daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Stretchable Phosphor/Boron Nitride Nanosheet/Polydimethylsiloxane Films for Thermal Management and Rapid Monitoring AITranslate

Qingdao University; Qingdao University; Qingdao University; Qingdao University; Qingdao University; Qingdao University; Qingdao University; Ocean University of China; PR China|Weihai Innovation Research Institute of Qingdao University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the integration, miniaturization, and increasing power density of electrical equipment and electronic devices, thermal management and real-time monitoring of the surface temperature variation are of importance. In this work, we present nanocomposite films based on NaNbO3:Pr3+ (NNOP) and hexagonal boron nitride nanosheets (BNNSs), and polydimethylsiloxane (PDMS) was adopted as a substrate. The sample demonstrated outstanding flexibility and elasticity as well as improved thermal management capability. Importantly, it displayed a fast response to the surface temperature of electrical equipment and electronic devices due to the thermally conductive networks constructed by BNNSs. As a result, under the same thermal stimulus, the luminescence from the sample occurred earlier compared to that without BNNSs, and it can be used for real-time monitoring of the surface temperature of electrical equipment and electronic devices, even under rolled and stretched states. We hope that our nanocomposite film has potential for the increasing thermal management and safety monitoring of modern devices and equipment.

KeyWords AITranslate

stretchability composite films thermal management thermoluminescence safe monitor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01793

Chinese Library Classification Number:

Citation Information:

With the integration, miniaturization, and increasing power density of electrical equipment and electronic devices, thermal management and real-time monitoring of the surface temperature variation are of importance. In this work, we present nanocomposite films based on NaNbO3:Pr3+ (NNOP) and hexagonal boron nitride nanosheets (BNNSs), and polydimethylsiloxane (PDMS) was adopted as a substrate. The sample demonstrated outstanding flexibility and elasticity as well as improved thermal management capability. Importantly, it displayed a fast response to the surface temperature of electrical equipment and electronic devices due to the thermally conductive networks constructed by BNNSs. As a result, under the same thermal stimulus, the luminescence from the sample occurred earlier compared to that without BNNSs, and it can be used for real-time monitoring of the surface temperature of electrical equipment and electronic devices, even under rolled and stretched states. We hope that our nanocomposite film has potential for the increasing thermal management and safety monitoring of modern devices and equipment.

quote

GB/T 7714-2015 [1] Tianshuo Li, Xin Li, Zongtao Chi, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01793.
MLA [1] Tianshuo Li, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01793.
APA [1] Tianshuo Li, Xin Li, Zongtao Chi, Longxiang Cheng, Qiaoli Wang, Huibao Chen, Yu Liu, JunCheng Zhang, & Bin Sun. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01793
IEEE [1] Tianshuo Li, Xin Li, Zongtao Chi, Longxiang Cheng, Qiaoli Wang, Huibao Chen, Yu Liu, JunCheng Zhang, and Bin Sun, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01793. keywords: {stretchability;composite films;thermal management;thermoluminescence;safe monitor}