Uniformly Dispersed Poly(lactic acid)-Grafted Lignin Nanoparticles Enhance Antioxidant Activity and UV-Barrier Properties of Poly(lactic acid) Packaging Films AITranslate
Abstract AITranslate
Poly(lactic acid) (PLA) represents one of the most widely used biodegradable polymers for food packaging applications. While this material provides many advantages, it is characterized by limited antioxidant and UV-barrier properties. Blending PLA with lignin is an attractive strategy to address these limitations. Lignin possesses antioxidant properties and absorbs UV-light and is a widely available low value byproduct of the paper and pulp industry. This study has explored the use of lignin nanoparticles to augment the properties of PLA-based films. A central challenge in the preparation of PLA–lignin nanoparticle blend films is to avoid nanoparticle aggregation, which could compromise optical properties as well as antioxidant activity, among others. To avoid nanoparticle aggregation in the PLA matrix, PLA-grafted lignin nanoparticles were prepared via organocatalyzed lactide ring-opening polymerization. In contrast to lignin and unmodified lignin nanoparticles, these PLA-grafted lignin nanoparticles could be uniformly dispersed in PLA for lignin contents up to 10 wt %. The addition of as little as the equivalent of 1 wt % of lignin of these nanoparticles effectively blocked transmission of 280 nm UV-light. At the same time, these blend films retained reasonable visible light transmittance. The optical properties of the PLA lignin blend films also benefited from the well-dispersed nature of the PLA-grafted nanoparticles, as evidenced by significantly higher visible light transmittance of blends of PLA and PLA-grafted nanoparticles, as compared to blends prepared from PLA with lignin or unmodified lignin nanoparticles. Finally, blending PLA with PLA-grafted lignin nanoparticles greatly augments the antioxidant activity of these films.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00420
Chinese Library Classification Number:
Citation Information:
Poly(lactic acid) (PLA) represents one of the most widely used biodegradable polymers for food packaging applications. While this material provides many advantages, it is characterized by limited antioxidant and UV-barrier properties. Blending PLA with lignin is an attractive strategy to address these limitations. Lignin possesses antioxidant properties and absorbs UV-light and is a widely available low value byproduct of the paper and pulp industry. This study has explored the use of lignin nanoparticles to augment the properties of PLA-based films. A central challenge in the preparation of PLA–lignin nanoparticle blend films is to avoid nanoparticle aggregation, which could compromise optical properties as well as antioxidant activity, among others. To avoid nanoparticle aggregation in the PLA matrix, PLA-grafted lignin nanoparticles were prepared via organocatalyzed lactide ring-opening polymerization. In contrast to lignin and unmodified lignin nanoparticles, these PLA-grafted lignin nanoparticles could be uniformly dispersed in PLA for lignin contents up to 10 wt %. The addition of as little as the equivalent of 1 wt % of lignin of these nanoparticles effectively blocked transmission of 280 nm UV-light. At the same time, these blend films retained reasonable visible light transmittance. The optical properties of the PLA lignin blend films also benefited from the well-dispersed nature of the PLA-grafted nanoparticles, as evidenced by significantly higher visible light transmittance of blends of PLA and PLA-grafted nanoparticles, as compared to blends prepared from PLA with lignin or unmodified lignin nanoparticles. Finally, blending PLA with PLA-grafted lignin nanoparticles greatly augments the antioxidant activity of these films.
quote
| GB/T 7714-2015 | [1] Alice Boarino, Aigoul Schreier, Yves Leterrier, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00420. |
| MLA | [1] Alice Boarino, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00420. |
| APA | [1] Alice Boarino, Aigoul Schreier, Yves Leterrier, & HarmAnton Klok. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00420 |
| IEEE | [1] Alice Boarino, Aigoul Schreier, Yves Leterrier, and HarmAnton Klok, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00420. keywords: {poly(lactic acid);lignin nanoparticles;food packaging;antioxidant;UVbarrier} |