Effects of Rare Earth Content on the Mechanical and Magnetic Properties of Sintered NdFeB Magnets AITranslate
Abstract AITranslate
The magnetic properties, microstructure and bending strength of the sintered NdFeB magnets with different rare earth content were studied. The results show that the bending strength, coercivity and demagnetization curve rectangularity of the sintered NdFeB magnets can be effectively enhanced by increas- ing rare earth content,but the remanence will be reduced. SEM images show that increasing rare earth con- tent can effectively improve the microstructure of casting strips and sintered NdFeB magnets, resulting in more uniform and continuous distribution of rare earth-rich phase and enhanced bending strength and coer- civity of sintered NdFeB magnets.
KeyWords AITranslate
1曾振鹏.烧结NdFeB永磁材料的断裂研究[J].稀有金属材料与工程,1996,25(3):18-21. 被引量:25
1柯庆进,许磊,李莎,戎茂华,王江.稀土Y-Fe-B合金的微观组织结构与相转变[J].桂林电子科技大学学报,2020,40(1):77-81.
2张洋湖,贺洪江,左志军,史荣莹,李建军,赵立新,黄光伟,郑立允.Ni对热变形Nd-Fe-B磁体磁性能及力学性能的影响[J].粉末冶金材料科学与工程,2021,26(1):40-46.
3张建华,李永峰,刘艳丽.晶界添加Pr-Cu对烧结Nd-La-Ce-Fe-B磁体磁性能和微观结构的影响[J].稀有金属与硬质合金,2022,50(1):57-62.
4胡利光,宋春燕,王书桓,赵定国,程世伟.稀土合金渗氮处理研究进展[J].稀有金属与硬质合金,2019,47(2):36-38. 被引量:1
5郭克星,夏鹏举.稀土镁变质对金属型铸造高铬铸铁Cr26耐磨性的影响[J].稀有金属与硬质合金,2019,47(2):39-44. 被引量:3
1王松,张卫红,周啸颖,王建刚.淬火回火工艺对高碳热磨片显微组织及耐磨性的影响[J].河北科技大学学报,2020,41(6):537-543. 被引量:5
2白公民.20CrMnTi钢表面稀土硼碳共渗层组织及性能[J].金属加工:热加工,2021(1):73-76. 被引量:1
3宋延沛,陈丹萍,周汉,林小丽,李丽.热处理工艺对Cr15Ni2MnMoCuNbRE铸钢组织及性能的影响[J].金属热处理,2022,47(2):178-182. 被引量:1
4郭克星.高铬铸铁耐磨性研究的进展[J].热处理,2023,38(1):1-5.
1谢珊珊,李慧,霍东兴,李亚敏.6.5%Si及梯度硅钢的制备工艺[J].热加工工艺,2017,46(18):39-42.
2氢对NdFeB磁体的增塑作用[J].金属功能材料,2017,24(4):38-38.
3钟林生,杜德诚.赣南脐橙果园土壤中稀土元素的检测[J].安徽农学通报,2017,23(18):12-12.
4张书琦,李鹏,徐征宇,汤浩,李金忠,仇宇舟,刘雪丽.特高压变压器用硅钢片应用磁性能的评估[J].中国电机工程学报,2017,37(18):5511-5518. 被引量:4
5邹姝颖,钟喜春,刘仲武,张翼飞,王开祥.V_2O_5掺杂改善锰锌铁氧体组织及性能的研究[J].电子元件与材料,2017,36(10):27-30.
6洪承志,谢质彬,韩改田.大型覆盖件有限元分析及结构优化设计研究[J].机械制造,2017,55(9):48-52.
7熊吉磊,潘顺康,成丽春,林培豪,姚青荣,范雨龙.Dy对Pr_2Fe_(17)合金微波吸收特性的影响(英文)[J].稀有金属材料与工程,2017,46(8):2060-2064. 被引量:1
8杨泽林,张世富,李洪,胡永攀,杨东宇.海上装配式输油管道连接处强度分析[J].重庆理工大学学报:自然科学,2017,31(9):68-72.
9徐龙凤.关于中职语文教学的定位研究[J].考试周刊,2017,0(78):40-41.
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
The magnetic properties, microstructure and bending strength of the sintered NdFeB magnets with different rare earth content were studied. The results show that the bending strength, coercivity and demagnetization curve rectangularity of the sintered NdFeB magnets can be effectively enhanced by increas- ing rare earth content,but the remanence will be reduced. SEM images show that increasing rare earth con- tent can effectively improve the microstructure of casting strips and sintered NdFeB magnets, resulting in more uniform and continuous distribution of rare earth-rich phase and enhanced bending strength and coer- civity of sintered NdFeB magnets.
quote
| GB/T 7714-2015 | [1] CHEN Yun-zhi, LIU Yu-hui, WANG Zhi-jian, et al. Effects of Rare Earth Content on the Mechanical and Magnetic Properties of Sintered NdFeB Magnets[J]. Rare Metals and Cemented Carbides, 2017(4): 52-55. |
| MLA | [1] CHEN Yun-zhi, et al., "Effects of Rare Earth Content on the Mechanical and Magnetic Properties of Sintered NdFeB Magnets." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 52-55. |
| APA | [1] CHEN Yun-zhi, LIU Yu-hui, WANG Zhi-jian, ZHU Wang-wei, PENG Yan, & WANG Chuan. (2017). Effects of Rare Earth Content on the Mechanical and Magnetic Properties of Sintered NdFeB Magnets. Rare Metals and Cemented Carbides(4), 52-55. |
| IEEE | [1] CHEN Yun-zhi, LIU Yu-hui, WANG Zhi-jian, ZHU Wang-wei, PENG Yan, and WANG Chuan, "Effects of Rare Earth Content on the Mechanical and Magnetic Properties of Sintered NdFeB Magnets," Rare Metals and Cemented Carbides, no. 4, pp. 52-55, 2017. keywords: {sintered NdFeB magnet;rare earth content;magnetic property;mechanical property;microstruc- ture;bending strength} |