daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Development of Milling Technology of NdFeB Permanent Magnet Material AITranslate

School of Materials Science and Engineering, Liaoning University of Technology;School of Materials Science and Engineering, Liaoning University of Technology;School of Materials Science and Engineering, Liaoning University of Technology;School of Materials Science and Engineering, Liaoning University of Technology;School of Materials Science and Engineering, Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of milling technology of NdFeB permanent magnet material is reviewed, and detailed description is made of the physical method, rapid solidification method, gas atomization method and HD method. With the improvement of milling technology, powder particle size, defects and magnetic properties are improved to various degree. Milling technology will be developed with the tendency towards the combination of various techniques.

KeyWords AITranslate

NdFeB permanent magnet material milling technology the latest development combination of various techniques

1Boris Boehenkov,Sergey Lutz. A review of modern ma- terials of permanent magnets[J]. Electrical Engineering,2004, (4) :201-203.

2Liu Z W, Huang H Y, Gao X X, et al. Microstructure and property evolution of isotropic and anisotropic NdFeB magnets fabricated from nanocrystalline ribbons by spark plasma sintering and hot deformation[J]. Jour- nal of Physics D : Applied Physics, 2011,44 (2) : 025003.

3Liu W Q,Cui Z Z,Yi X F,et al. Structure and magnetic properties of magnetically isotropic and anisotropic Nd-Fe-B permanent magnets prepared by spark plasma sintering technology[J]. Journal of Applied Physics, 2010,107(9) :09A719.

4Lee D, Bauser S, Higgins A,et al. Bulk anisotropic composite rare earth magnets[J]. Journal of Applied Phys ics,2009,99(8) :08B516.

5Yutaka M. Recent development of NdFeB sintered mag- nets and their applications[J]. Journal of Magnetism and Magnetic Materials, 2006,330 : 343-345.

6Wang Zhenxi. Rare earth permanent magnet industry in China[A]. The 5th international conference on rare earth development and application [C]. Baotou: The Chinese Society of Rare Earths,2007.

7Sam Liu, Lee Don, Huang Meiqing, et al. Research and development of bulk anisotropic nanograin composite rare earth permanent magnets[A]. Proc of 19th interna- tional workshop on RE PM and their applications[C]. Beijing China,2006. 123-135.

8Sagawa M,Fujimura S,Togawa N,et al. New material for permanent magnets on a base of Nd and Fe[J]. Journal of Applied Physics,1984, 55(6) :2 083-2 087.

9Schultz L,Wecker J, Hellstern E. Formation and properties of NdFeB prepared by mechanical alloying and solid- state reaction[J]. Journal of Applied Physics, 1987,61 3 583-3 585.

10Jurczyk M, Cook J S,Collocott S J. Application of high energy ball milling to the production of magnetic pow- ders from NdFeB-type alloys[J]. Journal of Alloys and Compounds,1995,217(1) : 65-68.

1李婷婷,崔艳.钕铁硼永磁材料专利技术综述[J].河南科技,2017,36(12):50-51. 被引量:1

1周巧英,陈仁杰,郭帅.钕铁硼磁体表面高耐蚀性锌铝涂层的制备及性能研究[J].电镀与涂饰,2020,39(3):165-170. 被引量:3

1段星,黄焱球,刘甜甜.BNBMT无铅压电陶瓷的制备及性能研究[J].佛山陶瓷,2009,19(6):1-4.

2郝忠彬,包大新,谭春林,杜君峰,王军强.N48H高性能烧结NdFeB永磁材料的开发[J].磁性材料及器件,2007,38(6):52-54. 被引量:3

3王仁祺.废旧锂离子电池中钴的回收[J].电源技术,2012,36(4):587-589. 被引量:5

4李镇隆.高压水雾化制粉技术在电触头制造领域中的应用[J].电工合金,1998(3):45-46. 被引量:2

5郝忠彬,张义龙,包大新,杜君峰,谭春林,王军强.N44SH高性能烧结NdFeB永磁材料的开发[J].磁性材料及器件,2008,39(2):42-43. 被引量:3

6刘湘连,董清飞,周寿增.工业生产高磁能积烧结NdFeB永磁的结构与性能[J].磁性材料及器件,1999,30(1):54-57. 被引量:7

7孔梅梅,张立永,王醒东,夏芳敏,林中山.高质量YBCO薄膜的沉积方法[J].广州化工,2013,41(1):38-40.

8何良惠,李自强,李升章,王祖森,彭忠东.共沉淀法制备压敏陶瓷掺杂氧化锌条件的研究[J].四川有色金属,1995(4):5-8.

9袁国辉,褚德威,孔凡涛,姜兆华.碱锰电池中锌合金粉的电化学性能[J].电池,2003,33(2):87-89. 被引量:4

10谭超.探析基于物理方法的风电功率预测系统在贺兰山风电场的应用[J].科技风,2011(1):201-201. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

The latest development of milling technology of NdFeB permanent magnet material is reviewed, and detailed description is made of the physical method, rapid solidification method, gas atomization method and HD method. With the improvement of milling technology, powder particle size, defects and magnetic properties are improved to various degree. Milling technology will be developed with the tendency towards the combination of various techniques.

quote

GB/T 7714-2015 [1] LI Yang, QI Jin-gang, WU Di, et al. The Latest Development of Milling Technology of NdFeB Permanent Magnet Material[J]. Rare Metals and Cemented Carbides, 2014(5): 28-33.
MLA [1] LI Yang, et al., "The Latest Development of Milling Technology of NdFeB Permanent Magnet Material." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 28-33.
APA [1] LI Yang, QI Jin-gang, WU Di, GAO Yong, & ZHAO Zuo-fu. (2014). The Latest Development of Milling Technology of NdFeB Permanent Magnet Material. Rare Metals and Cemented Carbides(5), 28-33.
IEEE [1] LI Yang, QI Jin-gang, WU Di, GAO Yong, and ZHAO Zuo-fu, "The Latest Development of Milling Technology of NdFeB Permanent Magnet Material," Rare Metals and Cemented Carbides, no. 5, pp. 28-33, 2014. keywords: {NdFeB;permanent magnet material;milling technology;the latest development;combination of various techniques}