1Rapid Hydrolysis of Waste and Scrap PA6 Textiles to ε-Caprolactam AITranslate

Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The great challenge for the chemical recycling of waste and scrap (Was) polyamide 6 (PA6) textiles is to achieve chemical recycling with short processes, low costs, and low energy consumption. An effective method was developed to convert waste PA6 textiles into high-purity ε-caprolactam (CPL) with a short process, low reaction temperature, and low water consumption. This work described in detail the feasibility of water as a catalyst for PA6 hydrolysis under subcritical water, enabling the degradation of roughly 100% of virgin PA6 (vPA6) and Was PA6 textiles into 89.9 and 91.6% of CPL under optimized conditions, i.e., 300 °C of temperature, a mass ratio (H2O/PA6) of 11:1, and 60 min of reaction time, respectively. Moreover, the purity of produced CPL was as high as 99.62%, similar to that of fresh CPL. Furthermore, the n-value of oligomers in liquid products ranged from 0 to 5. In contrast, the concentrations of cyclic oligomers (Cn) with n-value (n ≥ 1) and linear oligomers (Ln) with n-value (n ≥ 2) gradually decreased. In addition, the total contents of Cn were far less than those of Ln. In summary, Was PA6 textiles were easier to degrade than vPA6, and the concentration of the target monomer was higher. Overall, this study offers a green, elementary, and cost-effective technology to recycle and reuse CPL for hydrolysis of Was PA6 textiles.

KeyWords AITranslate

virgin PA6 waste and scrap PA6 textiles degradation εcaprolactam subcritical water
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01744

Chinese Library Classification Number:

Citation Information:

The great challenge for the chemical recycling of waste and scrap (Was) polyamide 6 (PA6) textiles is to achieve chemical recycling with short processes, low costs, and low energy consumption. An effective method was developed to convert waste PA6 textiles into high-purity ε-caprolactam (CPL) with a short process, low reaction temperature, and low water consumption. This work described in detail the feasibility of water as a catalyst for PA6 hydrolysis under subcritical water, enabling the degradation of roughly 100% of virgin PA6 (vPA6) and Was PA6 textiles into 89.9 and 91.6% of CPL under optimized conditions, i.e., 300 °C of temperature, a mass ratio (H2O/PA6) of 11:1, and 60 min of reaction time, respectively. Moreover, the purity of produced CPL was as high as 99.62%, similar to that of fresh CPL. Furthermore, the n-value of oligomers in liquid products ranged from 0 to 5. In contrast, the concentrations of cyclic oligomers (Cn) with n-value (n ≥ 1) and linear oligomers (Ln) with n-value (n ≥ 2) gradually decreased. In addition, the total contents of Cn were far less than those of Ln. In summary, Was PA6 textiles were easier to degrade than vPA6, and the concentration of the target monomer was higher. Overall, this study offers a green, elementary, and cost-effective technology to recycle and reuse CPL for hydrolysis of Was PA6 textiles.

quote

GB/T 7714-2015 [1] Hongmei Hu, Qianhui Xu, Lina Sun, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01744.
MLA [1] Hongmei Hu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01744.
APA [1] Hongmei Hu, Qianhui Xu, Lina Sun, Ruishu Zhu, Tingting Gao, Yong He, Bomou Ma, Jianyong Yu, & Xueli Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01744
IEEE [1] Hongmei Hu, Qianhui Xu, Lina Sun, Ruishu Zhu, Tingting Gao, Yong He, Bomou Ma, Jianyong Yu, and Xueli Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01744. keywords: {virgin PA6;waste and scrap PA6 textiles;degradation;εcaprolactam;subcritical water}