Research Progress of the Role of Sc in Al-Cu Alloys AITranslate
Abstract AITranslate
In view of the excellent comprehensive properties of Al-Cu alloys,the research progress of the effects of Sc and the combined addition of Sc and other elements in Al-Cu alloys at home and abroad is re-viewed,which include the changes of grain size,phase composition and distribution,physical and mechani-cal properties of Al-Cu alloys after the addition of Sc or the combined addition of Sc and other elements.The matters needing attention and the contents needing further study in future research are analyzed and discussed.
KeyWords AITranslate
1高文理,王帅,朱聪聪,毛郭灵,王璀.不同Cd含量对Al-Cu合金组织与性能的影响[J].湖南大学学报:自然科学版,2019,46(6):11-17. 被引量:1
2王璀,王帅,高文理.铸造方法对ZL205A-0.1%Sc合金组织和力学性能的影响[J].稀有金属与硬质合金,2019,47(6):37-41. 被引量:3
3梁文杰,潘青林,朱朝明,何运斌,刘元斐,尹志民.微量Sc对Al-Cu-Li-Zr合金的微观组织和拉伸性能的影响[J].稀有金属材料与工程,2006,35(4):550-553. 被引量:12
4潘青林,尹志民,邹景霞,陈显明,张传福.微量Sc在Al-Mg合金中的作用[J].金属学报,2001,37(7):749-753. 被引量:45
5徐国富,聂祚仁,金头男,荣莉,阮海琼,尹志民.Microstructure and properties of Al-4 Cu alloy containing Sc[J].中国有色金属学会会刊:英文版,2004,14(1):63-66. 被引量:3
6刘闪光,李国爱,罗传彪,李海超,陆政,戴圣龙.Sc元素对ZL205A合金组织和力学性能的影响[J].材料工程,2020,48(1):84-91. 被引量:5
7毛建伟,金头男,徐国富.含钪Al-Cu合金的显微组织[J].中国有色金属学报,2005,15(6):923-928. 被引量:14
8徐国富,牟申周,尹志民.微量Sc对Al-3.0%Cu合金时效硬化及析出行为的影响[J].矿冶工程,2006,26(2):92-95. 被引量:4
9徐国富,金头男,邹景霞,尹志民,聂祚仁.微量Sc元素对Al-Cu合金组织与性能的影响[J].材料热处理学报,2004,25(2):15-18. 被引量:11
1张新,徐宏,陈彤,王长顺,王延龙,徐兰军,李宏伟.新型液态模锻Al-Cu合金的成型性能和微观组织[J].中南大学学报:英文版,2022,29(1):60-79. 被引量:4
2平淡.不走寻常路 用活PPT圆柱形状[J].电脑爱好者,2022(6):46-47.
3董明晔,赵玥,李权,王福德,吴爱萍.焊丝中Cd元素的添加对电弧增材制造Al-Cu合金显微组织和力学性能的影响[J].中国有色金属学报:英文版,2022,32(3):750-764.
4吴雁,郭立新,肖礼军,李朝阳,孙士学.铜铝异种金属激光焊接焊缝成形和组织[J].兵器材料科学与工程,2022,45(1):66-69.
5温从剑,王政,张子越.位置伺服电机系统的鲁棒性模型预测控制[J].电气工程学报,2021,16(4):59-67.
6罗忠涛,王亚洲,王振华,田崇霏,包文忠,崔寅亮.缓凝剂复掺对磷酸镁水泥性能的影响[J].武汉理工大学学报,2019,41(5):7-11. 被引量:1
7辛叶春,徐伟,赵东杨,张波.超细层片结构Al-4%Cu合金的点蚀行为[J].中国腐蚀与防护学报,2022,42(2):274-280.
8陶扬,罗宇旭,刘清,刘晓芳,向明武,郭俊明.Cr掺杂尖晶石型LiMn_(2)O_(4)正极材料的研究进展[J].化工新型材料,2022,50(2):74-80.
9李广慧,周敏,李东南,赖茂椿,杨春蓉,陈跃娟.氧化铝陶瓷低温烧结研究[J].福建建筑,2022(2):56-59. 被引量:2
10王颖.破碎与重塑——立体主义对中国当代艺术创作的积极影响[J].美术文献,2021(11):52-53. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]
Citation Information:
In view of the excellent comprehensive properties of Al-Cu alloys,the research progress of the effects of Sc and the combined addition of Sc and other elements in Al-Cu alloys at home and abroad is re-viewed,which include the changes of grain size,phase composition and distribution,physical and mechani-cal properties of Al-Cu alloys after the addition of Sc or the combined addition of Sc and other elements.The matters needing attention and the contents needing further study in future research are analyzed and discussed.
quote
| GB/T 7714-2015 | [1] ZHONG Li-wei, WANG Jian, DING Xi-xi, et al. Research Progress of the Role of Sc in Al-Cu Alloys[J]. Rare Metals and Cemented Carbides, 2022(1): 52-56. |
| MLA | [1] ZHONG Li-wei, et al., "Research Progress of the Role of Sc in Al-Cu Alloys." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 52-56. |
| APA | [1] ZHONG Li-wei, WANG Jian, DING Xi-xi, FENG Zhao-hui, GAO Wen-li, & MAO Guo-ling. (2022). Research Progress of the Role of Sc in Al-Cu Alloys. Rare Metals and Cemented Carbides(1), 52-56. |
| IEEE | [1] ZHONG Li-wei, WANG Jian, DING Xi-xi, FENG Zhao-hui, GAO Wen-li, and MAO Guo-ling, "Research Progress of the Role of Sc in Al-Cu Alloys," Rare Metals and Cemented Carbides, no. 1, pp. 52-56, 2022. keywords: {Al-Cu alloy;Sc;θ′-Al2Cu phase;Al3Sc phase} |