Research Progress and Development Trend of Titanium Powder Preparation Technology AITranslate
Abstract AITranslate
The principle,research progress,advantages and disadvantages are briefly introduced of several titanium powder preparation technologies such as atomization method,hydrogenation dehydrogenation method,thermal reduction method,and radio frequency plasma spheroidization method.According to the deficiencies of each technology,the future development trend of titanium powder preparation is pointed out.
KeyWords AITranslate
1洪艳,曲涛,沈化森,王兆林,车小奎.氢化脱氢法制备钛粉工艺研究[J].稀有金属,2007,31(3):311-315. 被引量:23
2陈树民.攀枝花钒钛磁铁矿钛铁矿回收工艺流程优化探讨[J].矿产综合利用,2009(5):7-10. 被引量:7
3万贺利,徐宝强,戴永年,杨斌,刘大春.钙热还原法制备钛粉过程的研究[J].功能材料,2012,43(6):700-703. 被引量:10
4李保强,金化成,张延昌,胡鹏,袁方利,陈运法.3D打印用球形钛粉制备技术研究进展[J].过程工程学报,2017,17(5):911-917. 被引量:19
5欧阳鸿武,余文焘,陈欣,何世文,黄劲松.利用“球化效应”激光扫描制备球形Ti粉的研究[J].稀有金属材料与工程,2007,36(9):1608-1612. 被引量:7
6路新,刘程程,曲选辉.钛及钛合金粉末注射成形技术研究进展[J].粉末冶金技术,2013,31(2):139-144. 被引量:17
7黄龙贵,李海洋,郑战光,常岩军,贺德强.多向锻造强化纯钛的试验研究[J].热加工工艺,2017,46(15):29-32. 被引量:1
8谢焕文,邹黎明,刘辛,乐晨,蔡一湘.球形钛粉制备工艺现状[J].材料研究与应用,2014,8(2):78-82. 被引量:13
9古忠涛,叶高英,刘川东,童洪辉.射频等离子体球化Ti粉体的研究[J].材料开发与应用,2009,24(4):30-34. 被引量:6
10王尊,杨绍利.氢化脱氢工艺制备钛粉研究[J].金属材料与冶金工程,2014,42(5):23-27. 被引量:2
1张哲轩,赵文天,张会华,肖敏强,杨鹏伟,门路辉.EIGA雾化喷嘴对氩气-钛粉两相流模拟研究[J].兵器材料科学与工程,2021,44(2):78-84. 被引量:1
2张顺星,董佳辉,梁小宜.基于PROFINET的封闭式钛粉加工控制系统实现[J].中国设备工程,2023(5):135-137.
1张雪良,陶宇,贾建,曲敬龙.电极感应熔化气体雾化制粉工艺气体流场模拟研究[J].粉末冶金工业,2022,32(4):8-16. 被引量:2
1贾雷,严红燕,李慧,刘畅,张帅.金属铪的制备和精炼[J].热加工工艺,2020,0(1):10-15. 被引量:1
2李启军,章林,李兵兵,魏东斌,曲选辉.氢化脱氢法制备Nb-Ti基合金粉末[J].稀有金属材料与工程,2020,49(1):93-100. 被引量:1
3邹黎明,毛新华,胡可,刘辛.采用图像分析技术对球形Ti-6Al-4V粉末粒形的定量分析[J].稀有金属材料与工程,2020,49(3):950-955. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
The principle,research progress,advantages and disadvantages are briefly introduced of several titanium powder preparation technologies such as atomization method,hydrogenation dehydrogenation method,thermal reduction method,and radio frequency plasma spheroidization method.According to the deficiencies of each technology,the future development trend of titanium powder preparation is pointed out.
quote
| GB/T 7714-2015 | [1] LIU Chang, LI Hui, ZHANG Han-xin, et al. Research Progress and Development Trend of Titanium Powder Preparation Technology[J]. Rare Metals and Cemented Carbides, 2020(1): 35-39. |
| MLA | [1] LIU Chang, et al., "Research Progress and Development Trend of Titanium Powder Preparation Technology." Rare Metals and Cemented Carbides, no. 1, 2020, pp. 35-39. |
| APA | [1] LIU Chang, LI Hui, ZHANG Han-xin, & LIANG Jing-long. (2020). Research Progress and Development Trend of Titanium Powder Preparation Technology. Rare Metals and Cemented Carbides(1), 35-39. |
| IEEE | [1] LIU Chang, LI Hui, ZHANG Han-xin, and LIANG Jing-long, "Research Progress and Development Trend of Titanium Powder Preparation Technology," Rare Metals and Cemented Carbides, no. 1, pp. 35-39, 2020. keywords: {titanium powder;preparation technology;sphericity rate;research progress;development trend} |