Research Status of Preparation of Titanium and Its Alloys by Molten Salt Electrolysis AITranslate
Abstract AITranslate
As time develops,the processes for preparing titanium and its alloys have become more and more environmentally friendly.At present,molten salt electrolysis has gained significant attention in the field of preparing titanium and its alloys due to its low energy consumption and low pollution.The article introduces the reduction mechanisms of four methods,including FFC Cambridge process,OS calciothermic reduction method,solid oxygen permeable membrane(SOM)method,and USTB method,which have been the research hotspots of molten salt electrolysis in recent years.Meanwhile,the latest research progress of these methods is summarized to comparatively analyze their merits and demerits,and the future development of molten salt electrolysis is discussed based on the research status.
KeyWords AITranslate
1扈玫珑,白晨光,杜继红,邱贵宝,吕学伟,施瑞盟.熔盐电解制备钛及钛合金研究进展[J].钛工业进展,2009,26(3):7-12. 被引量:8
2曹大力,王吉坤,邱竹贤,石忠宁,王兆文,郭思辰.金属钛制备工艺研究进展[J].钛工业进展,2008,25(4):9-13. 被引量:7
3尚青亮,刘捷,方树铭,周林.金属钛粉的制备工艺[J].材料导报:纳米与新材料专辑,2013,27(1):97-100. 被引量:20
4胡耀强.海绵钛生产工艺综述[J].科技视界,2016(8):1-2. 被引量:3
5张娜,李兰杰,董自慧,张苏新,李九江,吴春亮.金属钛的制备研究[J].河北冶金,2020,0(5):37-40. 被引量:4
6贾雷,严红燕,李慧,刘畅,张帅.熔盐电解精炼制备高纯铪工艺研究进展[J].矿产综合利用,2020,0(1):33-38. 被引量:2
7孙金行,蔡艳青,王崇,李允,李瑾,许莹.熔盐法制备锆合金研究进展[J].矿产综合利用,2021(5):25-31. 被引量:1
8龙翔,李保金,汪云华,刘建良.熔盐电解TiO_2制取钛金属工艺研究进展[J].材料导报:纳米与新材料专辑,2013,27(2):78-82. 被引量:7
9赖冠全,邹星礼,程红伟,郑凯,李尚书,耿淑华,鲁雄刚.固体透氧膜(SOM)法由SiO_2电解制备多晶硅[J].功能材料,2016,47(2):2177-2182. 被引量:1
10罗晶.碳热还原法制备氮化钒铁合金的性能表征研究[J].矿产综合利用,2019,0(6):132-135. 被引量:2
1王明.稀土金属冶炼生产线的工艺设计[J].稀有金属与硬质合金,2023,51(4):13-17.
2袁振东,范永鑫,张宪硕.铀元素的发现及其概念的发展[J].化学教学,2023(10):92-97.
3张毅华,陆鈃,赵海懿,陈曦,王乔,冯宇,程晓晴,沈文飚.氢化镁调控的绿豆渗透耐性与一氧化氮介导的脯氨酸代谢有关[J].植物生理学报,2023,59(10):1964-1974.
Basic Information:
DOI:
Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]
Citation Information:
As time develops,the processes for preparing titanium and its alloys have become more and more environmentally friendly.At present,molten salt electrolysis has gained significant attention in the field of preparing titanium and its alloys due to its low energy consumption and low pollution.The article introduces the reduction mechanisms of four methods,including FFC Cambridge process,OS calciothermic reduction method,solid oxygen permeable membrane(SOM)method,and USTB method,which have been the research hotspots of molten salt electrolysis in recent years.Meanwhile,the latest research progress of these methods is summarized to comparatively analyze their merits and demerits,and the future development of molten salt electrolysis is discussed based on the research status.
quote
| GB/T 7714-2015 | [1] DONG Shuo, LIANG Jing-long. Research Status of Preparation of Titanium and Its Alloys by Molten Salt Electrolysis[J]. Rare Metals and Cemented Carbides, 2023(5): 1-7. |
| MLA | [1] DONG Shuo, and LIANG Jing-long. "Research Status of Preparation of Titanium and Its Alloys by Molten Salt Electrolysis." Rare Metals and Cemented Carbides, no. 5, 2023, pp. 1-7. |
| APA | [1] DONG Shuo, & LIANG Jing-long. (2023). Research Status of Preparation of Titanium and Its Alloys by Molten Salt Electrolysis. Rare Metals and Cemented Carbides(5), 1-7. |
| IEEE | [1] DONG Shuo and LIANG Jing-long, "Research Status of Preparation of Titanium and Its Alloys by Molten Salt Electrolysis," Rare Metals and Cemented Carbides, no. 5, pp. 1-7, 2023. keywords: {molten salt electrolysis;titanium;reduction mechanism;FFC Cambridge process;OS calciothermic reduction method;solid oxygen permeable membrane method;USTB method} |