daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Modulation of Electrical Characteristics of Polymer–Ceramic–Graphene Hybrid Composite for Piezoelectric Energy Harvesting Modulation of Electrical Characteristics of Polymer–Ceramic–Graphene Hybrid Composite for Piezoelectric Energy Harvesting AITranslate

C. V. Raman Global University; C. V. Raman Global University;Centre for Materials for Electronics Technology, Thrissur 680581; Xian International University; C. V. Raman Global University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The use of lead-based ceramics to enhance the piezoelectricity of poly(vinylidene fluoride) (PVDF) is the primary challenge toward nontoxic flexible piezoelectric devices. 0.67BiFeO3-0.33BaTiO3 (BF33BT) is one of the lead-free piezoceramics with high-temperature stability and comparable piezoelectric characteristics to existing lead-based piezoceramics. The work represents PVDF–BF33BT two-phase and PVDF–BF33BT–graphene oxide (GO) three-phase composites with detailed analysis of the dielectric, ferroelectric, and piezoelectric characterizations. Solvent-casting followed by the hot-pressing technique improves the electroactive β-phase of ≥60% in the composites. With BF33BT and GO loading, the dielectric constant and loss tangent increase; however, there is an abrupt rise at the threshold GO concentration of 0.08 wt %. The three-phase composite with 40 wt % BF33BT and 0.08 wt % GO records a dielectric constant of 303 and a loss tangent of 0.68. The harvester out of the same composition achieves a piezoelectric strain constant of 9 pC·N–1, an open-circuit voltage of ∼3.9 V, and a short-circuit current of 1.3 μA. The feasibility of the harvester was tested by powering a calculator by charging a 2.2 μF capacitor after rectification. The recoverable energy density also improves seven times, indicating that the PVDF–BF33BT–GO composite is preferable for piezoelectric and energy storage applications.

KeyWords AITranslate

threephase composite piezoelectric energy harvester percolation threshold dielectric ferroelectric energy storage density
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00078

Chinese Library Classification Number:

Citation Information:

The use of lead-based ceramics to enhance the piezoelectricity of poly(vinylidene fluoride) (PVDF) is the primary challenge toward nontoxic flexible piezoelectric devices. 0.67BiFeO3-0.33BaTiO3 (BF33BT) is one of the lead-free piezoceramics with high-temperature stability and comparable piezoelectric characteristics to existing lead-based piezoceramics. The work represents PVDF–BF33BT two-phase and PVDF–BF33BT–graphene oxide (GO) three-phase composites with detailed analysis of the dielectric, ferroelectric, and piezoelectric characterizations. Solvent-casting followed by the hot-pressing technique improves the electroactive β-phase of ≥60% in the composites. With BF33BT and GO loading, the dielectric constant and loss tangent increase; however, there is an abrupt rise at the threshold GO concentration of 0.08 wt %. The three-phase composite with 40 wt % BF33BT and 0.08 wt % GO records a dielectric constant of 303 and a loss tangent of 0.68. The harvester out of the same composition achieves a piezoelectric strain constant of 9 pC·N–1, an open-circuit voltage of ∼3.9 V, and a short-circuit current of 1.3 μA. The feasibility of the harvester was tested by powering a calculator by charging a 2.2 μF capacitor after rectification. The recoverable energy density also improves seven times, indicating that the PVDF–BF33BT–GO composite is preferable for piezoelectric and energy storage applications.

quote

GB/T 7714-2015 [1] Sakti Prasanna Muduli, Loree Lipsa, Abhisek Choudhary, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00078.
MLA [1] Sakti Prasanna Muduli, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00078.
APA [1] Sakti Prasanna Muduli, Loree Lipsa, Abhisek Choudhary, Shailendra Rajput, & Sabyasachi Parida. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00078
IEEE [1] Sakti Prasanna Muduli, Loree Lipsa, Abhisek Choudhary, Shailendra Rajput, and Sabyasachi Parida, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00078. keywords: {threephase composite piezoelectric energy harvester percolation threshold dielectric ferroelectric energy storage density}