In this paper,gallium nitrate was taken as the raw material,gallium oxyhydroxide was successfully prepared by gallium salt precipitation method,and the effects of process parameters such as precipitant type,reaction temperature,pH value and gallium ion concentration on the preparation of gallium oxyhydroxide were systematically investigated.The results show that the precipitation rate of gallium reaches 79.7%,and the precipitated product is white powder of gallium oxyhydroxide under the optimal conditions of ammonia as precipitant,reaction temperature of 70℃,pH value of 8,and gallium ion concentration of 0.16 mol/L.Theβ-Ga2O3powder with uniform morphology and conforming to the Ga2O33N standard in YS/T 741—2010 can be prepared by roasting the precipitated product at 800℃for 3 h.In this study,gallium nitrate can be efficiently converted into gallium oxyhydroxide with homogeneous morphology and size by gallium salt precipitation method,with simple process flow,low production cost,and prospect for industrialization.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TF843.1[冶金工程]
Citation Information:
In this paper,gallium nitrate was taken as the raw material,gallium oxyhydroxide was successfully prepared by gallium salt precipitation method,and the effects of process parameters such as precipitant type,reaction temperature,pH value and gallium ion concentration on the preparation of gallium oxyhydroxide were systematically investigated.The results show that the precipitation rate of gallium reaches 79.7%,and the precipitated product is white powder of gallium oxyhydroxide under the optimal conditions of ammonia as precipitant,reaction temperature of 70℃,pH value of 8,and gallium ion concentration of 0.16 mol/L.Theβ-Ga2O3powder with uniform morphology and conforming to the Ga2O33N standard in YS/T 741—2010 can be prepared by roasting the precipitated product at 800℃for 3 h.In this study,gallium nitrate can be efficiently converted into gallium oxyhydroxide with homogeneous morphology and size by gallium salt precipitation method,with simple process flow,low production cost,and prospect for industrialization.
quote
| GB/T 7714-2015 | [1] SHEN Le, AI Zhen, QI Li-juan, et al. Research on the Efficient Preparation of Gallium Oxide by Gallium Salt Precipitation Method[J]. Rare Metals and Cemented Carbides, 2025(3): 35-42. |
| MLA | [1] SHEN Le, et al., "Research on the Efficient Preparation of Gallium Oxide by Gallium Salt Precipitation Method." Rare Metals and Cemented Carbides, no. 3, 2025, pp. 35-42. |
| APA | [1] SHEN Le, AI Zhen, QI Li-juan, XU Liang, YANG Cheng, & ZHAO Zhuo. (2025). Research on the Efficient Preparation of Gallium Oxide by Gallium Salt Precipitation Method. Rare Metals and Cemented Carbides(3), 35-42. |
| IEEE | [1] SHEN Le, AI Zhen, QI Li-juan, XU Liang, YANG Cheng, and ZHAO Zhuo, "Research on the Efficient Preparation of Gallium Oxide by Gallium Salt Precipitation Method," Rare Metals and Cemented Carbides, no. 3, pp. 35-42, 2025. keywords: {precipitation method;efficient preparation;roasting;gallium nitrate;gallium oxyhydroxide;β-gallium oxide} |