daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Printed Wheatstone bridge with embedded polymer based piezoresistive sensors for strain sensing applications AITranslate

University of Minho; University of Minho; University of Minho;Basque Center for Materials, Applications and Nanostructures (BCMaterials); University of Minho;Basque Center for Materials, Applications and Nanostructures (BCMaterials)
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Printed sensors find an increasing interest essentially due to their characteristics of flexibility and low cost per unit area. In this work a screen printed Wheatstone bridge is presented, suitable for strain sensing applications. A piezoresistive ink composite based on biocompatible thermoplastic elastomer styrene-ethylene/butylene-styrene (SEBS) as matrix and multi-walled carbon nanotubes (MWCNT) as nanofillers was used as a piezoresistive sensing material. Different deposition techniques, such as, screen printing, spray painting and drop casting were evaluated in order to optimize the resistance variation related to the piezoresistive effect. Several Wheatstone bridges with one and two sensors were designed to obtain an output sensitivity as a function of the strain submitted to the sensors. Further, different sensor geometries were evaluated to maximize the strain output sensitivity. Electro-mechanical bending tests showed a good linearity and a sensitivity up to 18 mV/V in the all screen printed half Wheatstone bridge output with two MWCNT/SEBS sensors. Graphical abstract Download : Download high-res image (126KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2018.01.004

Chinese Library Classification Number:

Citation Information:

Printed sensors find an increasing interest essentially due to their characteristics of flexibility and low cost per unit area. In this work a screen printed Wheatstone bridge is presented, suitable for strain sensing applications. A piezoresistive ink composite based on biocompatible thermoplastic elastomer styrene-ethylene/butylene-styrene (SEBS) as matrix and multi-walled carbon nanotubes (MWCNT) as nanofillers was used as a piezoresistive sensing material. Different deposition techniques, such as, screen printing, spray painting and drop casting were evaluated in order to optimize the resistance variation related to the piezoresistive effect. Several Wheatstone bridges with one and two sensors were designed to obtain an output sensitivity as a function of the strain submitted to the sensors. Further, different sensor geometries were evaluated to maximize the strain output sensitivity. Electro-mechanical bending tests showed a good linearity and a sensitivity up to 18 mV/V in the all screen printed half Wheatstone bridge output with two MWCNT/SEBS sensors. Graphical abstract Download : Download high-res image (126KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] H.F. Castro, V. Correia, N. Pereira, et al. Additive Manufacturing, 2018(20). DOI:10.1016/j.addma.2018.01.004.
MLA [1] H.F. Castro, et al., Additive Manufacturing, no. 20, 2018, https://doi.org/10.1016/j.addma.2018.01.004.
APA [1] H.F. Castro, V. Correia, N. Pereira, P. Costab, J. Oliveiraa, & S. LancerosMéndez. (2018). Additive Manufacturing(20). https://doi.org/10.1016/j.addma.2018.01.004
IEEE [1] H.F. Castro, V. Correia, N. Pereira, P. Costab, J. Oliveiraa, and S. LancerosMéndez, Additive Manufacturing, no. 20, 2018, doi: 10.1016/j.addma.2018.01.004.