Siloxane Side-Chain-Modified Diketopyrrolopyrrole and Thienopyrrole Containing Small Molecules for Organic Field-Effect Transistors Siloxane Side-Chain-Modified Diketopyrrolopyrrole and Thienopyrrole Containing Small Molecules for Organic Field-Effect Transistors AITranslate
Abstract AITranslate
Thieno[3,2-b]pyrrole (TP) is a donor moiety employed in organic semiconducting small molecules and polymers. Among the TP-containing small molecules reported, benzo[c][1,2,5]thiadiazole (BT) acceptor-based donor–acceptor (DA) type molecules have shown mobilities of ∼0.1 cm2 V–1 s–1. In this study, we are reporting the synthesis, characterization, and testing of the organic field-effect transistor (OFET) performance of two donor–acceptor–donor (DAD) type small molecules with TP donors and siloxane-functionalized diketopyrrolopyrrole (DPP) acceptors, namely, diethyl 2,2′-((2,5-bis(6-(1,1,1,3,5,5,5-heptamethyltrisiloxan-3-yl)hexyl)-3,6-dioxo-2,3,5,6-tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)bis(thiophene-5,2-diyl))bis(4-methyl-4H-thieno[3,2-b]pyrrole-5-carboxylate (DPP-2T-2TP) and diethyl 2,2′-((2,5-bis(6-(1,1,1,3,5,5,5-heptamethyltrisiloxan-3-yl)hexyl)-3,6-dioxo-2,3,5,6 tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)bis(furan-5,2-diyl))bis(4-methyl-4H-thieno[3,2-b]pyrrole-5-carboxylate (DPP-2F-2TP). The difference between DPP-2T-2TP and DPP-2F-2TP is the spacer between the donor and acceptor. According to a few reports, siloxane-containing side chains were known to provide stability in ambient conditions in OFETs compared to their alkyl-substituted analogs. In this study, siloxane side-chain-substituted small molecular OFETs were fabricated, annealed, and tested under ambient conditions. Both molecules showed OFET activity with a maximum hole mobility of 4.10 × 10–2 cm2 V–1 s–1 (DPP-2T-2TP) and 6.40 × 10–5 (DPP-2F-2TP) cm2 V–1 s–1 in ambient conditions, where thiophene spacer containing DPP-2T-2TP had a better performance.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01033
Chinese Library Classification Number:
Citation Information:
Thieno[3,2-b]pyrrole (TP) is a donor moiety employed in organic semiconducting small molecules and polymers. Among the TP-containing small molecules reported, benzo[c][1,2,5]thiadiazole (BT) acceptor-based donor–acceptor (DA) type molecules have shown mobilities of ∼0.1 cm2 V–1 s–1. In this study, we are reporting the synthesis, characterization, and testing of the organic field-effect transistor (OFET) performance of two donor–acceptor–donor (DAD) type small molecules with TP donors and siloxane-functionalized diketopyrrolopyrrole (DPP) acceptors, namely, diethyl 2,2′-((2,5-bis(6-(1,1,1,3,5,5,5-heptamethyltrisiloxan-3-yl)hexyl)-3,6-dioxo-2,3,5,6-tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)bis(thiophene-5,2-diyl))bis(4-methyl-4H-thieno[3,2-b]pyrrole-5-carboxylate (DPP-2T-2TP) and diethyl 2,2′-((2,5-bis(6-(1,1,1,3,5,5,5-heptamethyltrisiloxan-3-yl)hexyl)-3,6-dioxo-2,3,5,6 tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)bis(furan-5,2-diyl))bis(4-methyl-4H-thieno[3,2-b]pyrrole-5-carboxylate (DPP-2F-2TP). The difference between DPP-2T-2TP and DPP-2F-2TP is the spacer between the donor and acceptor. According to a few reports, siloxane-containing side chains were known to provide stability in ambient conditions in OFETs compared to their alkyl-substituted analogs. In this study, siloxane side-chain-substituted small molecular OFETs were fabricated, annealed, and tested under ambient conditions. Both molecules showed OFET activity with a maximum hole mobility of 4.10 × 10–2 cm2 V–1 s–1 (DPP-2T-2TP) and 6.40 × 10–5 (DPP-2F-2TP) cm2 V–1 s–1 in ambient conditions, where thiophene spacer containing DPP-2T-2TP had a better performance.
quote
| GB/T 7714-2015 | [1] Chinthaka M. Udamulle Gedara, Ziyuan Ma, Md Muktadir Talukder, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01033. |
| MLA | [1] Chinthaka M. Udamulle Gedara, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01033. |
| APA | [1] Chinthaka M. Udamulle Gedara, Ziyuan Ma, Md Muktadir Talukder, Ruwan Gunawardhana, Michael C. Biewer, & Mihaela C. Stefan. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01033 |
| IEEE | [1] Chinthaka M. Udamulle Gedara, Ziyuan Ma, Md Muktadir Talukder, Ruwan Gunawardhana, Michael C. Biewer, and Mihaela C. Stefan, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01033. keywords: {diketopyrrolopyrrole siloxane side chain thieno[3;2b]pyrrole fusedring donor−acceptor small molecules organic fieldeffectShow More} |