daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of Binding Phase of TiO Cermet AITranslate

Xiangyi Zhongyuan Technology Co., Ltd.;Xiangyi Zhongyuan Technology Co., Ltd.;Xiangyi Zhongyuan Technology Co., Ltd.;Xiangyi Zhongyuan Technology Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the use of Cu-based and Fe-Cr-based alloy as the binding phase of TiO-based Cermet gild material.The results showed that pure Cu and Fe-Cr alloy has lower wettability on Tio,as is not suitable for TiO binding phase.The addition of small amount of Mo,C in Cu can distinctly improve the wettability,while the addition of proper amount of Al,Ni and Si into Cu-Mo-C means alloy color similar to gold and good wearability as well as very high inferface bond strength with TiO,as are suitable as binding phase of TiO ceramic.The wettability of Fe-Cr alloy can be remarkably improved and the reaction at Fe-Tio interface can be controlled to form very high strength at the interface with TiO by addition of surface active substance A,Fe-Cr can be used as binding phaes of TiO Ceramic.

KeyWords AITranslate

gild alloy metallic binding phase Cu-based alloy Fe-Cr alloy

1颜长舒,唐仁政,卢安贤,黄继武.石墨-铝硅复合材料的制备及性能[J].中南工业大学学报,1995,26(2):200-212. 被引量:5

2陈康华,包崇玺,刘红卫.金属/陶瓷润湿性(下)[J].材料科学与工程,1997,15(4):27-34. 被引量:37

3原日彬,吴殿军,王伟民,王震.金属液/固相润湿性研究进展[J].中国铸造装备与技术,1999(4):11-14. 被引量:8

4张金咏,傅正义,王为民.陶瓷-金属复合材料制备与研究[J].武汉工业大学学报,1999,21(2):10-13. 被引量:14

5陈康华,包崇玺,刘红卫.金属/陶瓷润湿性(上)[J].材料科学与工程,1997,15(3):6-10. 被引量:46

1张文朴.我国含钼新材料研究进展评述[J].中国钼业,2004,28(4):9-12. 被引量:2

1张文朴.落实科学发展观 再造中国钼业辉煌[J].中国钼业,2005,29(5):11-14.

2吴贤,张健,康新婷,荆鹏.钼粉的制备技术及研发现状[J].稀有金属材料与工程,2007,36(A03):562-566. 被引量:24

1李庆奎,赵红亮,钟晖,钟海云.一氧化钛基金属陶瓷仿金材料的制备及性能研究[J].稀有金属,2005,29(3):279-284. 被引量:1

2李庆奎,钟海云,李荐,戴艳阳.钛基仿金材料及其最新进展[J].稀有金属与硬质合金,2001,29(4):36-38.

3李本川,于凤林.Fe-Cr-C處减振合金[J].材料开发与应用,1990,5(4):8-12. 被引量:2

4成旦红,徐伟一,秦益琴,华立群,张仲燕.电沉积非晶态铁-铬合金镀层的研究[J].电化学,1997,3(2):202-205. 被引量:9

5张鉴清,曾潮流,牛焱,吴维(山文).铁铬合金热腐蚀的交流阻抗研究[J].中国腐蚀与防护学报,1993,13(3):274-278.

6马国亮,曹秋霞,秦歌.铁铬合金在塑性变形时温度对强化的影响[J].金属成形工艺,2003,21(6):101-102.

7唐多光,周自强,葛建生,陆庆桃.抗变色仿金合金的研究[J].金属科学与工艺,1991,10(1):77-82. 被引量:18

8李庆奎,钟晖,戴艳阳,钟海云.Fe-Cr合金在TiO陶瓷上的润湿及其机理[J].中国有色金属学报,2002,12(4):677-681. 被引量:8

9邢建东,周庆德.含碳量对Fe-20%Cr合金高温耐磨性的影响[J].钢铁,1992,27(8):56-60. 被引量:8

10薛涛.仿金材料的熔铸[J].五金科技,1992(3):15-15.

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料]

Citation Information:

Study is made on the use of Cu-based and Fe-Cr-based alloy as the binding phase of TiO-based Cermet gild material.The results showed that pure Cu and Fe-Cr alloy has lower wettability on Tio,as is not suitable for TiO binding phase.The addition of small amount of Mo,C in Cu can distinctly improve the wettability,while the addition of proper amount of Al,Ni and Si into Cu-Mo-C means alloy color similar to gold and good wearability as well as very high inferface bond strength with TiO,as are suitable as binding phase of TiO ceramic.The wettability of Fe-Cr alloy can be remarkably improved and the reaction at Fe-Tio interface can be controlled to form very high strength at the interface with TiO by addition of surface active substance A,Fe-Cr can be used as binding phaes of TiO Ceramic.

quote

GB/T 7714-2015 [1] TANG Xiao-ping, CAO Yu-min, LI Qing-kui, et al. Study of Binding Phase of TiO Cermet[J]. Rare Metals and Cemented Carbides, 2002(1): 9-12.
MLA [1] TANG Xiao-ping, et al., "Study of Binding Phase of TiO Cermet." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 9-12.
APA [1] TANG Xiao-ping, CAO Yu-min, LI Qing-kui, & ZHONG Hai-yun. (2002). Study of Binding Phase of TiO Cermet. Rare Metals and Cemented Carbides(1), 9-12.
IEEE [1] TANG Xiao-ping, CAO Yu-min, LI Qing-kui, and ZHONG Hai-yun, "Study of Binding Phase of TiO Cermet," Rare Metals and Cemented Carbides, no. 1, pp. 9-12, 2002. keywords: {gild alloy;metallic binding phase;Cu-based alloy;Fe-Cr alloy}