4
10孙厚祥,张化冰.Sn和Si掺杂AlPO4-5分子筛及其加氢脱硫反应性能研究[J].分子催化,2020,34(5):446-453. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:O643.362[理学—物理化学]
Citation Information:
V-Mo/Ti and V-Mo-Nb/Ti denitration catalysts were prepared,and the denitration activity and resistance to Na poisoning of the two catalysts were investigated and compared.XRD,BET,NH3-TPD,H2-TPR and XPS were used to characterize the catalysts.The results show that the addition of Nb can effectively inhibit the decrease in acidity and reducibility of the catalyst caused by Na poisoning,and the decrease of chemisorbed oxygen on surface of the Na-poisoned catalyst.Thus,V-Mo-Nb/Ti-Na catalyst exhibits better denitration activity than V-Mo/Ti-Na catalyst.
quote
| GB/T 7714-2015 | [1] HUANG Li, WANG Hu, ZONG Yu-hao, et al. Study on the Anti-Na Poisoning Performance of Nb Modified V-Mo/Ti Denitration Catalyst[J]. Rare Metals and Cemented Carbides, 2020(5): 34-37. |
| MLA | [1] HUANG Li, et al., "Study on the Anti-Na Poisoning Performance of Nb Modified V-Mo/Ti Denitration Catalyst." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 34-37. |
| APA | [1] HUANG Li, WANG Hu, ZONG Yu-hao, HAN Pei, & CHANG Zheng-feng. (2020). Study on the Anti-Na Poisoning Performance of Nb Modified V-Mo/Ti Denitration Catalyst. Rare Metals and Cemented Carbides(5), 34-37. |
| IEEE | [1] HUANG Li, WANG Hu, ZONG Yu-hao, HAN Pei, and CHANG Zheng-feng, "Study on the Anti-Na Poisoning Performance of Nb Modified V-Mo/Ti Denitration Catalyst," Rare Metals and Cemented Carbides, no. 5, pp. 34-37, 2020. keywords: {V-Mo/Ti catalyst;modification with niobium;denitration;Na poisoning} |