Fabrication of a Double-Network Hydrogel Based on Carboxymethylated Curdlan/Polyacrylamide with Highly Mechanical Performance for Cartilage Repair AITranslate
Abstract AITranslate
Double-network (DN) hydrogels have been confirmed to possess versatile mechanical properties. Herein, we fabricated a stretchable, tough, and self-recoverable DN hydrogel containing a physically cross-linked carboxymethylated curdlan (CMCD) network and a covalently cross-linked polyacrylamide (PAAm) network. The coupled hydrogen bonding and ionic associations of CMCD macromolecules as a sacrificial architecture endowed the CMCD/PAAm DN hydrogel with tunable, multiple, and recoverable mechanical properties within a large scope. The CMCD microcrystal network was transformed into a homogeneous structure via osmotic stress. The resulting DN hydrogel exhibited stretchable and tough mechanical properties with a tensile strength of 0.69 MPa and an elongation at a break of 2185% at a high water content of approximately 75%. The hydrogel was evaluated through in vitro cell experiments, including cytotoxicity evaluation, live/dead fluorescence microscopy, flow cytometry analysis, and in vivo cartilage repair. Our results show that the DN hydrogel manifests its competence for growth-factor-free cartilage repair and has great potential as a scaffold for cartilage repair.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01094
Chinese Library Classification Number:
Citation Information:
Double-network (DN) hydrogels have been confirmed to possess versatile mechanical properties. Herein, we fabricated a stretchable, tough, and self-recoverable DN hydrogel containing a physically cross-linked carboxymethylated curdlan (CMCD) network and a covalently cross-linked polyacrylamide (PAAm) network. The coupled hydrogen bonding and ionic associations of CMCD macromolecules as a sacrificial architecture endowed the CMCD/PAAm DN hydrogel with tunable, multiple, and recoverable mechanical properties within a large scope. The CMCD microcrystal network was transformed into a homogeneous structure via osmotic stress. The resulting DN hydrogel exhibited stretchable and tough mechanical properties with a tensile strength of 0.69 MPa and an elongation at a break of 2185% at a high water content of approximately 75%. The hydrogel was evaluated through in vitro cell experiments, including cytotoxicity evaluation, live/dead fluorescence microscopy, flow cytometry analysis, and in vivo cartilage repair. Our results show that the DN hydrogel manifests its competence for growth-factor-free cartilage repair and has great potential as a scaffold for cartilage repair.
quote
| GB/T 7714-2015 | [1] Pengguang Wang, Min Wu, Ruiqi Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01094. |
| MLA | [1] Pengguang Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01094. |
| APA | [1] Pengguang Wang, Min Wu, Ruiqi Li, Zhixiang Cai, & Hongbin Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01094 |
| IEEE | [1] Pengguang Wang, Min Wu, Ruiqi Li, Zhixiang Cai, and Hongbin Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01094. keywords: {carboxymethylated curdlan;ion crosslinking;osmotic stress method;UV initiation;doublenetwork hydrogel;mechanical properties;Show More} |