Polymer-Encapsulated Aerogel Fibers Prepared via Coaxial Wet Spinning with Stepwise Coagulation for Thermal Insulation AITranslate
Abstract AITranslate
Polymer-encapsulated aerogel fibers with high porosity, low density, and good mechanical properties are promising candidates for thermal insulation materials. However, the fabrication of polymer-encapsulated aerogel fibers needs complex processes, which hinders continuous and large-scale fabrication. Herein, we developed a simple yet efficient strategy to continuously fabricate polymer-encapsulated aerogel fibers through coaxial wet spinning followed by conventional freeze drying. The coaxial wet-spinning step features stepwise coagulations containing an inner aerogel precursor as the first coagulation bath and a subsequent water bath as the second coagulation bath. The morphology of polymer-encapsulated aerogel fibers exhibits a porous aerogel network structure of the core layer and porous sheath layer. Thus, the as-prepared aerogel fiber, with cellulose acetate/poly(acrylic acid) (CA/PAA) as the sheath layer and a cellulose nanofiber (CNF) aerogel as the core, possesses low sheath layer density (0.25 g cm–3) and high aerogel core porosity (99.34%). Due to the good mechanical properties of the CA/PAA sheath, the CA/PAA@CNF aerogel fiber shows a high tensile strength of 5.83 MPa. Moreover, the CA/PAA@CNF aerogel fiber exhibits an excellent thermal insulation performance (0.054 W m–1 K–1) ascribed to the multistage porous structure of the fiber, which can significantly reduce heat convection and heat transfer. The good mechanical properties and excellent thermal insulation performance endow the polymer-encapsulated aerogel fibers with promising application in the field of personal thermal management.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01648
Chinese Library Classification Number:
Citation Information:
Polymer-encapsulated aerogel fibers with high porosity, low density, and good mechanical properties are promising candidates for thermal insulation materials. However, the fabrication of polymer-encapsulated aerogel fibers needs complex processes, which hinders continuous and large-scale fabrication. Herein, we developed a simple yet efficient strategy to continuously fabricate polymer-encapsulated aerogel fibers through coaxial wet spinning followed by conventional freeze drying. The coaxial wet-spinning step features stepwise coagulations containing an inner aerogel precursor as the first coagulation bath and a subsequent water bath as the second coagulation bath. The morphology of polymer-encapsulated aerogel fibers exhibits a porous aerogel network structure of the core layer and porous sheath layer. Thus, the as-prepared aerogel fiber, with cellulose acetate/poly(acrylic acid) (CA/PAA) as the sheath layer and a cellulose nanofiber (CNF) aerogel as the core, possesses low sheath layer density (0.25 g cm–3) and high aerogel core porosity (99.34%). Due to the good mechanical properties of the CA/PAA sheath, the CA/PAA@CNF aerogel fiber shows a high tensile strength of 5.83 MPa. Moreover, the CA/PAA@CNF aerogel fiber exhibits an excellent thermal insulation performance (0.054 W m–1 K–1) ascribed to the multistage porous structure of the fiber, which can significantly reduce heat convection and heat transfer. The good mechanical properties and excellent thermal insulation performance endow the polymer-encapsulated aerogel fibers with promising application in the field of personal thermal management.
quote
| GB/T 7714-2015 | [1] Hongrui Sun, Wenxuan Mu, Xihua Cui, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01648. |
| MLA | [1] Hongrui Sun, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01648. |
| APA | [1] Hongrui Sun, Wenxuan Mu, Xihua Cui, Zhiguang Xu, Tao Zhang, & Yan Zhao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01648 |
| IEEE | [1] Hongrui Sun, Wenxuan Mu, Xihua Cui, Zhiguang Xu, Tao Zhang, and Yan Zhao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01648. keywords: {aerogel fiber;coaxial wet spinning;porous structure;thermal insulation;mechanical strength} |