Study on Optimization of Separation Effect of Selenium,Tellurium and Copper in Copper Anode Slime AITranslate
Abstract AITranslate
Based on the incomplete separation of selenium,tellurium,and copper in the selenite reduction section of the comprehensive recovery process for copper anode slime,a new process was proposed of supplementing chloride ions to the chlorinated de-selenium solution and an industrial trial of secondary selenite reduction was conducted while other parameters such as reduction time,temperature,and reductant flow rate remained unchanged.The results show that with the new process,the reduction rate of selenium in primary reduction can reach 99.72%,while the reduction degree of tellurium and copper is significantly inhi-bited.In the secondary reduction,the reduction rate of tellurium can reach 95.30%,while that of copper decreases to 4.71%.The selenium content of crude selenium product increases from 72.04%to 76.77%,the tellurium content decreases from 1.62%to 0.45%,and the copper content decreases from 2.17%to 1.01%.Compared with the original process,the improvement effect of the new process is significant.
KeyWords AITranslate
1肖鹏,王红军,叶逢春,易宇,纪宏巍,邱士伟.稀散金属硒、碲回收工艺现状与展望[J].金属矿山,2020,49(4):52-60. 被引量:12
2宁瑞,李伟,刘志中.铜阳极泥处理工艺对比及建议[J].金属材料与冶金工程,2018,46(6):42-47. 被引量:12
3吴克富,贾启金,李家合.提高粗硒品位的生产实践[J].有色金属:冶炼部分,2021(1):72-74. 被引量:2
4房孟钊.从铜阳极泥中高效分离回收硒的技术优化[J].硫磷设计与粉体工程,2022(5):36-39. 被引量:2
5章尚发,王冲,王华,杨坤彬,李英伟.氯化浸出-还原法处理铜阳极泥分铜渣[J].稀有金属与硬质合金,2014,42(1):5-8. 被引量:12
6刘凯华,贾梦鑫.HCl-NaClO_(3)体系控氧化电位法从半导体废料中回收硒的研究[J].有色金属:冶炼部分,2022(1):51-55. 被引量:1
1谭建军,智凤营.锌冶炼渣综合回收工艺探析[J].中国科技期刊数据库 工业A,2021(2):0099-0099.
2缪亚兵,郭灵敏.江西某硫化铜矿石选矿试验研究[J].现代矿业,2023,39(4):92-95.
3焦晓杰,句世俊,郝璐瑶.铜冶炼烟尘综合回收工艺浅析及建议[J].中国金属通报,2022(19):14-16.
4王永斌,冯志兵,岳瑞琪,贾启金,焦晓斌,侯铎.铜碲渣综合回收工艺与实践[J].甘肃冶金,2023,45(3):102-105.
5陆秋艳,张小鸿,张文婷,李丽林.富硒葛粉中硒形态分析及其对脂多糖诱导的AML12细胞氧化损伤的影响[J].环境化学,2023,42(10):3603-3607.
6陈凤,徐晓敏,吴丰勇,王菲.硒化合物对乙醇代谢物损伤的间充质干细胞体外增殖的影响[J].重庆医学,2023,52(21):3227-3231.
7吴卿,莫文君,刘洁琼,彭森,李倩男,万芮含.化学还原-生物刺激对高质量比Cr(Ⅵ)污染土壤治理及稳定化[J].安全与环境学报,2023,23(9):3346-3354.
8明守禄,张芳,彭军,赵立杰,李斐斐,常仕琦.氧化铁皮非等温碳热还原动力学研究[J].粉末冶金工业,2023,33(5):17-24.
9吴秋宇,雷泽锐,张浩峰,杜建伟,文树龙,贺框,张明杨,黄凯华.MOFs衍生镍单原子材料电催化还原化学镀镍废水中的亚磷酸盐[J].电镀与涂饰,2023,42(21):73-84.
10甘勇辉,王水琦.金线莲施硒的吸收与积累规律[J].中国土壤与肥料,2023(8):214-221.
Basic Information:
DOI:
Chinese Library Classification Number:TF843.5[冶金工程—有色金属冶金]
Citation Information:
Based on the incomplete separation of selenium,tellurium,and copper in the selenite reduction section of the comprehensive recovery process for copper anode slime,a new process was proposed of supplementing chloride ions to the chlorinated de-selenium solution and an industrial trial of secondary selenite reduction was conducted while other parameters such as reduction time,temperature,and reductant flow rate remained unchanged.The results show that with the new process,the reduction rate of selenium in primary reduction can reach 99.72%,while the reduction degree of tellurium and copper is significantly inhi-bited.In the secondary reduction,the reduction rate of tellurium can reach 95.30%,while that of copper decreases to 4.71%.The selenium content of crude selenium product increases from 72.04%to 76.77%,the tellurium content decreases from 1.62%to 0.45%,and the copper content decreases from 2.17%to 1.01%.Compared with the original process,the improvement effect of the new process is significant.
quote
| GB/T 7714-2015 | [1] WANG Peng-cheng, ZHANG Shang-fa, LUO Jin-song. Study on Optimization of Separation Effect of Selenium,Tellurium and Copper in Copper Anode Slime[J]. Rare Metals and Cemented Carbides, 2023(5): 28-31. |
| MLA | [1] WANG Peng-cheng, et al., "Study on Optimization of Separation Effect of Selenium,Tellurium and Copper in Copper Anode Slime." Rare Metals and Cemented Carbides, no. 5, 2023, pp. 28-31. |
| APA | [1] WANG Peng-cheng, ZHANG Shang-fa, & LUO Jin-song. (2023). Study on Optimization of Separation Effect of Selenium,Tellurium and Copper in Copper Anode Slime. Rare Metals and Cemented Carbides(5), 28-31. |
| IEEE | [1] WANG Peng-cheng, ZHANG Shang-fa, and LUO Jin-song, "Study on Optimization of Separation Effect of Selenium,Tellurium and Copper in Copper Anode Slime," Rare Metals and Cemented Carbides, no. 5, pp. 28-31, 2023. keywords: {copper anode slime;selenium;tellurium;copper;reduction;separation} |