daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Work Function Modulation of Bi/Au Bilayer System toward p-Type WSe2 FET Work Function Modulation of Bi/Au Bilayer System toward p-Type WSe2 FET AITranslate

The University of Tokyo; The University of Tokyo; Saitama University; The University of Tokyo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to attain high-performance p-type field-effect transistors (FETs) based on two-dimensional materials, it becomes imperative to mitigate Fermi level pinning. Employing Bi with a low work function of ∼4.2 eV, characterized by its low melting point, significant vapor pressure, and smaller density of states, has been instrumental in establishing pinning-free n-type contacts. In this context, we present a new approach for establishing p-type contacts. This approach involves the modulation of the effective work function through a bilayer electrode structure comprising ultrathin Bi and a thick Au with a high work function of ∼5.1 eV. The modulation of the effective work function has been clearly confirmed through capacitance─voltage measurements, conducted as a function of the thickness of the Bi layer. Consequent to these findings, a p-type WSe2 Schottky FET was demonstrated employing 2-nm-thick Bi/Au electrodes.

KeyWords AITranslate

IdVg characteristic Fermi level pinning Bismuth C−V measurement WSe2
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01091

Chinese Library Classification Number:

Citation Information:

In order to attain high-performance p-type field-effect transistors (FETs) based on two-dimensional materials, it becomes imperative to mitigate Fermi level pinning. Employing Bi with a low work function of ∼4.2 eV, characterized by its low melting point, significant vapor pressure, and smaller density of states, has been instrumental in establishing pinning-free n-type contacts. In this context, we present a new approach for establishing p-type contacts. This approach involves the modulation of the effective work function through a bilayer electrode structure comprising ultrathin Bi and a thick Au with a high work function of ∼5.1 eV. The modulation of the effective work function has been clearly confirmed through capacitance─voltage measurements, conducted as a function of the thickness of the Bi layer. Consequent to these findings, a p-type WSe2 Schottky FET was demonstrated employing 2-nm-thick Bi/Au electrodes.

quote

GB/T 7714-2015 [1] Ryuichi Nakajima, Tomonori Nishimura, Keiji Ueno, et al. ACS Applied Electronic Materials, 2024(6). DOI:10.1021/acsaelm.3c01091.
MLA [1] Ryuichi Nakajima, et al., ACS Applied Electronic Materials, no. 6, 2024, https://doi.org/10.1021/acsaelm.3c01091.
APA [1] Ryuichi Nakajima, Tomonori Nishimura, Keiji Ueno, & Kosuke Nagashio. (2024). ACS Applied Electronic Materials(6). https://doi.org/10.1021/acsaelm.3c01091
IEEE [1] Ryuichi Nakajima, Tomonori Nishimura, Keiji Ueno, and Kosuke Nagashio, ACS Applied Electronic Materials, no. 6, 2024, doi: 10.1021/acsaelm.3c01091. keywords: {IdVg characteristic Fermi level pinning Bismuth C−V measurement WSe2}