daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Magnetic Polymer Actuators with Self-Sensing Resistive Bending Response Based on Ternary Polymer Composites Magnetic Polymer Actuators with Self-Sensing Resistive Bending Response Based on Ternary Polymer Composites AITranslate

BCMaterials, Basque Center for Materials; University of Minho;BCMaterials, Basque Center for Materials; Universidad del País Vasco (UPV/EHU); University of Minho; University of Minho
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A multifunctional polymer-based composite has been designed based on poly(vinylidene fluoride) (PVDF) as polymer matrix and cobalt ferrite (CoFe2O4, CFO) and multiwalled carbon nanotubes (MWCNTs) as fillers, allowing to combine magnetic and electrical responses. The composites were prepared by solvent casting with a fixed 20 wt % concentration of CFO and varying the MWCNTs content between 0 and 3 wt %, allowing to tailor the electrical behavior. The morphology, polymer phase, and thermal and magnetic properties are nearly independent of the MWCNT filler content within the polymer matrix. On the other hand, the mechanical and electrical properties strongly depend on the MWCNT content and a maximum d.c. electrical conductivity value of 4 × 10–4 S·cm–1 has been obtained for the 20 wt %CFO-3 wt %MWCNT/PVDF sample, which is accompanied by an 11.1 emu·g–1 magnetization. The suitability of this composite for magnetic actuators with self-sensing strain characteristics is demonstrated with excellent response and reproducibility.

KeyWords AITranslate

multifunctional composites PVDF magnetic actuator resistive sensors strain sensors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00432

Chinese Library Classification Number:

Citation Information:

A multifunctional polymer-based composite has been designed based on poly(vinylidene fluoride) (PVDF) as polymer matrix and cobalt ferrite (CoFe2O4, CFO) and multiwalled carbon nanotubes (MWCNTs) as fillers, allowing to combine magnetic and electrical responses. The composites were prepared by solvent casting with a fixed 20 wt % concentration of CFO and varying the MWCNTs content between 0 and 3 wt %, allowing to tailor the electrical behavior. The morphology, polymer phase, and thermal and magnetic properties are nearly independent of the MWCNT filler content within the polymer matrix. On the other hand, the mechanical and electrical properties strongly depend on the MWCNT content and a maximum d.c. electrical conductivity value of 4 × 10–4 S·cm–1 has been obtained for the 20 wt %CFO-3 wt %MWCNT/PVDF sample, which is accompanied by an 11.1 emu·g–1 magnetization. The suitability of this composite for magnetic actuators with self-sensing strain characteristics is demonstrated with excellent response and reproducibility.

quote

GB/T 7714-2015 [1] Ander García Díez, Nelson Pereira, Carmen R. Tubio, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00432.
MLA [1] Ander García Díez, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00432.
APA [1] Ander García Díez, Nelson Pereira, Carmen R. Tubio, Jose Luis VilasVilela, Carlos M. Costa, & Senentxu LancerosMendez. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00432
IEEE [1] Ander García Díez, Nelson Pereira, Carmen R. Tubio, Jose Luis VilasVilela, Carlos M. Costa, and Senentxu LancerosMendez, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00432. keywords: {multifunctional composites PVDF magnetic actuator resistive sensors strain sensors}