Finely Controlled Synthesis of Zn1–xMgxO Nanoparticles with Uniform Size Distribution Used as Electron Transport Materials for Red QLEDs AITranslate

Zhejiang Normal University; Suzhou Institute of Nano-Tech and Nano-Bionics; Zhejiang Normal University; Zhejiang Normal University; Suzhou Institute of Nano-Tech and Nano-Bionics; Zhejiang Normal University; Suzhou Institute of Nano-Tech and Nano-Bionics;Zhejiang Bright Semiconductor Technology Co.; China University of Mining and Technology; Suzhou Institute of Nano-Tech and Nano-Bionics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this work, we report the finely controlled synthesis of Zn1–xMgxO nanoparticles (NPs) by a Corning advanced-flow reactor (AFR), which produced a uniform size distribution with 75% NPs in the range 3–4 nm with good reproducibility. The Zn1–xMgxO NPs have been applied as an electron transport layer (ETL) in red quantum light-emitting diodes (QLEDs). Different from the traditional method of one-pot synthesis which needs several hours to finish a synthetic cycle, the synthesis by AFR is much faster due to the fast heat and mass transport in the reaction chamber, and a typical synthetic cycle in the AFR needs only a few minutes. Optical properties of the NPs indicate that the Mg ion that substitutes the Zn ion in the ZnO matrix is almost linear with the doping concentration in the solution, which is consistent with the first-principles calculations. The Zn1–xMgxO NPs synthesized with the AFR were subsequently used as the ETL in fabricating red QLEDs, and the resultant performance exceeded that of the device based on the traditional one-pot synthesized NPs. For example, the external quantum efficiency, current efficiency, and power efficiency improved by 25.1%, 21.6%, and 26.9%, respectively. Moreover, better luminescence uniformity was observed in the QLED using the ZnMgO NPs synthesized with the AFR. The device reached an optimal performance when x is 15% in Zn1–xMgxO. The finely controlled synthesis of stable Zn1–xMgxO NPs has the potential in industry application to solve the critical issues of ETLs that impede progress in the mass production of QLEDs.

KeyWords AITranslate

Zn1−xMgxO AFR uniform size distribution QLED electron transport
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00088

Chinese Library Classification Number:

Citation Information:

In this work, we report the finely controlled synthesis of Zn1–xMgxO nanoparticles (NPs) by a Corning advanced-flow reactor (AFR), which produced a uniform size distribution with 75% NPs in the range 3–4 nm with good reproducibility. The Zn1–xMgxO NPs have been applied as an electron transport layer (ETL) in red quantum light-emitting diodes (QLEDs). Different from the traditional method of one-pot synthesis which needs several hours to finish a synthetic cycle, the synthesis by AFR is much faster due to the fast heat and mass transport in the reaction chamber, and a typical synthetic cycle in the AFR needs only a few minutes. Optical properties of the NPs indicate that the Mg ion that substitutes the Zn ion in the ZnO matrix is almost linear with the doping concentration in the solution, which is consistent with the first-principles calculations. The Zn1–xMgxO NPs synthesized with the AFR were subsequently used as the ETL in fabricating red QLEDs, and the resultant performance exceeded that of the device based on the traditional one-pot synthesized NPs. For example, the external quantum efficiency, current efficiency, and power efficiency improved by 25.1%, 21.6%, and 26.9%, respectively. Moreover, better luminescence uniformity was observed in the QLED using the ZnMgO NPs synthesized with the AFR. The device reached an optimal performance when x is 15% in Zn1–xMgxO. The finely controlled synthesis of stable Zn1–xMgxO NPs has the potential in industry application to solve the critical issues of ETLs that impede progress in the mass production of QLEDs.

quote

GB/T 7714-2015 [1] Dawei Qi, Liming Xie, Ming Yang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00088.
MLA [1] Dawei Qi, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00088.
APA [1] Dawei Qi, Liming Xie, Ming Yang, Xiuqing Meng, YuanQiuQiang Yi, Yafei Hao, Wenming Su, Liang Xu, Yanqin Gai, & Zheng Cui. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00088
IEEE [1] Dawei Qi, Liming Xie, Ming Yang, Xiuqing Meng, YuanQiuQiang Yi, Yafei Hao, Wenming Su, Liang Xu, Yanqin Gai, and Zheng Cui, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00088. keywords: {Zn1−xMgxO AFR uniform size distribution QLED electron transport}