Effects of SiC Particle Size on Density and Tensile Properties of High-pressure Torsion SiC_P/Al Composites AITranslate
Abstract AITranslate
The mixture powders were directly consolidated of SiC particles with different size and industrial pure aluminum by high-pressure torsion(HPT)to prepare SiC_P/Al composites.The volume of the composites was measured with drainage method,and then the density was calculated.Effects of SiC particle size on density and tensile properties of the composites were studied by tensile tests and SEM observation of the tensile fracture.The results show that with the increase of SiC particle size at 200 ℃,both the amount and specific surface area of the particles gradually decrease due to the certain SiC particle content,more large particles are broken by shearing force and weakly bound freshmen interface increases,resulting in both the density and tensile strength of the composites increasing firstly and then decreasing.Meanwhile,the dimples in tensile fracture have increased size with poorer distribution uniformity,the residue particles in the dimple increase,and therefore the composites have weakened ductile fracture characteristics and enhanced brittle fracture characteristics.
KeyWords AITranslate
1樊建中,桑吉梅,石力开.颗粒增强铝基复合材料的研制、应用与发展[J].材料导报,2001,15(10):55-57. 被引量:67
2李晓,李萍,薛克敏,王成.高压扭转压力对SiC_p-Al复合材料组织性能的影响[J].中国有色金属学报,2012,22(2):401-407. 被引量:12
3王文明,潘复生,孙旭炜,曾苏民,Lu Yun.SiCp/Al复合材料界面反应研究现状[J].重庆大学学报:自然科学版,2004,27(3):108-113. 被引量:28
4Xu H, Palmiere E J. Particulate refinement and redistri- bution during the axisymmetric compression of an Al/ SiCp metal matrix composite[J]. Composites (Part A) : Applied Science and Manufacturing, 1999,30 ( 3 ) : 203 - 211.
5周清,马宗义,赵杰,毕敬,朱世杰,王富岗.弥散质点和SiC颗粒复合强化铝基复合材料蠕变形变与断裂[J].金属学报,1998,34(1):107-112. 被引量:9
6郭成,程羽,尚春阳,苏文斌,许建群.SiC颗粒增强铝合金基复合材料断裂与强化机理[J].复合材料学报,2001,18(4):54-57. 被引量:37
7程羽,郭成,郭生武,陈金德.SiC颗粒增强Al基复合材料成形极限的研究[J].塑性工程学报,2001,8(1):1-3. 被引量:7
8Zhilyaev A P,Langdon T G. Using high-pressure torsion for metal processing: Fundamentals and applications [J]. Progress in Materials Science, 2008, 53 (6) : 893- 979.
9Sabirov I, Kolednik O, Pippan R. Homogenization of metal matrix composites by high-pressure torsion[J]. Metallurgical and Materials Transactions A, 2005, 36 (10):2 861-2 870.
10Zhilyaev A P,Nurislamova G V,Kim B K,et al. Exper- imental parameters influencing grain refinement and mierostructural evolution during high-pressure torsion [J]. Acta Materialia, 2003,51 ( 3 ) :753-765.
1何卫,吴昊,李德阁,王利民,陈胜男,阎佳思,肖伟,杨辉.粒度和界面原子调控对SiC/Al复合材料强度的影响[J].稀有金属材料与工程,2023,52(1):139-144.
2李萍,丁春慧,王薄笑天,吴广善,薛克敏.高压扭转诱导新型Al-Zn-Mg-Cu合金第二相回溶[J].中国有色金属学报,2019,0(1):11-17. 被引量:4
1李萍,许兵,徐洪磊,李云辉,严思梁,薛克敏.Al-Zn-Mg-Cu合金第二相在高压扭转变形中的回溶行为[J].中国有色金属学报,2021,31(9):2382-2389. 被引量:2
2仲晓晓,杨志刚,张尧,徐岩,顾勇飞,贾建波,骆俊廷.高压扭转变形2A12铝合金组织性能演变与断裂行为[J].中国有色金属学报,2022,32(8):2173-2184. 被引量:3
3尹冬松,张游游,王锰.多向压缩对ZK60镁合金微观组织和耐腐蚀性能的影响[J].黑龙江科技大学学报,2023,33(1):76-79.
4刘满平,任晓宇,陈昱林,贾志宏,丁立鹏,Hans J ROVEN.纳米晶Al-Mg-Si-Cu铝合金的微观结构、力学性能和时效相演变[J].中国有色金属学报,2023,33(6):1695-1706.
1贺鹏,薛克敏,王成国,李萍,石文超.HPT法对SiCp/Al复合材料颗粒断裂的影响[J].塑性工程学报,2015,22(2):117-120. 被引量:3
2薛克敏,钱陈豪,李萍,李晓.高压扭转圈数对碳化硅颗粒铝基复合材料组织和性能的影响[J].塑性工程学报,2012,19(2):92-95. 被引量:7
3李晓,李萍,薛克敏,王成,章凯.高压扭转法对SiC_p-Al基复合材料颗粒分布的影响[J].材料工程,2012,40(2):50-54. 被引量:11
4马俊林,李萍,徐杰,田野,薛克敏.HPT制备高含量SiC颗粒增强Al基复合材料的性能和致密化行为[J].稀有金属与硬质合金,2015,43(5):58-63.
5谢瑞,李萍,刘国凯,马俊林,薛克敏,贺鹏.不同粒径的SiC体积配比对SiC_p/Al基复合材料显微组织和拉伸性能的影响[J].粉末冶金工业,2016,26(6):24-29. 被引量:1
6石文超,李萍,李晓,薛克敏.颗粒体积分数对高压扭转的SiCp/Al基复合材料拉伸性能影响[J].粉末冶金工业,2013,23(1):46-51. 被引量:3
7林俐菁,王成国,乔硕.SiC颗粒尺寸对高压扭转制备SiCp/Al基复合材料金相组织和显微硬度影响[J].粉末冶金工业,2014,24(1):35-38.
8赵云龙.三种SPD方法概述[J].电大理工,2013(2):7-9.
9李晓,李萍,王成,张倩倩.基于SPD法颗粒增强铝基复合材料研究综述[J].粉末冶金工业,2011,21(1):60-64. 被引量:2
10李晓,李萍,张倩倩,王成,章凯.SiCp/Al基复合材料的高压扭转试验[J].精密成形工程,2010,2(6):29-31. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TB331[一般工业技术—材料科学与工程]
Citation Information:
The mixture powders were directly consolidated of SiC particles with different size and industrial pure aluminum by high-pressure torsion(HPT)to prepare SiC_P/Al composites.The volume of the composites was measured with drainage method,and then the density was calculated.Effects of SiC particle size on density and tensile properties of the composites were studied by tensile tests and SEM observation of the tensile fracture.The results show that with the increase of SiC particle size at 200 ℃,both the amount and specific surface area of the particles gradually decrease due to the certain SiC particle content,more large particles are broken by shearing force and weakly bound freshmen interface increases,resulting in both the density and tensile strength of the composites increasing firstly and then decreasing.Meanwhile,the dimples in tensile fracture have increased size with poorer distribution uniformity,the residue particles in the dimple increase,and therefore the composites have weakened ductile fracture characteristics and enhanced brittle fracture characteristics.
quote
| GB/T 7714-2015 | [1] SUN Da-zhi, XUE Ke-min, WANG Cheng-guo, et al. Effects of SiC Particle Size on Density and Tensile Properties of High-pressure Torsion SiC_P/Al Composites[J]. Rare Metals and Cemented Carbides, 2016(2): 64-67. |
| MLA | [1] SUN Da-zhi, et al., "Effects of SiC Particle Size on Density and Tensile Properties of High-pressure Torsion SiC_P/Al Composites." Rare Metals and Cemented Carbides, no. 2, 2016, pp. 64-67. |
| APA | [1] SUN Da-zhi, XUE Ke-min, WANG Cheng-guo, & LI Ping. (2016). Effects of SiC Particle Size on Density and Tensile Properties of High-pressure Torsion SiC_P/Al Composites. Rare Metals and Cemented Carbides(2), 64-67. |
| IEEE | [1] SUN Da-zhi, XUE Ke-min, WANG Cheng-guo, and LI Ping, "Effects of SiC Particle Size on Density and Tensile Properties of High-pressure Torsion SiC_P/Al Composites," Rare Metals and Cemented Carbides, no. 2, pp. 64-67, 2016. keywords: {SiCP/Al composite;high-pressure torsion;SiC particle;particle size;density;tensile property} |