Liquid-Crystalline Naphthalene and Perylene Bisimides with a D2–π2–A Architecture for High-Mobility Organic Field-Effect Transistors Liquid-Crystalline Naphthalene and Perylene Bisimides with a D2–π2–A Architecture for High-Mobility Organic Field-Effect Transistors AITranslate
Abstract AITranslate
We designed and synthesized four naphthalene and perylene bisimide-based imidazole-containing liquid-crystalline (NI and PI) derivatives based on a donor−π–acceptor−π–donor (D2–π2–A) architecture. These compounds bear 10 flexible peripheral chains to ensure liquid crystallinity and solution processability making them suitable to use as organic semiconductors. All four compounds stabilized different columnar phases. Higher thermal stability and lower band gaps were also observed in both NI and PI derivatives. NI derivatives showed larger Stokes shifts, while PI derivatives exhibited very high molar extinction coefficients. Two solution-processable liquid-crystalline compounds (NI-12 and PI-12) were utilized for the fabrication of organic field-effect transistors, exhibiting a hole mobility of 1.99 cm2/V·s for NI-12 and 0.63 cm2/V·s for PI-12 derivatives at room temperature in normal air conditions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00179
Chinese Library Classification Number:
Citation Information:
We designed and synthesized four naphthalene and perylene bisimide-based imidazole-containing liquid-crystalline (NI and PI) derivatives based on a donor−π–acceptor−π–donor (D2–π2–A) architecture. These compounds bear 10 flexible peripheral chains to ensure liquid crystallinity and solution processability making them suitable to use as organic semiconductors. All four compounds stabilized different columnar phases. Higher thermal stability and lower band gaps were also observed in both NI and PI derivatives. NI derivatives showed larger Stokes shifts, while PI derivatives exhibited very high molar extinction coefficients. Two solution-processable liquid-crystalline compounds (NI-12 and PI-12) were utilized for the fabrication of organic field-effect transistors, exhibiting a hole mobility of 1.99 cm2/V·s for NI-12 and 0.63 cm2/V·s for PI-12 derivatives at room temperature in normal air conditions.
quote
| GB/T 7714-2015 | [1] Vinod Kumar Vishwakarma, Mrinmoy Roy, Rajan Singh, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00179. |
| MLA | [1] Vinod Kumar Vishwakarma, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00179. |
| APA | [1] Vinod Kumar Vishwakarma, Mrinmoy Roy, Rajan Singh, Doddamane Sreenivasamurthy Shankar Rao, Roy Paily, & Achalkumar Ammathnadu Sudhakar. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00179 |
| IEEE | [1] Vinod Kumar Vishwakarma, Mrinmoy Roy, Rajan Singh, Doddamane Sreenivasamurthy Shankar Rao, Roy Paily, and Achalkumar Ammathnadu Sudhakar, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00179. keywords: {naphthalene bisimides perylene bisimides liquid crystals selfassembly organic fieldeffect transistors hole mobilityShow More} |