Study on Surface Modification of MnMoO4for Improving Electrochemical Properties of Lithium-rich Manganese-based Cathode Materials AITranslate

China Electric Power Research Institute;China Electric Power Research Institute;China Electric Power Research Institute;China Electric Power Research Institute;China Electric Power Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-rich manganese-based cathode materials Li1.2[Ni0.13Co0.13Mn0.54]O2 with particle size of 200~300nm were successfully synthesized via the coprecipitation-high temperature solid-state method.And MnMoO4 with oxygen vacancy was deposited on the surface of the materials via wet chemical deposition to improve the electrochemical performance.It is found that surface-modified MnMoO4 successfully induces the formation of spinel LiMn2O4 structure on the surface of the materials,and the special surface heterogeneity can reduce the side-reaction between the bulk and the electrolyte,effectively accommodate oxygen loss during the first charge and promote lithium ion diffusion.Compared with the initial material,the initial Coulombic efficiency of the material modified with MnMoO4 increases from 74.41%to 81.48%,and the capacity of the modified material after 100cycles boosts from 175.8mA·h/g to 205.7mA·h/g,exhibiting excellent electrochemical properties.

KeyWords AITranslate

Li-ion battery lithium-rich manganese-based cathode material MnMoO4 spinel phase electrochemical property

1丁飞翔,李建玲,邓福海,徐国峰,李战雨,刘艳莹.不同PrPO_4包覆方法对富锂锰基正极材料电化学性能的影响[J].稀有金属与硬质合金,2018,46(2):27-31. 被引量:1

1黄鹏,邹大中,牛棒棒,陈浩舟,李勋.高能量密度富锂锰基正极材料结构调控与性能研究[J].稀有金属与硬质合金,2022,50(1):63-69. 被引量:3

2冯婷,王睿,王京玥,王磊营,石沁灵,王立帆,詹纯.压电材料K_(0.5)Na_(0.5)NbO_(3)表面修饰高镍正极材料LiNi_(0.83)Co_(0.12)Mn_(0.05)O_(2)的电化学性能研究[J].稀有金属与硬质合金,2022,50(5):89-95. 被引量:1

1罗欢,李豪,袁盛旭,张亚萍,李劲超.富锂锰基正极材料的改性及其电化学性能研究[J].化学研究与应用,2022,34(8):1862-1871.

2李建华,陈敏,黄二梅.化工园区硫酸锰产业链式发展研究[J].中国锰业,2022,40(6):66-69.

3韦玉红,华骏,彭商权,肖佳俊,章聪华,谭旭峰,颜文斌.TiO_(2)包覆对V_(2)O_(5)锂离子电池负极材料电化学性能的影响[J].稀有金属与硬质合金,2023,51(2):90-97.

1李燕,卢瑶,郭俊明,向明武.镧改性尖晶石LiMn2O4正极材料的研究进展[J].电池,2020,50(1):78-82. 被引量:5

2张晟,廖凯,车兴飞,钟利萍,龚海.铝合金材料非均匀表面应力的逐层构建与还原[J].材料科学与工艺,2019,27(6):12-18.

3贾建波,鹿超,杨志刚,董添添,顾勇飞,徐岩.固溶+时效处理对粉末冶金Ti-22Al-25Nb合金显微硬度的影响[J].材料研究学报,2020,0(3):198-208. 被引量:1

4郭幼丹,王大镇,吴华峰,吴亚平.10CrNi3MoV船用钢热冲压成形表层渐变微观结构与抗冲击性能[J].船舶工程,2019,41(11):105-109. 被引量:1

5朱晓军,李锋,欧东斌,陈连忠,周凯.高导C/C材料在疏导式热防护中的应用探索[J].力学季刊,2020,41(1):171-178. 被引量:2

6沈霞,侯潇棐,李永霞,徐阿生,杨小林.银白杨不定芽诱导与增殖分化研究[J].林业资源管理,2020,0(1):116-124. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ152[化学工程—电化学工业]

Citation Information:

Lithium-rich manganese-based cathode materials Li1.2[Ni0.13Co0.13Mn0.54]O2 with particle size of 200~300nm were successfully synthesized via the coprecipitation-high temperature solid-state method.And MnMoO4 with oxygen vacancy was deposited on the surface of the materials via wet chemical deposition to improve the electrochemical performance.It is found that surface-modified MnMoO4 successfully induces the formation of spinel LiMn2O4 structure on the surface of the materials,and the special surface heterogeneity can reduce the side-reaction between the bulk and the electrolyte,effectively accommodate oxygen loss during the first charge and promote lithium ion diffusion.Compared with the initial material,the initial Coulombic efficiency of the material modified with MnMoO4 increases from 74.41%to 81.48%,and the capacity of the modified material after 100cycles boosts from 175.8mA·h/g to 205.7mA·h/g,exhibiting excellent electrochemical properties.

quote

GB/T 7714-2015 [1] GENG Meng-meng, YANG Kai, MAO Hong-xing, et al. Study on Surface Modification of MnMoO4for Improving Electrochemical Properties of Lithium-rich Manganese-based Cathode Materials[J]. Rare Metals and Cemented Carbides, 2020(1): 61-67.
MLA [1] GENG Meng-meng, et al., "Study on Surface Modification of MnMoO4for Improving Electrochemical Properties of Lithium-rich Manganese-based Cathode Materials." Rare Metals and Cemented Carbides, no. 1, 2020, pp. 61-67.
APA [1] GENG Meng-meng, YANG Kai, MAO Hong-xing, GAO Yun-xing, & ZHONG Jian-jian. (2020). Study on Surface Modification of MnMoO4for Improving Electrochemical Properties of Lithium-rich Manganese-based Cathode Materials. Rare Metals and Cemented Carbides(1), 61-67.
IEEE [1] GENG Meng-meng, YANG Kai, MAO Hong-xing, GAO Yun-xing, and ZHONG Jian-jian, "Study on Surface Modification of MnMoO4for Improving Electrochemical Properties of Lithium-rich Manganese-based Cathode Materials," Rare Metals and Cemented Carbides, no. 1, pp. 61-67, 2020. keywords: {Li-ion battery;lithium-rich manganese-based cathode material;MnMoO4;spinel phase;electrochemical property}