Preparation and Characterization of Low-temperature La/Ce Doped Manganese-based Denitration Catalyst AITranslate
Abstract AITranslate
Low-temperature La/Ce doped Mn-based denitration catalyst powders were prepared by copre-cipitation.The sulfur resistance of the catalyst powders was improved by SO42- acidification treatment.ICP,FT-IR,XRD,SEM,BET and denitration activity test were used to characterize the catalyst.The results show that when calcination temperature is 500 ℃ and 0.2 mol/L H2SO4 is employed for acidification treatment, the prepared La1-Ce6-Mn/Ti catalyst powder has the largest Mn/Ti mass ratio and the most active sites with specific surface area of 105.34 m2/g and denitration efficiency of 84% at 200 ℃.
KeyWords AITranslate
1李歌,王宝冬,马静,周佳丽,李永龙,徐文强,韩一帆,孙琦.低温锰基分子筛脱硝催化剂的研究进展[J].环境化学,2018,37(4):769-781. 被引量:5
2李威.金属氧化物低温NH3-SCR催化剂的抗水抗硫性能[J].化工管理,2020(22):96-97. 被引量:1
3黄金,仲兆平,朱林,薛建明,许月阳,吴培亭.锰铈改性钒钨钛中低温SCR催化剂脱硝及抗水抗硫性能[J].化工进展,2018,37(6):2242-2248. 被引量:11
4王金玉,朱怀志,安泽文,巩建,王翠苹.Mn基脱硝催化剂抗水抗硫改性的模拟与实验研究[J].化工学报,2019,70(12):4635-4644. 被引量:5
5张呈祥,张晓鹏.Mn-Ce系列低温SCR催化剂抗硫性研究进展[J].化工进展,2015,34(7):1866-1871. 被引量:8
6杨波,沈岳松,祝社民,曾燕伟,沈树宝.Mn-La-Ce-Ni-O_x低温脱硝的影响因素[J].南京工业大学学报:自然科学版,2015,37(5):6-11. 被引量:3
7肖海平,豆朝宗,袁宗海,李建,葛金林,吕洪坤.含硫钾盐对V2O5-WO3/TiO2催化剂上SO3生成特性的影响[J].动力工程学报,2020,40(2):145-151. 被引量:2
8许振冲,吴爽,周明东,刘静敏.过渡金属Ag、Co、Ni、Cu在CeAlO催化剂载体上的脱硝活性研究[J].稀有金属与硬质合金,2015,43(6):46-51. 被引量:1
9许振冲,吴爽.In/Al_2O_3催化剂低温脱硝性能研究[J].稀有金属与硬质合金,2016,44(4):48-52. 被引量:1
1黄力,王虎,纵宇浩,常峥峰,高义博,李金珂,于洋.P对V-Mo/Ti脱硝催化剂的性能影响研究[J].钢铁钒钛,2022,43(1):67-73.
2王莹,赵然,张凯,武文斐.独居石负载钼氧化物催化材料制备及其NH3-SCR脱硝性能研究[J].稀有金属与硬质合金,2023,51(1):40-46.
1张艳,张浩宇,杨诗雨.铬含量变化对铬锰钢耐腐蚀性能的影响[J].腐蚀与防护,2021,42(5):34-37. 被引量:1
2张延兵,李晓环,刘巧巧,周璇,李梦,陈英赞.Mn-FeO_(x)/PDOPA@CNTs催化剂的原位制备及低温脱硝性能[J].化学工程,2021,49(2):18-23. 被引量:1
3常峥峰,高义博,黄力,王虎,纵宇浩,刘洋,李金珂.海泡石纤维在平板式脱硝催化剂中的应用[J].工业催化,2021,29(5):38-42.
4赵岩.探析固体废物的综合利用[J].区域治理,2021(5):0182-0183.
5郭梓阳,霍旺晨,张育新,任山,杨剑.锰基低温NH 3-SCR脱硝催化剂的研究概述[J].材料导报,2021,35(13):13085-13099. 被引量:9
6杨思娴,钟文钰,李超贤,苏秋瑶,许炳佳,何谷平,孙丰强.聚苯胺纳米线/SnO2复合光催化材料的光化学制备与性能[J].高等学校化学学报,2021,42(6):1942-1951. 被引量:3
7袁亚梅,陈慧,赵丹阳,吴驰,耿皎,沈俭一.新型磷化钴和硫化钴催化剂的制备及其在加氢精制反应中的活性[J].南京大学学报:自然科学版,2021,57(3):512-524.
8欧毓迎,陆正华.高频变压器引脚的腐蚀原因[J].腐蚀与防护,2021,42(5):78-81.
9马赟赟.马铃薯中生物碱的电化学性能的研究[J].甘肃科技,2021,37(10):36-39.
10杨军伟,孙林,熊培祺,杨淼.酸化在酸敏性砂岩储层中的可行性分析[J].辽宁化工,2021,50(5):738-740. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TQ426.83[化学工程]
Citation Information:
Low-temperature La/Ce doped Mn-based denitration catalyst powders were prepared by copre-cipitation.The sulfur resistance of the catalyst powders was improved by SO42- acidification treatment.ICP,FT-IR,XRD,SEM,BET and denitration activity test were used to characterize the catalyst.The results show that when calcination temperature is 500 ℃ and 0.2 mol/L H2SO4 is employed for acidification treatment, the prepared La1-Ce6-Mn/Ti catalyst powder has the largest Mn/Ti mass ratio and the most active sites with specific surface area of 105.34 m2/g and denitration efficiency of 84% at 200 ℃.
quote
| GB/T 7714-2015 | [1] YANG Jie, LI Xia, DU Hong-wei, et al. Preparation and Characterization of Low-temperature La/Ce Doped Manganese-based Denitration Catalyst[J]. Rare Metals and Cemented Carbides, 2021(3): 41-45. |
| MLA | [1] YANG Jie, et al., "Preparation and Characterization of Low-temperature La/Ce Doped Manganese-based Denitration Catalyst." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 41-45. |
| APA | [1] YANG Jie, LI Xia, DU Hong-wei, & LIU Zhao-gang. (2021). Preparation and Characterization of Low-temperature La/Ce Doped Manganese-based Denitration Catalyst. Rare Metals and Cemented Carbides(3), 41-45. |
| IEEE | [1] YANG Jie, LI Xia, DU Hong-wei, and LIU Zhao-gang, "Preparation and Characterization of Low-temperature La/Ce Doped Manganese-based Denitration Catalyst," Rare Metals and Cemented Carbides, no. 3, pp. 41-45, 2021. keywords: {low-temperature manganese-based catalyst;denitration activity;coprecipitation;sulfur resis-tance;sulfuric acid acidification} |