daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Study on the Phase Transition of WO3-xwith High Activity in H2-Reduction AITranslate

Powder Metallurgical Research Institute of Zhongnan University of Technology;Powder Metallurgical Research Institute of Zhongnan University of Technology;Powder Metallurgical Research Institute of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

By means of an in-situ high temperature X-ray diffractiontechnics, the phase transition process and the transition kinetics ofWO3-x with high activity during H2-reduction has been studied, theformation mechanism of superfine W-powder d'uring the reduction wasdisonssed.

KeyWords AITranslate

WO3-x H2-reduction XRD phase transition kinetics.uperfine W-powder preparation

1罗斌辉,张华明.生产优质粗颗粒WC的工艺研究[J].稀有金属与硬质合金,2008,36(1):38-41. 被引量:1

2罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14

3张文朴.钨钼基础工业化学(十)[J].中国钨业,1997,0(12):21-27.

4谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2

1林高安.钨粉形貌与粒度分布对成形性和压坯强度的影响[J].粉末冶金材料科学与工程,2009,14(4):260-264. 被引量:30

2迟静,李惠琪,王淑峰,李敏.矿用WC硬质合金的研究进展与趋势[J].矿山机械,2010,38(8):23-28. 被引量:7

3傅小明.蓝钨循环氧化还原对钨粉末粒度分布的影响[J].硬质合金,2010,27(4):221-223. 被引量:6

4何英.脉冲加热库仑定氧法测定掺杂钨粉中的氧[J].稀有金属与硬质合金,2010,38(2):62-63. 被引量:3

5谢中华,张秋和,王文华,陈树茂.钨粉制备工艺对压坯强度影响的研究[J].中国钨业,2010,25(6):28-30. 被引量:9

6吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3

7雷纯鹏,唐建成,刘万顺,吴爱华,张方.纳米钨/碳化钨粉末的形貌遗传特性及其对粉末均匀性的影响[J].硬质合金,2012,29(5):302-308. 被引量:4

8谢中华,王文华,陈树茂,张秋和,徐绍梅,杜燕.仲钨酸铵自还原制备蓝色氧化钨工艺技术研究[J].中国钨业,2013,28(1):39-41. 被引量:8

9唐建成,雷纯鹏,刘刚,吴爱华.氧化钨的形貌结构对纳米WC粉末均匀性的影响[J].稀有金属材料与工程,2014,43(5):1229-1233. 被引量:7

10德志强.高质量结晶钨粉制取的工艺研究[J].硬质合金,2014,31(3):166-172. 被引量:1

1都兴红,解斌,娄太平.钒钛磁铁矿固态还原的研究[J].东北大学学报:自然科学版,2012,33(5):685-688. 被引量:9

2胡蒙均,尹方庆,魏瑞瑞,邓青宇,扈玫珑.真空碳热还原-酸浸含钛高炉渣制备TiC分析[J].重庆大学学报:自然科学版,2015,38(6):99-106. 被引量:2

3张世来,刘福生,彭小娟,张明建,李永宏,马小娟,薛学东.纳秒尺度金属熔化相变数值模拟及实验验证[J].物理学报,2011,60(1):365-370. 被引量:1

4黄虹.氢还原亚微米钨粉的生产—第Ⅱ部分:APT的控制分解和氧化物的氢还原[J].钨钼材料,1993(4):15-21.

5罗琳,刘永康,何伯泉.一水硬铝石-高岭石型铝土矿焙烧脱硅热力学机理研究[J].有色金属,1999,51(1):25-30. 被引量:18

6J.,A.,Kromhout,韦菁(译),秦玲玲(校对).高速连铸用结晶器保护渣的研究[J].钢铁译文集,2010(1):15-24.

7J.A.Kromhout,韦菁(译),秦玲玲(校对).高速浇铸对结晶器保护渣的要求[J].钢铁译文集,2008(2):1-8.

8王新成,俞海明.电弧炉脱[S][P]和[Pb][Zn]的操作实践[J].特殊钢,2005,26(4):44-45. 被引量:4

9毛佳君,李秋菊,王道净,洪新.不锈钢粉尘中低温氢还原实验研究[J].材料与冶金学报,2009,8(4):258-262. 被引量:3

10Bust.,JA,陈安庆.用非等温热解重量法对金属氧化物还原的动力学研究—第Ⅱ部分:粉末床还原...[J].钨钼材料,1995(3):1-6.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]

Citation Information:

By means of an in-situ high temperature X-ray diffractiontechnics, the phase transition process and the transition kinetics ofWO3-x with high activity during H2-reduction has been studied, theformation mechanism of superfine W-powder d'uring the reduction wasdisonssed.

quote

GB/T 7714-2015 [1] ZOU Zhi-qiang, WANG Xiao, QIAN Chong-liang. A Study on the Phase Transition of WO3-xwith High Activity in H2-Reduction[J]. Rare Metals and Cemented Carbides, 1995(1): 1-5.
MLA [1] ZOU Zhi-qiang, et al., "A Study on the Phase Transition of WO3-xwith High Activity in H2-Reduction." Rare Metals and Cemented Carbides, no. 1, 1995, pp. 1-5.
APA [1] ZOU Zhi-qiang, WANG Xiao, & QIAN Chong-liang. (1995). A Study on the Phase Transition of WO3-xwith High Activity in H2-Reduction. Rare Metals and Cemented Carbides(1), 1-5.
IEEE [1] ZOU Zhi-qiang, WANG Xiao, and QIAN Chong-liang, "A Study on the Phase Transition of WO3-xwith High Activity in H2-Reduction," Rare Metals and Cemented Carbides, no. 1, pp. 1-5, 1995. keywords: {WO3-x;H2-reduction;XRD;phase transition kinetics.uperfine W-powder preparation}