Abstract AITranslate

β-phase content of the α+β type Ti-6Al-4V sheet can be increased through deuterium treatment under 0.1 MPa hydrogen atmosphere.And the alloy grain size can be reduced.The alloy with deuterium absorption 0.5% (mass/percentage) is stripped at 973K temperature and grain size is reduced from initial 20 micro meter down to 1~3 micro meter when the stripping temperature goes down to 873k to obtain fine and super-fine Ti alloy.The testing results showed that the alloy's mechanical property such as super-plastic elongation,etc is increased with the reduction of the grain size.

KeyWords AITranslate

Ti alloy deuterium treatment ultra-fine grain mechanical property

1Nakahigashi J, et al.Ultra- fine grain and tensile properties of titanitun alloys obtained through prvtitun treatment[J]. Journal of Alloys and Compounds, 2002, 330:384.

2Kimetal J S. Analysis on botmdary sliding and its accommodation rrxxte during superplastic deformation of two- phase Ti -6Al - 4V alloy[J] .Metals and Materials, 1998,29(1) :217.

1李东,赵永庆.钛合金晶粒细化研制进展[J].材料导报,2005,19(F11):421-422. 被引量:6

2金秋亚,黄继华,侯金保,张蕾,滕俊飞.细晶钛合金的制备方法[J].航天制造技术,2006(5):44-46. 被引量:5

3曾立英,赵永庆,李倩.钛合金低温超塑性的研究进展[J].热加工工艺,2006,35(22):61-65. 被引量:13

4孙前江,王高潮,李淼泉.细化晶粒对钛合金超塑性的影响[J].材料导报,2010,24(17):126-129. 被引量:7

5王苗,杨延清,罗贤.超细晶钛合金的制备及性能研究现状[J].材料导报,2013,27(13):94-98. 被引量:7

1刘奇先,刘杨,高凯.钛合金的研究进展与应用[J].航天制造技术,2011(4):45-48. 被引量:34

2王荣华,陈明和,陈国亮,范平,李枫,周兆锋.TC4钛合金盒形件超塑成形工艺[J].热加工工艺,2008,37(11):46-48. 被引量:9

3赵文娟,丁桦,曹富荣,赵敬伟,张亚玲,侯红亮.Ti6Al4V合金的低温超塑性拉伸变形行为[J].材料研究学报,2008,22(3):269-273. 被引量:10

4张鹏省,曾卫东,赵永庆.钛及钛合金热氢处理技术[J].热加工工艺,2009,38(12):133-136. 被引量:1

5李成清,王树林.机械合金化制备纳米钛-锆合金的研究进展[J].中国材料进展,2009,28(7):67-71. 被引量:2

6李成清,王树林.纳米钛-锆合金制备技术的研究进展[J].材料导报:纳米与新材料专辑,2009,23(2):9-11.

7吴晨刚,王高潮,董洪波,耿启冬.TA15钛合金的超塑性研究及组织变化[J].热加工工艺,2009,38(24):5-7. 被引量:1

8孙前江,王高潮,李淼泉.细化晶粒对钛合金超塑性的影响[J].材料导报,2010,24(17):126-129. 被引量:7

9张田,张永康,任旭东,姜大伟,皇甫喁卓,阮亮.渗铝激光冲击复合处理对00Cr12合金钢高温拉伸性能的影响[J].金属热处理,2012,37(2):92-95. 被引量:1

10徐烽,颜银标.多向锻造法细化钛及钛合金晶粒的研究现状[J].钛工业进展,2012,29(2):15-18. 被引量:12

1李吉(摘).通过减小铸坯振痕深度使铸态γ晶粒细化[J].连铸,2008(4):45-45.

2李吉夫.连铸热处理钢所用保护渣的结晶分析[J].连铸,2008(1):26-26.

3李吉夫(摘).连铸用结晶器保护渣结晶过程的分析[J].连铸,2007(5):38-38.

4吴义添,张其昕.四氧化三锰的研制[J].中国锰业,1990(4):38-41. 被引量:18

5康启平,郭世柏.球磨时间和烧结温度对烧结制备钼-铜合金性能的影响[J].机械工程材料,2010,34(10):28-30. 被引量:1

6谈树苹,郝小娟,赵立飞.在线直流辉光放电光源的研制[J].中国原子能科学研究院年报,2008(1):267-267.

7张刚,李劼,赖延清,孙小刚.烧结气氛对Ni-Fe尖晶石陶瓷致密化和导电性能的研究[J].功能材料,2005,36(11):1709-1711. 被引量:6

8胡海波.添加剂对WC-Ni硬质合金组织结构与力学性能的影响[J].稀有金属与硬质合金,2013,41(1):55-59. 被引量:4

9南海娟,吴引江,王琳,王翠翠,佘勃强.几种金属多孔材料在高温硫化氢气氛中的腐蚀性能研究[J].粉末冶金工业,2010,20(6):28-31. 被引量:5

10邱光汉,曾舟山,李益民,林好转,曲选辉,黄伯云.MIM Fe 基合金的合金化强化[J].中国有色金属学报,1997,7(4):119-122. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF125.22[冶金工程—粉末冶金]

Citation Information:

β-phase content of the α+β type Ti-6Al-4V sheet can be increased through deuterium treatment under 0.1 MPa hydrogen atmosphere.And the alloy grain size can be reduced.The alloy with deuterium absorption 0.5% (mass/percentage) is stripped at 973K temperature and grain size is reduced from initial 20 micro meter down to 1~3 micro meter when the stripping temperature goes down to 873k to obtain fine and super-fine Ti alloy.The testing results showed that the alloy's mechanical property such as super-plastic elongation,etc is increased with the reduction of the grain size.

quote

GB/T 7714-2015 [1] YANG Yang. Mechanical Property and Preparation of Fine and Ultra-fineTi Alloythrough Deuterium Treatment[J]. Rare Metals and Cemented Carbides, 2005(1): 57-60.
MLA [1] YANG Yang. "Mechanical Property and Preparation of Fine and Ultra-fineTi Alloythrough Deuterium Treatment." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 57-60.
APA [1] YANG Yang. (2005). Mechanical Property and Preparation of Fine and Ultra-fineTi Alloythrough Deuterium Treatment. Rare Metals and Cemented Carbides(1), 57-60.
IEEE [1] YANG Yang, "Mechanical Property and Preparation of Fine and Ultra-fineTi Alloythrough Deuterium Treatment," Rare Metals and Cemented Carbides, no. 1, pp. 57-60, 2005. keywords: {Ti alloy;deuterium treatment;ultra-fine grain;mechanical property}