Flexible, Breathable, and Hydrophobic Iontronic Tactile Sensors Based on a Nonwoven Fabric Platform for Permeable and Waterproof Wearable Sensing Applications Flexible, Breathable, and Hydrophobic Iontronic Tactile Sensors Based on a Nonwoven Fabric Platform for Permeable and Waterproof Wearable Sensing Applications AITranslate

Hebei University of Technology; Tianjin University of Technology and Education; Tianjin University of Technology and Education; University of Jinan; Hebei University of Technology; Hebei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Flexible tactile sensors are under high pursuit for wearable electronics toward healthcare monitoring, human–machine interaction, and artificial intelligence. Permeability and hydrophobicity are emerging unique properties and require significant dedication of research efforts. Herein, we develop a type of flexible, breathable, and waterproof iontronic tactile sensor based on a nonwoven fabric platform using a facile dip-drying and solution-spraying technique. The intrinsic open-ended porous structure of the fabric offers air permeability (∼224.9 mm s–1), and the stearic acid microsheets decorated on the outside of the sensor provides effective hydrophobic protection (water contact angle ∼151.9°). The designed electrode-to-electrolyte interfacing microstructures of MXene microspheres and nanosheets on the fabric electrodes and the hierarchical structures with conical secondary features of chrysanthemum pollen on the fabric electrolyte endow the sensor with a high sensitivity of 214.92 kPa–1 and a wide detection range of 0–45 kPa. Fast response time, low detection limit, good dynamic response, and excellent stability are also achieved. With the help of a home-built mechatronic sensing system, the developed fabric tactile sensor can be practically used either as sensor units for human health status monitoring and motion detection or as a sensor array for spatial pressure distribution identification of human–object interaction.

KeyWords AITranslate

iontronic tactile sensor fabric sensor breathable permeable hydrophobicity waterproof
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01369

Chinese Library Classification Number:

Citation Information:

Flexible tactile sensors are under high pursuit for wearable electronics toward healthcare monitoring, human–machine interaction, and artificial intelligence. Permeability and hydrophobicity are emerging unique properties and require significant dedication of research efforts. Herein, we develop a type of flexible, breathable, and waterproof iontronic tactile sensor based on a nonwoven fabric platform using a facile dip-drying and solution-spraying technique. The intrinsic open-ended porous structure of the fabric offers air permeability (∼224.9 mm s–1), and the stearic acid microsheets decorated on the outside of the sensor provides effective hydrophobic protection (water contact angle ∼151.9°). The designed electrode-to-electrolyte interfacing microstructures of MXene microspheres and nanosheets on the fabric electrodes and the hierarchical structures with conical secondary features of chrysanthemum pollen on the fabric electrolyte endow the sensor with a high sensitivity of 214.92 kPa–1 and a wide detection range of 0–45 kPa. Fast response time, low detection limit, good dynamic response, and excellent stability are also achieved. With the help of a home-built mechatronic sensing system, the developed fabric tactile sensor can be practically used either as sensor units for human health status monitoring and motion detection or as a sensor array for spatial pressure distribution identification of human–object interaction.

quote

GB/T 7714-2015 [1] Guifen Sun, Yongxiang Jiang, Hongchang Sun, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01369.
MLA [1] Guifen Sun, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01369.
APA [1] Guifen Sun, Yongxiang Jiang, Hongchang Sun, Peng Wang, Chuizhou Meng, & Shijie Guo. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01369
IEEE [1] Guifen Sun, Yongxiang Jiang, Hongchang Sun, Peng Wang, Chuizhou Meng, and Shijie Guo, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01369. keywords: {iontronic tactile sensor fabric sensor breathable permeable hydrophobicity waterproof}