A Thermoset Shape Memory Polymer-Based Syntactic Foam with Flame Retardancy and 3D Printability AITranslate

Southern University and A&M College; Louisiana State University; Louisiana State University; Southern University and A&M College; Southern University and A&M College; Louisiana State University; Louisiana State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Here we report a thermoset shape memory polymer-based syntactic foam inherently integrated with flame retardancy, good mechanical properties, excellent shape memory effect, and 3D printability. The syntactic foam is fabricated by incorporating a high-temperature shape memory polymer (HTSMP) as the matrix, with 40 vol % hollow glass microspheres (HGM) K20, K15, and K1 as fillers. Compressive behavior, strain-controlled programming followed by free recovery, stress recovery, and flame retardancy of these three syntactic foams were studied. Dynamic mechanical analysis and thermal characterization validate their high glass transition temperature (Tg = ∼250 °C) and excellent thermal stability. Our results suggest that the foam consisting of K20 HGM exhibits high compressive strength (81.8 MPa), high recovery stress (6.8 MPa), and excellent flame retardancy. Furthermore, this syntactic foam was used for three-dimensional (3D) printing by an extruder developed in our lab. Honeycomb, sinusoidal shapes, and free-standing helical spring were printed for demonstration. This high-temperature photopolymer-based syntactic foam integrated with high Tg, flame retardancy, high recovery stress, and 3D printability can be beneficial in different sectors such as aerospace, construction, oil and gas, automotive, and electronic industries.

KeyWords AITranslate

shape memory polymer syntactic foam flame retardancy stress recovery 3D printing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01596

Chinese Library Classification Number:

Citation Information:

Here we report a thermoset shape memory polymer-based syntactic foam inherently integrated with flame retardancy, good mechanical properties, excellent shape memory effect, and 3D printability. The syntactic foam is fabricated by incorporating a high-temperature shape memory polymer (HTSMP) as the matrix, with 40 vol % hollow glass microspheres (HGM) K20, K15, and K1 as fillers. Compressive behavior, strain-controlled programming followed by free recovery, stress recovery, and flame retardancy of these three syntactic foams were studied. Dynamic mechanical analysis and thermal characterization validate their high glass transition temperature (Tg = ∼250 °C) and excellent thermal stability. Our results suggest that the foam consisting of K20 HGM exhibits high compressive strength (81.8 MPa), high recovery stress (6.8 MPa), and excellent flame retardancy. Furthermore, this syntactic foam was used for three-dimensional (3D) printing by an extruder developed in our lab. Honeycomb, sinusoidal shapes, and free-standing helical spring were printed for demonstration. This high-temperature photopolymer-based syntactic foam integrated with high Tg, flame retardancy, high recovery stress, and 3D printability can be beneficial in different sectors such as aerospace, construction, oil and gas, automotive, and electronic industries.

quote

GB/T 7714-2015 [1] Rubaiyet Abedin, Xiaming Feng, John Pojman, Jr., et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01596.
MLA [1] Rubaiyet Abedin, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01596.
APA [1] Rubaiyet Abedin, Xiaming Feng, John Pojman, Jr., Samuel Ibekwe, Patrick Mensah, Isiah Warner, & Guoqiang Li. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01596
IEEE [1] Rubaiyet Abedin, Xiaming Feng, John Pojman, Jr., Samuel Ibekwe, Patrick Mensah, Isiah Warner, and Guoqiang Li, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01596. keywords: {shape memory polymer;syntactic foam;flame retardancy;stress recovery;3D printing}