Preliminary Discussion on the Design of Recycled Water Supply Systems for Rare Metals Metallurgical Plants AITranslate
Abstract AITranslate
Based on layout and special requirements for balanced water pressure of the rare metal pyro-metallurgical plants,the design measures and treatment method of recycled water supply system are given so as to ensure safe handling of the water equipment and save water resource.
KeyWords AITranslate
1钱以明.高层建筑空调[M].上海:同济大学出版社,1993.266.
1黄国涛,沈致和.单晶硅生产车间循环给水系统的设计[J].山西建筑,2008,34(15):14-16.
2张晓静.冶金工业给排水工程设计方法探讨[J].中国高新技术企业,2010(4):88-89. 被引量:2
1王倩.浅谈工业给排水工程的造价控制与管理措施[J].城市建设:下旬,2011(3):101-101.
2席宇.冶金工业给排水工程设计分析[J].世界有色金属,2020(7):226-227.
1郑绪功.敞开式循环给水系统在300米~3高炉的应用[J].冶金动力,1990(1):59-62.
2闫建章.浅谈小型连铸浊环水系统的稳压问题[J].山西冶金,1997,0(2):23-24.
3吴峥,徐仁中,周云麟.鞍钢5号中薄板坯连铸机现代化技术改造[J].鞍钢技术,2004(1):48-51.
4吴峥,王明仁,周云麟.鞍钢1700炼钢-连铸连轧短流程现代化技术改造[J].鞍钢技术,2001(6):29-33.
5原兵燕,王庆丰,宁小锋,孟巍,王义.安钢2200m^3高炉INBA渣处理系统改造[J].工业安全与环保,2008,34(1):48-50. 被引量:2
6严斌.浅谈封闭式冷却循环给水系统的设计[J].工程设计与研究(长沙),2002(2):46-48.
7张文朴.钨钼基础工业化学(八)[J].中国钨业,1997,0(Z1):45-51. 被引量:1
8赵永平.炉渣脱水器溢水原因分析及治理[J].河北冶金,2014(1):60-62.
9包新荣,连兵.甘肃省铁合金及电石行业节能对策分析研究[J].甘肃科技,2012,28(6):1-4.
10严斌.浅谈封闭式冷却循环给水系统设计[J].湖南有色金属,2002,18(1):38-39.
Basic Information:
DOI:
Chinese Library Classification Number:TF808[冶金工程—有色金属冶金]
Citation Information:
Based on layout and special requirements for balanced water pressure of the rare metal pyro-metallurgical plants,the design measures and treatment method of recycled water supply system are given so as to ensure safe handling of the water equipment and save water resource.
quote
| GB/T 7714-2015 | [1] YING Hui. Preliminary Discussion on the Design of Recycled Water Supply Systems for Rare Metals Metallurgical Plants[J]. Rare Metals and Cemented Carbides, 2001(3): 53-55. |
| MLA | [1] YING Hui. "Preliminary Discussion on the Design of Recycled Water Supply Systems for Rare Metals Metallurgical Plants." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 53-55. |
| APA | [1] YING Hui. (2001). Preliminary Discussion on the Design of Recycled Water Supply Systems for Rare Metals Metallurgical Plants. Rare Metals and Cemented Carbides(3), 53-55. |
| IEEE | [1] YING Hui, "Preliminary Discussion on the Design of Recycled Water Supply Systems for Rare Metals Metallurgical Plants," Rare Metals and Cemented Carbides, no. 3, pp. 53-55, 2001. keywords: {rare metal metallurgical plant;recycled water supply system,large drag;identical equation} |