Macroporous Silicone Sheets Integrated with Meshes for Various Applications AITranslate

Tohoku University; Tohoku University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Flexible macroporous silicone gels were prepared using methyltrimethoxysilane and dimethyldimethoxysilane as coprecursors via a two-step reaction catalyzed by acetic acid and ammonia solution. A sheet-shaped material was integrated with the gel by immersing the mesh in the sol during the reaction. The mesh reinforced sheet having a thickness of several millimeters was resistant to bending and pulling and easy to handle, though the physical properties such as hydrophobicity and oleophilicity possessed by the bulk surface were not lost. The composite sheets are used for various applications such as water–oil separation, manipulation of water droplets by adsorption on hydrophobic surfaces, and preparation of giant vesicle dispersions by taking advantage of surface properties and porosity.

KeyWords AITranslate

sol−gel silicone porous materials oil/water separation droplet manipulation vesicle formation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00382

Chinese Library Classification Number:

Citation Information:

Flexible macroporous silicone gels were prepared using methyltrimethoxysilane and dimethyldimethoxysilane as coprecursors via a two-step reaction catalyzed by acetic acid and ammonia solution. A sheet-shaped material was integrated with the gel by immersing the mesh in the sol during the reaction. The mesh reinforced sheet having a thickness of several millimeters was resistant to bending and pulling and easy to handle, though the physical properties such as hydrophobicity and oleophilicity possessed by the bulk surface were not lost. The composite sheets are used for various applications such as water–oil separation, manipulation of water droplets by adsorption on hydrophobic surfaces, and preparation of giant vesicle dispersions by taking advantage of surface properties and porosity.

quote

GB/T 7714-2015 [1] Gen Hayase, Shinichiro M. Nomura. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00382.
MLA [1] Gen Hayase, and Shinichiro M. Nomura. ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00382.
APA [1] Gen Hayase, & Shinichiro M. Nomura. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00382
IEEE [1] Gen Hayase and Shinichiro M. Nomura, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00382. keywords: {sol−gel;silicone;porous materials;oil/water separation;droplet manipulation;vesicle formation}