Principle and Application of High temperature Oxidation of Metal in the Design of Cemented Carbide Material AITranslate
Abstract AITranslate
The principle and application of high temperature oxidation of metal and the composition design of hot rollring cemented carbide have been introduced.It has also been indicated that the rolling performance of cemented carbide can be improved with rare earth addition.
KeyWords AITranslate
1金属材料教研室.金属腐蚀及耐蚀合金化原理[M].长沙:中南矿冶学院,1981.
2田家凯,Ansell Gs.合金及显微结构设计[M].北京:冶金工业出版社,1985.
3ZHANGLi,etal.ANewHardmetalforMiningwithNi-CoBinder[J].InternationalJournalofRefractoryMetalsandHardMaterials.1996,14(4):245.
4JAMESJOakes.EffectofCrandMoAdditionstotheBinderPhaseofCementedCarbidesUsedforRodMillRolls[J].MetalPowderReport.1987,42(7,8):492.
1闫兴义,孙玉福,张炎,王美喜.Al对ZG40Cr25Ni20抗磨耐热钢高温抗氧化性的影响[J].铸造技术,2010,31(3):292-294. 被引量:11
2杨洋,王成铎,王光辉,孙玉福.铌对奥氏体耐热钢组织和高温抗氧化性能的影响[J].铸造,2018,67(2):112-117. 被引量:6
3王渊博,吕晓霞,韩丽平.基于TGA-DTA联用技术的本科生开放性创新实验探索[J].现代科学仪器,2021,38(3):90-94.
4陈珮琳,赵艳君,李平珍,温威莹,叶伯溪,韦凤.316L不锈钢高温氧化及高温拉伸性能[J].材料热处理学报,2022,43(11):103-110.
5王钦娟,林少阳,刘东.Mo对00Cr20Ni20耐热钢高温氧化行为影响[J].特种铸造及有色合金,2023,43(5):660-663.
1张炎.铝对HK40耐热钢组织和冲击性能的影响[J].铸造技术,2012,33(9):1031-1033. 被引量:4
2邓想,崔宇.钨对抗磨耐热钢组织和性能的影响[J].铸造技术,2012,33(9):1037-1038. 被引量:7
3王刘利,赵靖宇,吕烨哲,司光东,孙玉福.铝对马氏体抗磨耐热钢高温抗氧化性能的影响[J].铸造,2012,61(12):1439-1442. 被引量:2
4孟倩,喇培清,撒兴瑞.高铝奥氏体不锈钢研究现状及发展趋势[J].材料导报,2013,27(17):101-104. 被引量:2
5许旭鹏,刘守平,韩校宇,鲍俊.Fe-Cr-Al-Si铁素体耐热钢组织结构与抗氧化性[J].材料热处理学报,2017,38(1):106-111. 被引量:7
6郭鑫,喇培清,李恒,卢学峰,魏玉鹏.高铝304奥氏体不锈钢温轧态的性能研究[J].材料研究学报,2017,31(3):175-181. 被引量:1
7付立铭,陈善平,张瑞娜,安淼,索忠源,单爱党.碳含量对Cr25系高铬铸钢组织及性能的影响[J].机械工程材料,2017,41(4):106-110. 被引量:4
8韩成府,路王珂,陈天聪,孙玉福.Al、Ti和W对ZG40Cr25Ni20抗磨耐热钢组织及性能影响[J].铸造技术,2018,39(8):1682-1685. 被引量:3
9刘锐卓,张策,王成铎,王光辉,杨洋,孙玉福.ZG35Cr26Ni12WNRE奥氏体耐热钢的研制[J].铸造技术,2019,40(5):431-435.
10滕铝丹,张拓,臧其玉,杨弋涛.Nb对铸造双相耐热钢高温氧化的影响[J].钢铁研究学报,2019,31(4):415-423. 被引量:5
1严心娥.Ti 600合金热处理过程中的氧化行为研究[J].铸造技术,2015,36(6):1444-1446.
2许兵,廉冰娴.阳极氧化制备氧化钛薄膜机理探讨[J].电镀与精饰,2012,34(6):40-42.
3张玲,朱建军.高合金钢管穿孔顶头的开发[J].现代冶金,2017,45(1):29-33. 被引量:2
4马宗耀,谢发勤,费敬银,杜肖,刘洪波.飞机蒙皮表面氧化膜快速电刷阳极氧化修复[J].电镀与精饰,2007,29(6):38-39. 被引量:4
5杨华春,杨金炳,赖仙红,杨小川,普晓明.超临界锅炉用TP347H、内壁喷丸TP347H和TP347HFG钢管选择探讨[J].东方锅炉,2015,0(1):24-31. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG333.17[金属学及工艺—金属压力加工];TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The principle and application of high temperature oxidation of metal and the composition design of hot rollring cemented carbide have been introduced.It has also been indicated that the rolling performance of cemented carbide can be improved with rare earth addition.
quote
| GB/T 7714-2015 | [1] ZHANG Li, WU En-xi, HUANG Bo-yun. Principle and Application of High temperature Oxidation of Metal in the Design of Cemented Carbide Material[J]. Rare Metals and Cemented Carbides, 2000(4): 19-22. |
| MLA | [1] ZHANG Li, et al., "Principle and Application of High temperature Oxidation of Metal in the Design of Cemented Carbide Material." Rare Metals and Cemented Carbides, no. 4, 2000, pp. 19-22. |
| APA | [1] ZHANG Li, WU En-xi, & HUANG Bo-yun. (2000). Principle and Application of High temperature Oxidation of Metal in the Design of Cemented Carbide Material. Rare Metals and Cemented Carbides(4), 19-22. |
| IEEE | [1] ZHANG Li, WU En-xi, and HUANG Bo-yun, "Principle and Application of High temperature Oxidation of Metal in the Design of Cemented Carbide Material," Rare Metals and Cemented Carbides, no. 4, pp. 19-22, 2000. keywords: {cemented carbide;material design;oxidation at high temperature;roll} |