daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Controllable Growth of High Quality MAPbX3 Perovskite Single Crystals for X-ray Detection Controllable Growth of High Quality MAPbX3 Perovskite Single Crystals for X-ray Detection AITranslate

Institute of Materials;Institute of Materials;Institute of Materials; Shandong University;Institute of Materials;Institute of Materials;Institute of Materials;Institute of Materials;Institute of Materials;Institute of Materials; Southwest University of Science & Technology;Institute of Materials
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The crystal quality limits the mobility-lifetime (μτ) product and the further applications of perovskite single crystals (PSC) in high energy radiation detections regardless of their high attenuation coefficient. In this paper, high-quality and controllable growth of MAPbX3 PSCs is demonstrated using the liquid-diffusion induced crystallization (LDSC) method. The growth kinetics are modeled to demonstrate the feasibility of the controllable growth via keeping the growth in the mass-transport-limited regime. The crystal growth rate is confirmed theoretically and experimentally to be constant and solely dependent on the growth temperature. A facile method is developed to measure the growth rate without disturbing or suspending the whole process. MAPbBr3 PSC grown at the optimal condition demonstrates a full-width at half-maximum of the (100) X-ray rocking curves of 0.0096°, a fluorescence lifetime of 1099 ns, a trap density of 4.5 × 109 cm–3, and a μτ product of 1.495 × 10–2 cm2 V–1. The resulting MAPbBr3 X-ray detector has a sensitivity of 2181 μC Gyair–1 cm–2. All results indicate that the controllable growth is beneficial to the crystal qualities and device performances. The concept proposed here will be inspiring for the community of researchers of perovskite materials.

KeyWords AITranslate

perovskite single crystals low trap density Xray detectors crystal growth kinetics growth rate measurement
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01424

Chinese Library Classification Number:

Citation Information:

The crystal quality limits the mobility-lifetime (μτ) product and the further applications of perovskite single crystals (PSC) in high energy radiation detections regardless of their high attenuation coefficient. In this paper, high-quality and controllable growth of MAPbX3 PSCs is demonstrated using the liquid-diffusion induced crystallization (LDSC) method. The growth kinetics are modeled to demonstrate the feasibility of the controllable growth via keeping the growth in the mass-transport-limited regime. The crystal growth rate is confirmed theoretically and experimentally to be constant and solely dependent on the growth temperature. A facile method is developed to measure the growth rate without disturbing or suspending the whole process. MAPbBr3 PSC grown at the optimal condition demonstrates a full-width at half-maximum of the (100) X-ray rocking curves of 0.0096°, a fluorescence lifetime of 1099 ns, a trap density of 4.5 × 109 cm–3, and a μτ product of 1.495 × 10–2 cm2 V–1. The resulting MAPbBr3 X-ray detector has a sensitivity of 2181 μC Gyair–1 cm–2. All results indicate that the controllable growth is beneficial to the crystal qualities and device performances. The concept proposed here will be inspiring for the community of researchers of perovskite materials.

quote

GB/T 7714-2015 [1] Ziming Zhang, Haibin Li, Haipeng Di, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01424.
MLA [1] Ziming Zhang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01424.
APA [1] Ziming Zhang, Haibin Li, Haipeng Di, Dong Liu, Wei Jiang, Jiwei Ren, Zhengfang Fan, Feiyi Liao, Lin Lei, Gaocai Li, Ying Xiong, & Yiying Zhao. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01424
IEEE [1] Ziming Zhang, Haibin Li, Haipeng Di, Dong Liu, Wei Jiang, Jiwei Ren, Zhengfang Fan, Feiyi Liao, Lin Lei, Gaocai Li, Ying Xiong, and Yiying Zhao, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01424. keywords: {perovskite single crystals low trap density Xray detectors crystal growth kinetics growth rate measurement}