Study of Recovery of Value Metals from Waelz Clinker by Physical Separation AITranslate

Zhuzhou Metallurgical Group Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

It is very difficult to recycle and reuse Waelz clinker because of its fine particle size,high residual coke breeze,large hardness and complex compositions of low content of value metals. Based on the differences in magnetism and specific gravity between iron rich part and carbon rich part, some processes have been developed to separate part of coke breeze by hydraulic washing, to separate iron rich part from coke breeze by crushing-magnetic separation, to produce iron powder by ball milling-magnetic separation, and to produce silver-iron ore by gravity separation for the recovery of Ag, Cu and In from clinker by physical separation and for'proper comprehensive reuse of Waelz waste clinker in Zn hydrometallurgical industry.

KeyWords AITranslate

comprehensive recovery Waelz clinker magnetic separation gravity separation

1李昌福.凡口窑渣冶炼工艺试验研究[J].矿冶,2002,11(3):56-59. 被引量:9

2吴克立.鼓风炉炼铅加入铁屑的作用及合理用量[J].有色金属:冶炼部分,1992(3):13-14. 被引量:1

3Tomita Masatoshi.Treatment of Dust[P].JP Pat:59170225,1984-09-26.

4Schriefer John.Reaping the value from dust and slag[J].Iron Age New Steel,1997,13(2):24.

5王伟光.锌渣综合利用的研究与应用[J].矿冶,1996,5(1):74-80. 被引量:8

6赵平.从炼锌渣中回收有价元素[J].矿产保护与利用,2000,20(5):47-49. 被引量:9

1李静,牛皓,彭金辉,张世敏,张利波,魏昶,范兴祥,黄孟阳.锌窑渣综合回收利用研究现状及展望[J].矿产综合利用,2008(6):44-48. 被引量:23

2马娇,焦红光,潘兰英,张传祥,张宏方.干法磁选在锌挥发窑窑渣综合利用中的应用研究[J].河南理工大学学报:自然科学版,2009,28(6):788-791. 被引量:5

3王纪明,彭兵,柴立元,李密,彭宁.锌浸渣还原焙烧-磁选回收铁[J].中国有色金属学报,2012,22(5):1455-1461. 被引量:26

4何仕超,刘志宏,刘智勇,李玉虎,李启厚.湿法炼锌窑渣铁精矿的浸出热力学分析[J].中国有色金属学报,2013,23(12):3430-3439. 被引量:7

5王立丽,李正要,林蜀勇,曹君磊,邓文翔.某锌挥发窑渣银回收试验[J].现代矿业,2015,0(2):54-57. 被引量:8

6彭兵,李燕春,柴立元,刘恢,闵小波,胡明,袁莹珍,雷杰,彭宁.锌浸渣硫酸铵焙烧-选择性浸出回收锌[J].中国有色金属学报,2015,25(9):2596-2603. 被引量:10

7丁喻,陈文如,沈裕军,刘黄,郑铁铮,蔡云卓.高磷碳酸锰矿与锌窑渣集约冶炼实验研究[J].中国锰业,2016,34(3):72-77. 被引量:1

8徐华军.高炉瓦斯灰火法富集回收锌处理工艺[J].有色冶金节能,2019,35(1):27-28. 被引量:3

9李硕,邵延海,何浩,张谦,吴海祥,杨森,常军,蒋丰祥.锌窑渣中有价金属综合回收研究现状及展望[J].矿产保护与利用,2019,39(1):138-143. 被引量:5

10孟昕阳,李宇.提锌二次尾渣制备微晶玻璃的工艺优化[J].有色金属科学与工程,2020,11(2):27-33. 被引量:3

1杨大锦.2008年云南冶金年评[J].云南冶金,2009,38(2):36-53.

2王福生,车欣.浸锌渣综合利用现状及发展趋势[J].天津化工,2010,24(3):1-3. 被引量:21

3丁倩倩,吴克明,袁芳沁,王磊,柯兴.高温挥发法从沉铁渣中回收锌的试验研究[J].湿法冶金,2011,30(3):234-236. 被引量:9

4戴兴征,曾鹏,任锐,黄孟阳,王晓连.锌窑渣氧化气固相反应过程分析[J].四川冶金,2011,33(4):36-39. 被引量:1

5杨建军,李永祥,任锐,黄孟阳,苟军军.锌窑渣受热行为特性研究[J].有色金属工程,2011,1(5):45-47. 被引量:1

6肖军辉,冯启明,樊珊萍,徐龙华,王振.玻利维亚铜、钨、锡多金属尾矿的综合利用[J].中国有色金属学报,2013,23(10):2949-2961. 被引量:4

7何仕超,刘志宏,刘智勇,李玉虎,李启厚.湿法炼锌窑渣铁精矿的浸出热力学分析[J].中国有色金属学报,2013,23(12):3430-3439. 被引量:7

8卢宇飞,熊国焕,何艳明.锌冶炼浸出渣资源化利用技术分析[J].云南冶金,2014,43(1):93-96. 被引量:8

9刘群,谭军,陈启元,廖舟,张平民,尹周澜.沉铁渣回收利用中的脱硫试验研究[J].有色金属:冶炼部分,2014(2):1-4. 被引量:4

10韩俊伟,刘维,覃文庆,柴立元,郑永兴,杨康.高铁锌焙砂选择性还原焙烧-两段浸出锌[J].中国有色金属学报,2014,24(2):511-518. 被引量:19

1郝春霞,赵玉柱,吴振宇.生活垃圾中废塑料分选回收技术概述[J].环境与发展,2013,25(11):27-29. 被引量:2

2张记市,苏存荣,谢刚.昆明城市生活垃圾处理研究[J].云南环境科学,2004,23(1):3-5. 被引量:6

3锌挥发窑烟气脱硫装置成功试车[J].现代材料动态,2012(9):19-20.

4王辉.湿法炼锌工业挥发窑窑渣资源化综合循环利用[J].中国有色冶金,2007,36(6):46-50. 被引量:9

5王广林.硫铁矿烧渣重选法生产铁精粉的全循环用水[J].化工矿业通讯,1997(1):9-9.

6锌挥发窑烟气脱碗装置成功试车[J].中国铅锌锡锑,2012(7):69-69.

7杨翠灵.东莞市生活垃圾处理现状及建议[J].广东地质,2013(1):155-158.

8程学丰,孙瑛.淮南市城市生活垃圾现状和处理对策探讨[J].安徽理工大学学报:自然科学版,2007,27(1):1-4. 被引量:3

9董安民.坚持因地制宜 综合利用废渣资源 大力发展和推广新型墙体材料[J].砖瓦,1999(3):6-7.

10黄威.磁选法有效处理城市生活垃圾[J].再生资源研究,2003(1):45-45.

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

It is very difficult to recycle and reuse Waelz clinker because of its fine particle size,high residual coke breeze,large hardness and complex compositions of low content of value metals. Based on the differences in magnetism and specific gravity between iron rich part and carbon rich part, some processes have been developed to separate part of coke breeze by hydraulic washing, to separate iron rich part from coke breeze by crushing-magnetic separation, to produce iron powder by ball milling-magnetic separation, and to produce silver-iron ore by gravity separation for the recovery of Ag, Cu and In from clinker by physical separation and for'proper comprehensive reuse of Waelz waste clinker in Zn hydrometallurgical industry.

quote

GB/T 7714-2015 [1] WANG Hui. Study of Recovery of Value Metals from Waelz Clinker by Physical Separation[J]. Rare Metals and Cemented Carbides, 2007(1): 31-35.
MLA [1] WANG Hui. "Study of Recovery of Value Metals from Waelz Clinker by Physical Separation." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 31-35.
APA [1] WANG Hui. (2007). Study of Recovery of Value Metals from Waelz Clinker by Physical Separation. Rare Metals and Cemented Carbides(1), 31-35.
IEEE [1] WANG Hui, "Study of Recovery of Value Metals from Waelz Clinker by Physical Separation," Rare Metals and Cemented Carbides, no. 1, pp. 31-35, 2007. keywords: {comprehensive recovery;Waelz clinker;magnetic separation;gravity separation}