Optimizing Microstructure Morphology and Reducing Electronic Losses in 1 cm2 Polymer Solar Cells to Achieve Efficiency over 15% AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; Zhengzhou University; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The successful demonstration of high-performance organic solar cells (OSCs) on a relatively large area is vital for their industrial viability and future application. When the device area is enlarged from several mm2 to the scale of >1 cm2, critical losses caused by film inhomogeneity or defects in the photoactive layer strongly restrict the performance and reproducibility of OSCs. In this work, we demonstrate that through delicate optimization of a photoactive layer and minimization of optoelectronic losses, an impressive external quantum efficiency maximum up to 88% and an internal quantum efficiency peak of 97% are achieved for nonfullerene OSCs. Further incorporating fullerene as the third component into the photoactive layer optimizes the microstructure morphology, enabling large-scale devices with an area of >1.1 cm2, surpassing the 15% efficiency milestone. The exciting results demonstrated in this work highlight the strategic priority to minimize losses through both materials and electronic engineering toward high-performance large-area OSCs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01447

Chinese Library Classification Number:

Citation Information:

The successful demonstration of high-performance organic solar cells (OSCs) on a relatively large area is vital for their industrial viability and future application. When the device area is enlarged from several mm2 to the scale of >1 cm2, critical losses caused by film inhomogeneity or defects in the photoactive layer strongly restrict the performance and reproducibility of OSCs. In this work, we demonstrate that through delicate optimization of a photoactive layer and minimization of optoelectronic losses, an impressive external quantum efficiency maximum up to 88% and an internal quantum efficiency peak of 97% are achieved for nonfullerene OSCs. Further incorporating fullerene as the third component into the photoactive layer optimizes the microstructure morphology, enabling large-scale devices with an area of >1.1 cm2, surpassing the 15% efficiency milestone. The exciting results demonstrated in this work highlight the strategic priority to minimize losses through both materials and electronic engineering toward high-performance large-area OSCs.

quote

GB/T 7714-2015 [1] Baobing Fan, Zhaomiyi Zeng, Wenkai Zhong, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01447.
MLA [1] Baobing Fan, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01447.
APA [1] Baobing Fan, Zhaomiyi Zeng, Wenkai Zhong, Lei Ying, Difei Zhang, Meijing Li, Feng Peng, Ning Li, Fei Huang, & Yong Cao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01447
IEEE [1] Baobing Fan, Zhaomiyi Zeng, Wenkai Zhong, Lei Ying, Difei Zhang, Meijing Li, Feng Peng, Ning Li, Fei Huang, and Yong Cao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01447.