Simulation Analysis and Research on Temperature Field in Rare Earth Electrolytic Cell AITranslate
Abstract AITranslate
With 15 kA rare earth electrolytic cell as the research object,its temperature field was simulated by using the electro-thermal coupling module of COMSOL software,and the law was analyzed of tempera- ture distribution in the rare earth electrolytic cell. The results show that the transverse temperature distri- bution in the rare earth electrolysis cell is as follows:the region between the arc-shaped anode and its adja- cent cathode has the highest temperature,and the region between the cathode and the cathode has slightly lower temperature. The temperature rises at first and then declines from top to bottom along the vertical direction of the electrolytic cell.
KeyWords AITranslate
1王祥生,王志强,陈德宏,庞思明,徐立海,李宗安,颜世宏.稀土金属制备技术发展及现状[J].稀土,2015,36(5):123-132. 被引量:27
2胡宪伟,王兆文,罗旭东,路贵民,崔建忠,陈广华.氟化物熔盐中含钕及钕—氧络合离子存在形式的研究[J].稀土,2008,29(5):58-60. 被引量:8
3刘中兴,齐素慈.3kA钕电解槽流场的数值模拟[J].稀有金属材料与工程,2007,36(2):194-196. 被引量:19
4任永红,汪进宝,贺友多,刘中兴.稀土电解槽的电场计算与槽电压分析[J].包头钢铁学院学报,2003,22(4):313-317. 被引量:16
5邓左民,张小联,王俊.稀土电解槽温度场的数值分析[J].江西有色金属,2004,18(1):26-27. 被引量:12
6刘中兴,伍永福,张宏光.稀土熔盐电解槽电场的仿真模拟[J].有色金属:冶炼部分,2008(1):34-37. 被引量:23
7张小联.稀土熔盐电解中电解槽温度分布测定[J].江西有色金属,1998,12(4):24-25. 被引量:3
8伍永福,刘中兴,李曙阳,任永红.稀土熔盐电解槽内温度场数值模拟[J].有色金属:冶炼部分,2012(1):27-31. 被引量:18
9尹小东,刘中兴,曹运涛.稀土熔盐电解槽的热平衡计算[J].包头钢铁学院学报,2002,21(1):19-22. 被引量:16
1廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4
2龚姚腾,周宏杰,逄启寿,王海辉.15 kA稀土电解槽阴阳极中心距对槽内电热场影响的模拟分析[J].稀有金属与硬质合金,2018,46(2):1-5. 被引量:7
3冯羽生,逄启寿,许礼刚.不同阴阳极圆心距下稀土电解槽的电解特性分析[J].厦门大学学报:自然科学版,2018,57(4):581-586. 被引量:9
4龚姚腾,李玉泽,逄启寿,王海辉,冯羽生.多因素对稀土电解槽电解效率的影响[J].有色金属工程,2019,9(8):53-58. 被引量:6
5逄启寿,张雨开,黄杰,张浩.稀土电解槽不同阴极结构的电解特性分析[J].稀土,2019,40(5):17-23. 被引量:4
6闫光礼,冯羽生,徐水太.镝铁阴极电蚀对稀土电解槽电解特性的影响[J].有色金属科学与工程,2019,10(6):92-96. 被引量:1
7叶楠,逄启寿,张浩,王海辉.大电流稀土电解槽阳极结构研究[J].中国稀土学报,2020,38(1):83-89. 被引量:5
8逄启寿,叶楠,张浩,周宏杰.6kA稀土电解槽电极位置对电场影响的模拟分析[J].机械设计与制造,2021(2):157-159. 被引量:1
9杨培宏,王新春,刘玉宝,张耀,张自雷,吕东澔.稀土熔盐电解智能控制系统研究与应用[J].稀土,2022,43(3):34-40. 被引量:2
10逄启寿,刘胜,万福兴.不同保温层厚度下稀土电解槽电热场分析[J].中国有色冶金,2023,52(1):68-74.
1廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4
2龚姚腾,李玉泽,逄启寿,王海辉,冯羽生.多因素对稀土电解槽电解效率的影响[J].有色金属工程,2019,9(8):53-58. 被引量:6
3逄启寿,张雨开,黄杰,张浩.稀土电解槽不同阴极结构的电解特性分析[J].稀土,2019,40(5):17-23. 被引量:4
4闫光礼,冯羽生,徐水太.镝铁阴极电蚀对稀土电解槽电解特性的影响[J].有色金属科学与工程,2019,10(6):92-96. 被引量:1
5叶楠,逄启寿,张浩,王海辉.大电流稀土电解槽阳极结构研究[J].中国稀土学报,2020,38(1):83-89. 被引量:5
6唐焱,刘金.稀土金属及合金12kA电解槽优化设计仿真研究[J].装备制造技术,2020(3):5-9. 被引量:2
7刘庆生,程华金,谈成亮,邱建民,李华杰.非均一极距对稀土电解多相流影响的数值模拟及实验验证[J].有色金属科学与工程,2020,11(5):59-68.
8潘利生,杨欢,李博,魏小林,陈红迪,史维秀.稀土冶炼电解槽余热取热试验研究[J].洁净煤技术,2020,26(5):153-158.
9逄启寿,叶楠,张浩,周宏杰.6kA稀土电解槽电极位置对电场影响的模拟分析[J].机械设计与制造,2021(2):157-159. 被引量:1
10冯羽生,严少卿.管式稀土萃取槽中搅拌桨转速优选研究[J].现代矿业,2021,37(4):149-151. 被引量:1
1罗立刚.电热饼的结构、选购与安全使用[J].电世界,1994,35(11):44-45.
2马茹欣,解林.电热液体保温器[J].现代日用科学,1989(2):7-7.
3关于Metcal烙铁的问答[J].世界产品与技术,2001(7):53-55.
4刘岩,欧阳涵,刘卓,邹洋,赵璐明,田静静,黎鸣,江文,李舟.基于摩擦纳米发电机的自驱动计步传感器[J].电子科技大学学报,2017,46(5):790-794. 被引量:2
5杜鸣笛,贾雅琼,何淑珍.亚波长金属光栅的凹槽深度对太赫兹伪表面等离子体影响(英文)[J].红外与激光工程,2017,46(8):19-23. 被引量:1
6曾彦珺,王彤,李怡,盛华夏.基于有限元法的±500kV同塔双回线路电磁环境仿真计算[J].电测与仪表,2017,54(17):18-24. 被引量:11
7焦万才,杜银.QFP元件引脚钎焊温度场的瞬态数值模拟[J].电焊机,2017,47(9):57-61.
8程龙泉,魏金民,赵凯.氧化物燃料电池动态性能的COMSOL模拟[J].电源技术,2017,41(9):1299-1300.
9蒋买勇.锚注加固在山区水闸工程中的应用研究[J].中国农村水利水电,2017(9):146-149.
10董华,张文婵,林欢,张敬奎.石墨烯粉末导热性能的研究[J].热科学与技术,2017,16(4):259-265. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
With 15 kA rare earth electrolytic cell as the research object,its temperature field was simulated by using the electro-thermal coupling module of COMSOL software,and the law was analyzed of tempera- ture distribution in the rare earth electrolytic cell. The results show that the transverse temperature distri- bution in the rare earth electrolysis cell is as follows:the region between the arc-shaped anode and its adja- cent cathode has the highest temperature,and the region between the cathode and the cathode has slightly lower temperature. The temperature rises at first and then declines from top to bottom along the vertical direction of the electrolytic cell.
quote
| GB/T 7714-2015 | [1] WANG Hai-hui, PANG Qi-shou, GAO Piao-piao. Simulation Analysis and Research on Temperature Field in Rare Earth Electrolytic Cell[J]. Rare Metals and Cemented Carbides, 2017(4): 12-15. |
| MLA | [1] WANG Hai-hui, et al., "Simulation Analysis and Research on Temperature Field in Rare Earth Electrolytic Cell." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 12-15. |
| APA | [1] WANG Hai-hui, PANG Qi-shou, & GAO Piao-piao. (2017). Simulation Analysis and Research on Temperature Field in Rare Earth Electrolytic Cell. Rare Metals and Cemented Carbides(4), 12-15. |
| IEEE | [1] WANG Hai-hui, PANG Qi-shou, and GAO Piao-piao, "Simulation Analysis and Research on Temperature Field in Rare Earth Electrolytic Cell," Rare Metals and Cemented Carbides, no. 4, pp. 12-15, 2017. keywords: {rare earth electrolysis;electrolytic cell;temperature field;temperature distribution;simulation analysis;COMSOL software} |