High Short-Circuit Current Density via Integrating the Perovskite and Ternary Organic Bulk Heterojunction AITranslate

The University of Hong Kong; Southern University of Science and Technology; University of Massachusetts; The University of Hong Kong; University of Massachusetts; Southern University of Science and Technology; Southern University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We demonstrate a record short-circuit current density (28.06 mA/cm2) in a single-junction perovskite solar cell with a 1.6 eV bandgap absorber. We achieve this by integrating a ternary organic bulk heterojunction structure into a perovskite top layer to extend the photoresponse to the near-infrared region.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01964

Chinese Library Classification Number:

Citation Information:

We demonstrate a record short-circuit current density (28.06 mA/cm2) in a single-junction perovskite solar cell with a 1.6 eV bandgap absorber. We achieve this by integrating a ternary organic bulk heterojunction structure into a perovskite top layer to extend the photoresponse to the near-infrared region.

quote

GB/T 7714-2015 [1] Wei Chen, Huiliang Sun, Qin Hu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01964.
MLA [1] Wei Chen, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01964.
APA [1] Wei Chen, Huiliang Sun, Qin Hu, Aleksandra B. Djurišić, Thomas P. Russell, Xugang Guo, & Zhubing He. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01964
IEEE [1] Wei Chen, Huiliang Sun, Qin Hu, Aleksandra B. Djurišić, Thomas P. Russell, Xugang Guo, and Zhubing He, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01964.