daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Binder on Formability of SCR Denitration Catalyst from Rare Earth Tailings Activated by Sulfuric Acid AITranslate

Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology;Key Laboratory of Efficient and Clean Combustion of Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Formed catalyst was prepared by adding binders(sesbania powder,sodium carboxymethyl cellu-lose and guar gum)into sulphuric acid activated rare earth tailings catalyst powder.The effects of types and amounts of binders on the denitration performance of formed catalysts were investigated.The formed catalysts were characterized by means of catalytic activity evaluation,compressive strength test,BET,XRD and H2-TPR.The results show that after extrusion forming of catalyst powder,the specific surface area de-creases from 3.70 m2/g to 1.22 m2/g,and the denitration efficiency is only 56%.The addition of 2.5%guar gum enhances the adhesion among the rare earth tailings powder particles,enabling the catalyst to be smoothly extruded,and has the effect of pore formation,greatly improving the specific surface area and redox capacity of the catalyst.Under the combined action of 5%polyethylene glycol and 2.5%guar gum,the formed acid activated rare earth tailings catalyst has a denitration efficiency of 91.6%and excellent N2 selectivity,truly realizing the resource utilization of rare earth tailings.

KeyWords AITranslate

formed catalyst rare earth tailings binder NH3-SCR denitration efficiency nitrogen selectivity
No data

Basic Information:

DOI:

Chinese Library Classification Number:TQ426.68[化学工程]

Citation Information:

Formed catalyst was prepared by adding binders(sesbania powder,sodium carboxymethyl cellu-lose and guar gum)into sulphuric acid activated rare earth tailings catalyst powder.The effects of types and amounts of binders on the denitration performance of formed catalysts were investigated.The formed catalysts were characterized by means of catalytic activity evaluation,compressive strength test,BET,XRD and H2-TPR.The results show that after extrusion forming of catalyst powder,the specific surface area de-creases from 3.70 m2/g to 1.22 m2/g,and the denitration efficiency is only 56%.The addition of 2.5%guar gum enhances the adhesion among the rare earth tailings powder particles,enabling the catalyst to be smoothly extruded,and has the effect of pore formation,greatly improving the specific surface area and redox capacity of the catalyst.Under the combined action of 5%polyethylene glycol and 2.5%guar gum,the formed acid activated rare earth tailings catalyst has a denitration efficiency of 91.6%and excellent N2 selectivity,truly realizing the resource utilization of rare earth tailings.

quote

GB/T 7714-2015 [1] HOU Li-min, YE Yu-qiao, WANG Xin-zhan, et al. Effect of Binder on Formability of SCR Denitration Catalyst from Rare Earth Tailings Activated by Sulfuric Acid[J]. Rare Metals and Cemented Carbides, 2024(5): 43-49.
MLA [1] HOU Li-min, et al., "Effect of Binder on Formability of SCR Denitration Catalyst from Rare Earth Tailings Activated by Sulfuric Acid." Rare Metals and Cemented Carbides, no. 5, 2024, pp. 43-49.
APA [1] HOU Li-min, YE Yu-qiao, WANG Xin-zhan, SUN Xian-kang, LI Jia-ming, LU Lin-bo, CHEN Han, & WU Wen-fei. (2024). Effect of Binder on Formability of SCR Denitration Catalyst from Rare Earth Tailings Activated by Sulfuric Acid. Rare Metals and Cemented Carbides(5), 43-49.
IEEE [1] HOU Li-min, YE Yu-qiao, WANG Xin-zhan, SUN Xian-kang, LI Jia-ming, LU Lin-bo, CHEN Han, and WU Wen-fei, "Effect of Binder on Formability of SCR Denitration Catalyst from Rare Earth Tailings Activated by Sulfuric Acid," Rare Metals and Cemented Carbides, no. 5, pp. 43-49, 2024. keywords: {formed catalyst;rare earth tailings;binder;NH3-SCR;denitration efficiency;nitrogen selectivity}