Solar water evaporation is an environment-friendly and clean way of wastewater treatment and seawater desalination. However, a solar evaporator based on a hydrogel substrate still needs excellent toughness to ensure continuous and stable utilization while achieving a fast evaporation rate. In this research, a solar evaporator based on a dual network hydrogel was fabricated by double chemical cross-linking, consisting of polyacrylamide (PAAm), carboxymethyl cellulose (CMC), and CuS. By utilizing N,N′-methylenebisacrylamide (MBA) and Fe3+ for a double chemical cross-linking agent, PAAm and CMC (PAAm–CMC) formed an interpenetrating dual network structure, which is helpful to improve the mechanical properties of a photothermal membrane. The breaking elongation of a CuS/PAAm–CMC membrane is 480%. Meanwhile, the hydrophilic network ensured the high efficiency of water transmission and water activation. The evaporation rate reached 1.613 kg m–2 h–1 at 1 sun, and the photothermal conversion efficiency reached 79%. In the process of a simulated desalination experiment (10 wt % NaCl solution), the evaporation rate did not decrease after 10 cycles, indicating the self-cleaning ability and good durability of CuS/PAAm–CMC.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01422
Chinese Library Classification Number:
Citation Information:
Solar water evaporation is an environment-friendly and clean way of wastewater treatment and seawater desalination. However, a solar evaporator based on a hydrogel substrate still needs excellent toughness to ensure continuous and stable utilization while achieving a fast evaporation rate. In this research, a solar evaporator based on a dual network hydrogel was fabricated by double chemical cross-linking, consisting of polyacrylamide (PAAm), carboxymethyl cellulose (CMC), and CuS. By utilizing N,N′-methylenebisacrylamide (MBA) and Fe3+ for a double chemical cross-linking agent, PAAm and CMC (PAAm–CMC) formed an interpenetrating dual network structure, which is helpful to improve the mechanical properties of a photothermal membrane. The breaking elongation of a CuS/PAAm–CMC membrane is 480%. Meanwhile, the hydrophilic network ensured the high efficiency of water transmission and water activation. The evaporation rate reached 1.613 kg m–2 h–1 at 1 sun, and the photothermal conversion efficiency reached 79%. In the process of a simulated desalination experiment (10 wt % NaCl solution), the evaporation rate did not decrease after 10 cycles, indicating the self-cleaning ability and good durability of CuS/PAAm–CMC.
quote
| GB/T 7714-2015 | [1] Jun Chen, Dawei Wang, Xin Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01422. |
| MLA | [1] Jun Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01422. |
| APA | [1] Jun Chen, Dawei Wang, Xin Li, Hao Sun, Hanxiao Zhao, Ying Li, Xuefeng Liu, & Gang Shi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01422 |
| IEEE | [1] Jun Chen, Dawei Wang, Xin Li, Hao Sun, Hanxiao Zhao, Ying Li, Xuefeng Liu, and Gang Shi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01422. keywords: {CuS/PAAm−CMC membrane;dual chemical crosslinked network;heat transfer;solar water evaporation;desalination} |