Drift-and-fill mining under cemented paste backfill for sill pillar recovery at Olympias mine AITranslate
Abstract AITranslate
At Olympias Underground Mine,drift-and-fill mining under the cemented paste backfill is required for the safe and effective recovery of sill pillars within complex geology and variable ground conditions.Cured cemented paste backfill provides critical confinement to the surrounding rock,enabling controlled blasting and reducing the risk of instability during mining.This case study reviews operational practices and design considerations specific to Olympias Mine,including geomechanics and geotechnical aspects of mining with paste backfill,paste fill strength requirements and quality control,curing times,blast sequencing,and the integration of ground support systems.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TD803[矿业工程—矿山开采]
Citation Information:
At Olympias Underground Mine,drift-and-fill mining under the cemented paste backfill is required for the safe and effective recovery of sill pillars within complex geology and variable ground conditions.Cured cemented paste backfill provides critical confinement to the surrounding rock,enabling controlled blasting and reducing the risk of instability during mining.This case study reviews operational practices and design considerations specific to Olympias Mine,including geomechanics and geotechnical aspects of mining with paste backfill,paste fill strength requirements and quality control,curing times,blast sequencing,and the integration of ground support systems.
quote
| GB/T 7714-2015 | [1] Eirini Psychari, Ourania Mousli, Dimosthenis Koskiniotis, et al. MetaResource, 2026(1): 32-46. |
| MLA | [1] Eirini Psychari, et al., MetaResource, no. 1, 2026, pp. 32-46. |
| APA | [1] Eirini Psychari, Ourania Mousli, Dimosthenis Koskiniotis, & Mehmet Yumlu. (2026). MetaResource(1), 32-46. |
| IEEE | [1] Eirini Psychari, Ourania Mousli, Dimosthenis Koskiniotis, and Mehmet Yumlu, MetaResource, no. 1, pp. 32-46, 2026. |