daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Regulating the Molecular Shape of Nonfused Electron Acceptors Enables Efficient Organic Solar Cells AITranslate

Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; East China Normal University; Donghua University; Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonfused electron acceptor based organic solar cells (OSCs) have garnered increasing curiosity, because of their simple synthetic route and versatile chemical modification capabilities. However, nonfused acceptors with varying molecular symmetries have rarely been explored, and their structure–property–performance relationship remains unclear. In this work, two nonfused acceptors, namely, DTBDT-4Cl and DTBTT-4Cl with different molecular shapes, were synthesized and systematically investigated. The asymmetric acceptor DTBTT-4Cl with a C-shape molecular backbone exhibits more compact π–π stacking and higher crystallinity than the centrosymmetric S-shape acceptor DTBDT-4Cl. Remarkably, a promising power conversion efficiency (PCE) of 13.8% with a the open-circuit voltage (VOC) as high as 0.916 V, a short-circuit current density (JSC) of 21.9 mA cm–2, and a fill factor (FF) of 68.5% was achieved, which significantly surpasses 11.3% for the DTBDT-4Cl-based devices. The enhanced performance could primarily be attributed to the enhanced intermolecular interactions, improved charge transfer, and suppressed charge recombination. These findings underscore the importance of precise control of the molecular shape through rational molecular design represents an effective strategy for adjusting the miscibility and thus the photovoltaic performance of nonfused electron acceptor-based OSCs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01020

Chinese Library Classification Number:

Citation Information:

Nonfused electron acceptor based organic solar cells (OSCs) have garnered increasing curiosity, because of their simple synthetic route and versatile chemical modification capabilities. However, nonfused acceptors with varying molecular symmetries have rarely been explored, and their structure–property–performance relationship remains unclear. In this work, two nonfused acceptors, namely, DTBDT-4Cl and DTBTT-4Cl with different molecular shapes, were synthesized and systematically investigated. The asymmetric acceptor DTBTT-4Cl with a C-shape molecular backbone exhibits more compact π–π stacking and higher crystallinity than the centrosymmetric S-shape acceptor DTBDT-4Cl. Remarkably, a promising power conversion efficiency (PCE) of 13.8% with a the open-circuit voltage (VOC) as high as 0.916 V, a short-circuit current density (JSC) of 21.9 mA cm–2, and a fill factor (FF) of 68.5% was achieved, which significantly surpasses 11.3% for the DTBDT-4Cl-based devices. The enhanced performance could primarily be attributed to the enhanced intermolecular interactions, improved charge transfer, and suppressed charge recombination. These findings underscore the importance of precise control of the molecular shape through rational molecular design represents an effective strategy for adjusting the miscibility and thus the photovoltaic performance of nonfused electron acceptor-based OSCs.

quote

GB/T 7714-2015 [1] Jiaoyu Xu, Kexin Yu, Wenting Liang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c01020.
MLA [1] Jiaoyu Xu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c01020.
APA [1] Jiaoyu Xu, Kexin Yu, Wenting Liang, Cuifen Zhang, Xiaoli Zhou, Rongna Lyu, Shenbo Zhu, Yongjie Cui, Xueliang Shi, Fengkun Chen, Zaifei Ma, Yangen Huang, & Huawei Hu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c01020
IEEE [1] Jiaoyu Xu, Kexin Yu, Wenting Liang, Cuifen Zhang, Xiaoli Zhou, Rongna Lyu, Shenbo Zhu, Yongjie Cui, Xueliang Shi, Fengkun Chen, Zaifei Ma, Yangen Huang, and Huawei Hu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c01020.