The Latest Development of Synthesis and Application of NbC AITranslate
Abstract AITranslate
Review is made of the latest development of the main preparation methods of NbC and its application in many fields. It is pointed out that NbC will have wide application in the future in such fields as metallurgy, machinery industry and aerospace technology.
KeyWords AITranslate
1任俊,徐广尧,王文梅.铌[M].南京:南京大学出版社,2001.
2王肇信,幸良佐,曾芳萍.铌钽冶金学[M].北京:稀有金属冶金学会铌钽冶金专业委员会,1998.
3何坤池.超细碳化铌粉的研制生产[A].稀有金属冶金学会1998年年会论文集[C].石嘴山:稀有金属冶金学会,1998.131-134.
4郭伟.一种超细碳化铌粉末的制备方法[P].中国专利:201110145430.9,2011-12-14.
5崔照雯.机械合金化法制备超细碳化铌颗粒的研究[D].石家庄:河北科技大学,2010.
6张浩,朱芳.钽、铌碳化物制备技术的研究进展[J].稀有金属与硬质合金,2009,37(2):47-49. 被引量:8
7boyun huang Academician of Chinese Academy of Engineering,Vice-president of China Association for Science and Technology,Vice-chairmen of China Postdoctoral Science Foundation.Preface[J].中国有色金属学会会刊:英文版,2009,0(S3):527-527. 被引量:57
8Tian D Xia,Zuhair A Munir,Yan L Tang,et al. Struc ture formation in combustion synthesis of Al2O3-NbC composites[J]. J Am Ceram Soc, 2000,83(3) .. 507-512.
9Adnan Goldstein, Ania Singurindi. Al2 O3- NbC based metal cutting tools by microwave sintering followed by hot isotatic pressing[J]. J Am Ceram Soc, 2000, 83 (6):1 530-1 532.
10Barry H Rabin, Gaty E Korth,Richartl L Williamaon. Fabrication of titanium carbide-alumian composites by combustion synthesis and subsequent dynamic consoli- dation[J]. J Am Ceram Soc, 1990,73 (7) : 2 156-2 157.
1蒋玉花,王培.ICP-AES法测定碳化铌中杂质元素[J].硬质合金,2016,33(6):416-422.
2杨家富,陈伟鹏,赵增武,郑坤灿,庞雅丹,赵光进.真空碳热还原制备碳化钛和碳化铌粉体的研究[J].稀有金属与硬质合金,2020,48(4):28-32. 被引量:1
3马晓清,黄丽娜.一步原位制备Nb_(2)O_(5)/NbC复合材料用于高效光催化氧化[J].功能材料,2021,52(11):11169-11176.
4王储,文明,洪汛海,郭靖.机械活化对Nb_(2)O_(5)微波碳热还原的影响[J].有色金属:冶炼部分,2022(2):83-89.
1崔健,张国华.高纯超细碳化钛粉体制备[J].江西冶金,2023,43(4):265-272.
1余娟,常桥稳,谢娇,陈家林,闫智英,叶青松,姜婧,晏彩先,刘伟平.贵金属纳米粒子的常见合成方法及应用[J].贵金属,2013,34(S01):155-160. 被引量:1
2李式模,葛双燕,王群.氢能源的开发和应用(二)[J].低温与特气,1987,5(2):1-7.
3王新龙,贾红兵,李玉桂.有机磷缓蚀剂研究进展[J].腐蚀与防护,2000,21(8):356-358. 被引量:11
4赵树萍.钛合金微弧氧化涂层的相成分及涂层的定向合成[J].国外金属热处理,2003,24(2):23-26. 被引量:6
5陈循介.美国机床市场、数控机床需求与展望[J].机电新产品导报,2005(11):102-105.
6郑贺.光荣与梦想——北京国际宇航空间技术及应用展览会巡礼[J].科学新闻,2001(22):20-20.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
Review is made of the latest development of the main preparation methods of NbC and its application in many fields. It is pointed out that NbC will have wide application in the future in such fields as metallurgy, machinery industry and aerospace technology.
quote
| GB/T 7714-2015 | [1] LIU Yu-bao, LI Lin, ZHANG Xian-heng, et al. The Latest Development of Synthesis and Application of NbC[J]. Rare Metals and Cemented Carbides, 2014(1): 66-69. |
| MLA | [1] LIU Yu-bao, et al., "The Latest Development of Synthesis and Application of NbC." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 66-69. |
| APA | [1] LIU Yu-bao, LI Lin, ZHANG Xian-heng, & ZHAO Er-xiong. (2014). The Latest Development of Synthesis and Application of NbC. Rare Metals and Cemented Carbides(1), 66-69. |
| IEEE | [1] LIU Yu-bao, LI Lin, ZHANG Xian-heng, and ZHAO Er-xiong, "The Latest Development of Synthesis and Application of NbC," Rare Metals and Cemented Carbides, no. 1, pp. 66-69, 2014. keywords: {NbC;preparation;application;composite material;coating material} |