Study on the Technology of Recovering Vanadium from Precipitated Mother Liquor by Ion Exchange AITranslate

School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China;School of Resources,Environment and Safety Engineering,University of South China
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vanadium in the precipitated mother liquor from the hydrolytic precipitation process was reco-vered by ion exchange,and the effects of resin type,feed solution pH,temperature and adsorption time on vanadium adsorption were investigated.The kinetics and isothermal adsorption model of vanadium adsorption by D314 resin were studied.The column dynamic adsorption and desorption tests of vanadium were carried out,and the qualified desorption solution was used to dissolve red vanadium.The results show that under the conditions of pH 2.4,temperature 45℃and adsorption time 40 h,the saturated adsorption capacity of D314 resin for V2O5is 243 mg/mL.With 5%NaOH+10%NaCl as a desorption agent,the V2O5concentration at the peak of desorption solution reaches 67.5 g/L with an enrichment ratio of 23.6 times.The adsorption behavior of vanadium on D314 resin conforms to the pseudo-first-order adsorption kinetic equation,and the isothermal adsorption process conforms to the Langmuir model.The recovery of vana-dium from the precipitated mother liquor by ion exchange shows an adsorption rate of over 95.5%and a desorption rate of over 98.2%.The qualified desorption solution can be used to dissolve red vanadium.The technology is feasible and the process is simple,providing a technical way for vanadium recovery.

KeyWords AITranslate

vanadium recovery precipitated mother liquor ion exchange resin adsorption desorption dynamics

1伍珍秀,蒋霖.钒铬溶液水解沉钒试验研究[J].钢铁钒钛,2020(5):22-26. 被引量:4

2王俊,朱学军,曾成华,邓俊,杨涛,王明月,吴艳婷,谢斌.高浓度钒液沉钒工艺研究进展[J].钢铁钒钛,2020(5):8-13. 被引量:4

3张曦月,孙红娟,彭同江,梁小毅,马腾.旺苍含钒石墨矿的工艺矿物学及钒的赋存状态研究[J].矿产综合利用,2020(3):136-142. 被引量:5

4朱先正,霍广生,倪捷,宋琼.利用离子交换树脂从钼酸盐溶液中分离钨和钒(英文)[J].中国有色金属学报:英文版,2017,27(12):2727-2732. 被引量:11

5陈波,包申旭,张一敏.N235浸渍树脂的制备及对钒的吸附研究[J].稀有金属,2018,42(8):891-896. 被引量:9

6阳亚玲,颜文斌,高峰.离子交换树脂分离钒渣浸出液中钒与铬[J].过程工程学报,2017,17(1):84-91. 被引量:6

7朱晓波,李望,管学茂.钒钛磁铁矿弱磁富集-酸浸提钒研究[J].矿冶工程,2016,36(3):70-73. 被引量:6

8万洪强,宁顺明.离子交换树脂吸附钒的动力学研究[J].矿冶工程,2010,30(4):73-76. 被引量:19

9谭超,肖路,王好,李鹏飞.偏钒酸铵连续化制备高纯五氧化二钒片钒研究[J].工业炉,2019,41(4):20-22. 被引量:3

10郑汝伟,包申旭,张一敏.P204-TBP浸渍树脂的制备及对钒(Ⅳ)的吸附研究[J].有色金属:冶炼部分,2018(1):39-43. 被引量:3

1刘淑珍,苏颖玥,陈红梅,常远,袁春龙.酿造技术对野生猕猴桃果酒有机酸组成及其品质的影响[J].酿酒科技,2021(4):71-78. 被引量:5

2刘遵义,谭磊,曲静,杨卉,郝燕.丙烯酸接枝改性氧化石墨烯及其对Ce(Ⅲ)的吸附性能研究[J].功能材料,2023,54(1):1144-1153. 被引量:2

3师嘉澳,马占玲,陈思佳,励建荣.聚乙烯亚胺改性果胶-Fe_(3)O_(4)对亮绿废水的吸附性能研究[J].化工新型材料,2022,50(12):146-150.

4李嘉俊,黄燕秋,谢舒静,伍卫红.响应面法优化白簕叶总皂苷提取工艺及其大孔树脂静态吸附研究[J].广东化工,2023,50(5):49-51. 被引量:1

5邱陵,贾东方,原纪炳,林雪,何炳林.金的离子交换与吸附化学——Ⅱ.大孔交联聚甲基丙烯酸酯 MET-802对 AuCl4-的吸附及解吸动力学[J].化学学报,1988(10):945-951.

6林清,陈启石,田振邦,王俊,张京京.两种形式RPFC-Ⅰ纤维对Pb(Ⅱ)的吸附研究[J].中原工学院学报,2022,33(6):12-18.

7韦琴,刘清怡,范康俊,梅辉.荷叶和罗布麻总黄酮的富集纯化工艺研究[J].粮食与油脂,2023,36(3):81-84.

8赵莉,席晓晶,高杰,李扬,马晓梦,张慧盈,魏敏洁,陈华军,田文杰.新生态MnO_(2)的制备及其对2,4-二硝基苯酚吸附性能的影响[J].硅酸盐通报,2023,42(1):295-301.

9孙宇格,陈林,姚楠,赵春全,胡楠.紫苏籽蛋白协助泡沫分离去除亚甲基蓝[J].当代化工研究,2023(4):163-166.

10张建丰,李晓君,王小慧,侯亚蕊,刘青业,李娜.火麻籽壳多酚不同提取工艺及其抗氧化性[J].食品研究与开发,2023,44(6):153-158.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

Vanadium in the precipitated mother liquor from the hydrolytic precipitation process was reco-vered by ion exchange,and the effects of resin type,feed solution pH,temperature and adsorption time on vanadium adsorption were investigated.The kinetics and isothermal adsorption model of vanadium adsorption by D314 resin were studied.The column dynamic adsorption and desorption tests of vanadium were carried out,and the qualified desorption solution was used to dissolve red vanadium.The results show that under the conditions of pH 2.4,temperature 45℃and adsorption time 40 h,the saturated adsorption capacity of D314 resin for V2O5is 243 mg/mL.With 5%NaOH+10%NaCl as a desorption agent,the V2O5concentration at the peak of desorption solution reaches 67.5 g/L with an enrichment ratio of 23.6 times.The adsorption behavior of vanadium on D314 resin conforms to the pseudo-first-order adsorption kinetic equation,and the isothermal adsorption process conforms to the Langmuir model.The recovery of vana-dium from the precipitated mother liquor by ion exchange shows an adsorption rate of over 95.5%and a desorption rate of over 98.2%.The qualified desorption solution can be used to dissolve red vanadium.The technology is feasible and the process is simple,providing a technical way for vanadium recovery.

quote

GB/T 7714-2015 [1] HAO Xuan-zhang, WANG Qing-liang, LEI Zhi-wu, et al. Study on the Technology of Recovering Vanadium from Precipitated Mother Liquor by Ion Exchange[J]. Rare Metals and Cemented Carbides, 2023(1): 17-23.
MLA [1] HAO Xuan-zhang, et al., "Study on the Technology of Recovering Vanadium from Precipitated Mother Liquor by Ion Exchange." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 17-23.
APA [1] HAO Xuan-zhang, WANG Qing-liang, LEI Zhi-wu, WANG Hong-qiang, HU Fang, FAN Shi-yao, SU Yu-cheng, LE Dong-dong, & HU E-ming. (2023). Study on the Technology of Recovering Vanadium from Precipitated Mother Liquor by Ion Exchange. Rare Metals and Cemented Carbides(1), 17-23.
IEEE [1] HAO Xuan-zhang, WANG Qing-liang, LEI Zhi-wu, WANG Hong-qiang, HU Fang, FAN Shi-yao, SU Yu-cheng, LE Dong-dong, and HU E-ming, "Study on the Technology of Recovering Vanadium from Precipitated Mother Liquor by Ion Exchange," Rare Metals and Cemented Carbides, no. 1, pp. 17-23, 2023. keywords: {vanadium recovery;precipitated mother liquor;ion exchange resin;adsorption;desorption;dynamics}