Preface to the special issue on refractory high-entropy materials AITranslate

School of Materials Science and Engineering
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Refractory high-entropy alloys(RHEAs),composed of multiple refractory elements,such as Nb,Mo,Ta,W,Ti,Zr,Hf,in nearor non-equiatomic ratios,have recently emerged as promising structural materials for extreme environments due to their high melting points,excellent high-temperature mechanical properties,and superior micro structural stability.Compared to conventional HEAs based on elements like Ni,Fe,or Cr,RHEAs offer enhanced elevated-temperature performance but face challenges including segregation during solidification,relatively poor room-temperature ductility,and,most important,high-temperature oxidation.

KeyWords AITranslate

extreme environments room temperature ductility RHEAs structural materials refractory high entropy alloys segregation soli refractory elementssuch SEGREGATION
No data

Basic Information:

DOI:

Chinese Library Classification Number:TG139[一般工业技术—材料科学与工程]

Citation Information:

Refractory high-entropy alloys(RHEAs),composed of multiple refractory elements,such as Nb,Mo,Ta,W,Ti,Zr,Hf,in nearor non-equiatomic ratios,have recently emerged as promising structural materials for extreme environments due to their high melting points,excellent high-temperature mechanical properties,and superior micro structural stability.Compared to conventional HEAs based on elements like Ni,Fe,or Cr,RHEAs offer enhanced elevated-temperature performance but face challenges including segregation during solidification,relatively poor room-temperature ductility,and,most important,high-temperature oxidation.

quote

GB/T 7714-2015 [1] Yi-Ping Lu. Tungsten, 2025(4): 679-679.
MLA [1] Yi-Ping Lu. Tungsten, no. 4, 2025, pp. 679-679.
APA [1] Yi-Ping Lu. (2025). Tungsten(4), 679-679.
IEEE [1] Yi-Ping Lu, Tungsten, no. 4, pp. 679-679, 2025.