Substituent Effects of Electron-Withdrawing and Electron-Donating Groups on Photovoltaic Properties of Quinoxaline-Based Polymers AITranslate

Pukyong National University; Pukyong National University; Pukyong National University; Pukyong National University; Hannam University; Core Research Institute; Pukyong National University; Pukyong National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, a string of quinoxaline-based D–A-type polymers possessing either electron-withdrawing or electron-donating groups were developed to explore their impact on the photovoltaic efficiency of the polymers. Once the reference polymer PBF-CF3Qx was prepared, extra fluorine atoms and methoxy units were selectively added on the 6,7-positions of the quinoxaline unit of the PBF-CF3Qx reference to provide two objective polymers, PBF-CF3QxF and PBF-CF3QxM, respectively. Owing to the significant influence of the existing electron-withdrawing or electron-donating substituents, each polymer displayed considerably discernible optical, electrochemical, and morphological features. Moreover, the conventional nonfullerene photovoltaic devices based on PBF-CF3QxF and PBF-CF3QxM exhibited superior power conversion efficiencies of 11.37 and 11.18%, respectively, compared to the device based on the PBF-CF3Qx reference 6.96%). These results emphasize the significance of electron-withdrawing and electron-donating substituents in quinoxaline-based polymers for controlling their intrinsic and photovoltaic attributes.

KeyWords AITranslate

quinoxaline electronwithdrawing electrondonating substituent effect fluorine methoxy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01624

Chinese Library Classification Number:

Citation Information:

Herein, a string of quinoxaline-based D–A-type polymers possessing either electron-withdrawing or electron-donating groups were developed to explore their impact on the photovoltaic efficiency of the polymers. Once the reference polymer PBF-CF3Qx was prepared, extra fluorine atoms and methoxy units were selectively added on the 6,7-positions of the quinoxaline unit of the PBF-CF3Qx reference to provide two objective polymers, PBF-CF3QxF and PBF-CF3QxM, respectively. Owing to the significant influence of the existing electron-withdrawing or electron-donating substituents, each polymer displayed considerably discernible optical, electrochemical, and morphological features. Moreover, the conventional nonfullerene photovoltaic devices based on PBF-CF3QxF and PBF-CF3QxM exhibited superior power conversion efficiencies of 11.37 and 11.18%, respectively, compared to the device based on the PBF-CF3Qx reference 6.96%). These results emphasize the significance of electron-withdrawing and electron-donating substituents in quinoxaline-based polymers for controlling their intrinsic and photovoltaic attributes.

quote

GB/T 7714-2015 [1] Dinda Fariesta Nugraha, Danbi Kim, Eunhye Yang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01624.
MLA [1] Dinda Fariesta Nugraha, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01624.
APA [1] Dinda Fariesta Nugraha, Danbi Kim, Eunhye Yang, Seok Woo Lee, Dong Ryeol Whang, Sang A. Lee, Sung Heum Park, & Dong Wook Chang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01624
IEEE [1] Dinda Fariesta Nugraha, Danbi Kim, Eunhye Yang, Seok Woo Lee, Dong Ryeol Whang, Sang A. Lee, Sung Heum Park, and Dong Wook Chang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01624. keywords: {quinoxaline electronwithdrawing electrondonating substituent effect fluorine methoxy}