The Redraw Process for American 218 Tungsten Wire AITranslate
Abstract AITranslate
The general description of a redraw process for American famous 218 tungsten wire is given. The quality control during the manufacturing of the fine tungsten wire is discussed.
KeyWords AITranslate
1刘志英,桂建.不锈钢细丝网的钎焊[J].焊接,1996(2):26-27. 被引量:2
2徐禾水.CO_2气体保护焊细丝的质量分析[J].焊接技术,1991(1):34-37.
3周兴鑫.杯形件拉伸工艺及模具[J].模具工业,1993(6):22-23.
4其它焊接设备[J].机械制造文摘:焊接分册,1996,0(3):31-31.
5周靖华.Q235与QT400-10钢的细丝CO_2焊[J].焊接,2000(2):42-42.
6王新桥,陈静仪,赵志敏,李静.拉伸试验因素对微细丝的力学性能影响[J].功能材料,1991,22(3):160-167. 被引量:3
7陈三平,朱志云.提高钨钼拉丝模使用寿命的探讨[J].中国钨业,2003,18(3):24-26. 被引量:8
8杨威,王彩霞.压缩机储液筒的拉伸工艺和模具设计[J].黑龙江科技信息,2007(11X):36-36.
9钟翔山.阶梯型异形盖的拉伸工艺及模具设计[J].模具制造,2004,4(8):27-30.
10鲜光斌,罗琳.浅谈汽车纵梁件如何选择拉伸和成形工艺[J].模具制造,2012,12(3):32-35.
Basic Information:
DOI:
Chinese Library Classification Number:TG356[金属学及工艺—金属压力加工]
Citation Information:
The general description of a redraw process for American famous 218 tungsten wire is given. The quality control during the manufacturing of the fine tungsten wire is discussed.
quote
| GB/T 7714-2015 | [1] LIU Chu-yun. The Redraw Process for American 218 Tungsten Wire[J]. Rare Metals and Cemented Carbides, 1995(4): 57-61. |
| MLA | [1] LIU Chu-yun. "The Redraw Process for American 218 Tungsten Wire." Rare Metals and Cemented Carbides, no. 4, 1995, pp. 57-61. |
| APA | [1] LIU Chu-yun. (1995). The Redraw Process for American 218 Tungsten Wire. Rare Metals and Cemented Carbides(4), 57-61. |
| IEEE | [1] LIU Chu-yun, "The Redraw Process for American 218 Tungsten Wire," Rare Metals and Cemented Carbides, no. 4, pp. 57-61, 1995. keywords: {tungsten wire, drawing proces, annealing,tensile strength} |