Applications of USA and Russian Developed Titanium and Its Alloys in Tank AITranslate

Northwest Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of Ti and Ti alloy physical and chemical properties and their effect on lowering tank weight,brief description is made of the present application of USA and Russia developed Ti and Ti alloy in the tank.

KeyWords AITranslate

USA Russia Ti and Ti alloy tank application

1[1]Montgomevy J S,et al.Low-Cost titanium armors for Combat vehicles[J].Journal of Metals,1997,49(5):45.

2[2]Campbell G.Titanium applications for the abrams main battle tank[A].In:International Titanium Association Conference ed.Proceedings of the 1996 International Titanium Association conference[C].Las Vegs NV:International Titanium Association Conference,1996.105.

3[3]Wells M G H,el al.Evaluation of a russian titanium tank boor[A].In:MMMS ed.Non-Aerospace Applications of Titanium[C].USA:MMMS,1998.305.

1李明兵,朱知寿,王新南,费跃,祝力伟,商国强,李静.TC32钛合金的动态力学性能及损伤特点[J].航空材料学报,2016,36(5):7-13. 被引量:2

1李明兵,王新南,商国强,祝力伟,李静,刘格辰,信云鹏,朱知寿.双态组织TC32钛合金的抗弹性能及损伤机制[J].中国有色金属学报,2021,31(2):365-372. 被引量:3

2杨柳,王莹,吴静怡,刘昕.α+β两相钛合金的动态压缩性能对抗弹性能的影响分析[J].钢铁钒钛,2022,43(4):42-47. 被引量:1

1陈建宇,徐更光.GAP应用研究进展[J].兵工自动化,2015,34(4):67-70. 被引量:12

2张光全,董海山.2,4-二硝基苯甲醚为基熔铸炸药的研究进展[J].含能材料,2010,18(5):604-609. 被引量:41

3吕金顺,陈华乐,王惠君.军事隐蔽材料及其化学制备[J].化学教育,1999,14(2):1-3. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TJ811[兵器科学与技术—武器系统与运用工程];TG146.23[金属学及工艺—金属材料]

Citation Information:

In view of Ti and Ti alloy physical and chemical properties and their effect on lowering tank weight,brief description is made of the present application of USA and Russia developed Ti and Ti alloy in the tank.

quote

GB/T 7714-2015 [1] HUANG Hong. Applications of USA and Russian Developed Titanium and Its Alloys in Tank[J]. Rare Metals and Cemented Carbides, 2002(3): 45-47.
MLA [1] HUANG Hong. "Applications of USA and Russian Developed Titanium and Its Alloys in Tank." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 45-47.
APA [1] HUANG Hong. (2002). Applications of USA and Russian Developed Titanium and Its Alloys in Tank. Rare Metals and Cemented Carbides(3), 45-47.
IEEE [1] HUANG Hong, "Applications of USA and Russian Developed Titanium and Its Alloys in Tank," Rare Metals and Cemented Carbides, no. 3, pp. 45-47, 2002. keywords: {USA;Russia;Ti and Ti alloy;tank;application}