Study on Preparation of WO_3-ZSM-5/SBA-15 Catalyst and its Catalytic Oxidation Desulfurization Performance for FCC Gasoline AITranslate

College of Chemistry,Chemical Engineering and Environmental Engineering,Liaoning Shihua University;College of Chemistry,Chemical Engineering and Environmental Engineering,Liaoning Shihua University;College of Chemistry,Chemical Engineering and Environmental Engineering,Liaoning Shihua University;College of Chemistry,Chemical Engineering and Environmental Engineering,Liaoning Shihua University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

10% WO_3-ZSM-5/SBA-15 catalyst was synthesized by modifying ZSM-5/SBA-15 microporous and mesoporous composite molecular sieve with tungstate acid as tungsten source.And the catalyst was characterized by XRD and SEM.The results show that tungstate acid is distributed uniformly on the catalyst surface.Taking FCC gasoline as the research object,the effects were investigated of reaction temperature,reaction time,H_2O_2 dosage,and WO_3-ZSM-5/SBA-15 amount on catalytic oxidation desulfurization rate.The results show that the desulfurization rate reaches 71.89% under the following conditions:FCC gasoline of 20 mL,reaction temperature of 70 ℃,reaction time of 100 min,mass ratio of catalyst to FCC gasoline of 1∶50,volume ratio of H_2O_2 to FCC gasoline of 2%.The desulfurization sequence of different sulfides is DBT〉4,6-DMDBT〉BT.

KeyWords AITranslate

WO3-ZSM-5/SBA-15 catalyst FCC gasoline catalytic oxidation desulfurization

1刘玉良.FCC汽油脱硫工艺及发展现状[J].广州化工,2010,38(2):16-19. 被引量:18

2张景成,柳云骐,安高军,柴永明,付庆涛,刘晨光.吸附脱硫技术生产清洁油品[J].化学进展,2008,20(11):1834-1845. 被引量:37

3张丽,李春虎,侯影飞,于英民,张新玲.吸附法车用燃料油脱硫技术进展[J].精细石油化工进展,2007,8(8):51-55. 被引量:4

4冯丽娟,高晶晶,王振永,李春虎.柴油吸附脱硫技术研究进展[J].精细石油化工进展,2006,7(6):46-50. 被引量:13

5TAM P S, KITTRELL J R, ELDRIDGE J W. Desulfu- rization of fuel oil by oxidation and extraction (2) : Ki- netic modeling of oxidation reaction [J]. Industrial & Engineering Chemistry Research, 1990,29 (3) : 324-328.

6TAM P S, KITTRELL J R, ELDRIDGE J W. Desulfu- rization of fuel oil by oxidation and extraction (1) : En- hancement of extraction oil yield[J]. Industrial & Engi- neering Chemistry Research, 1990,29 (3) : 321-324.

7李林,唐晓东,粟松涛.NO_x-空气催化氧化直馏汽油脱硫[J].石化技术与应用,2008,26(3):213-215. 被引量:5

8蒋宗轩,吕宏缨,张永娜,李灿.燃油氧化脱硫(英文)[J].催化学报(英文),2011,32(5):707-715. 被引量:27

9王东青,孙发民,贾鹏飞,王锐.MCM-41/Y介孔-微孔复合分子筛的合成及其加氢裂化性能研究[J].炼油技术与工程,2013,43(6):45-48. 被引量:4

10徐群财,冀德坤,丁福臣,李术元.ZSM-5/MCM-41复合分子筛用于FCC汽油脱硫的初步考察[J].石油化工高等学校学报,2013,26(3):1-5. 被引量:7

1丁邦琴,周杰,朱蓓蓓,马志军,高巍.磷钼酸/氧化石墨烯复合材料的制备及其氧化脱硫性能[J].石油化工,2017,46(10):1255-1259. 被引量:2

1Wang Zihao,Li Xiuping,Hao Yangyang,Zhao Rongxiang.Synthesis of H_(2)WO_(4)/GO and Its Oxidative Desulfurization Activity[J].中国炼油与石油化工:英文版,2021,23(2):66-76. 被引量:4

2郭延凯,郭金燕,赵娟,马志远,牛艳艳,杨佳琪,廉静.电沉积制备PMo_(12)/rGO/PPy阳极及其在微生物燃料电池中的应用[J].环境工程,2022,40(3):147-153. 被引量:1

1丁元生,许祥娟,赵大勇,张连中.二氧化硅负载硼钨酸催化氧化柴油脱硫的研究[J].辽宁化工,2015,44(12):1426-1428. 被引量:1

2徐新龙,沈健.微孔-介孔复合分子筛的合成方法研究进展[J].石化技术与应用,2013,31(5):437-441. 被引量:1

3刘翰.3722催化剂半成品干胶制备的工艺改进[J].炼油与催化,1995(2):50-54.

4莫易敏,邹岚,赵源,陈祥斌,俞宝良,李博.摩擦行程对磨损自补偿性的效应[J].材料保护,1997,30(2):14-16. 被引量:6

5张君涛,闫圆圆,郝娜娜,申志兵,梁生荣.微孔-介孔复合分子筛的合成及催化应用[J].现代化工,2014,34(1):43-47. 被引量:4

6付辉,李会鹏,赵华,王健,张晶华.WO_3-ZSM-5/MCM-41用于FCC汽油催化氧化脱硫工艺研究[J].精细石油化工,2013,30(6):19-22. 被引量:2

7李丹东,刘彤,贾欢欢,西仁古丽.加帕尔,张连梓,于海,赵荣祥,石薇薇.钨酸铜催化氧化脱除模拟油中的硫化物[J].辽宁石油化工大学学报,2015,35(2):12-16. 被引量:2

8李倩,宋春敏,王云芳.改性吸附剂的制备及汽油吸附脱硫性能评价[J].当代化工,2010,39(5):512-515. 被引量:5

9中国石油石油化工研究院开发复合分子筛提高加氢催化剂性能[J].石油化工,2013,42(1):52-52.

10郝尚青,刘建,崔振伟,杨传江.基于光纤传感与智能识别的管道安全预警技术[J].石油规划设计,2017,28(2):38-42. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TE624[石油与天然气工程—油气加工工程]

Citation Information:

10% WO_3-ZSM-5/SBA-15 catalyst was synthesized by modifying ZSM-5/SBA-15 microporous and mesoporous composite molecular sieve with tungstate acid as tungsten source.And the catalyst was characterized by XRD and SEM.The results show that tungstate acid is distributed uniformly on the catalyst surface.Taking FCC gasoline as the research object,the effects were investigated of reaction temperature,reaction time,H_2O_2 dosage,and WO_3-ZSM-5/SBA-15 amount on catalytic oxidation desulfurization rate.The results show that the desulfurization rate reaches 71.89% under the following conditions:FCC gasoline of 20 mL,reaction temperature of 70 ℃,reaction time of 100 min,mass ratio of catalyst to FCC gasoline of 1∶50,volume ratio of H_2O_2 to FCC gasoline of 2%.The desulfurization sequence of different sulfides is DBT〉4,6-DMDBT〉BT.

quote

GB/T 7714-2015 [1] HAN Cong, LI Hui-peng, ZHAO Hua, et al. Study on Preparation of WO_3-ZSM-5/SBA-15 Catalyst and its Catalytic Oxidation Desulfurization Performance for FCC Gasoline[J]. Rare Metals and Cemented Carbides, 2016(5): 32-36.
MLA [1] HAN Cong, et al., "Study on Preparation of WO_3-ZSM-5/SBA-15 Catalyst and its Catalytic Oxidation Desulfurization Performance for FCC Gasoline." Rare Metals and Cemented Carbides, no. 5, 2016, pp. 32-36.
APA [1] HAN Cong, LI Hui-peng, ZHAO Hua, & CAI Tian-feng. (2016). Study on Preparation of WO_3-ZSM-5/SBA-15 Catalyst and its Catalytic Oxidation Desulfurization Performance for FCC Gasoline. Rare Metals and Cemented Carbides(5), 32-36.
IEEE [1] HAN Cong, LI Hui-peng, ZHAO Hua, and CAI Tian-feng, "Study on Preparation of WO_3-ZSM-5/SBA-15 Catalyst and its Catalytic Oxidation Desulfurization Performance for FCC Gasoline," Rare Metals and Cemented Carbides, no. 5, pp. 32-36, 2016. keywords: {WO3-ZSM-5/SBA-15 catalyst;FCC gasoline;catalytic oxidation;desulfurization}