daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Remote Epitaxy and Exfoliation of GaN via Graphene Remote Epitaxy and Exfoliation of GaN via Graphene AITranslate

Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Jilin University; Jilin University; Xidian University; Xidian University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The remote epitaxy of GaN via graphene has attracted much attention due to the potential of easy mechanical exfoliation, and the exfoliated layers can be transferred onto foreign substrates according to the application needs, which is beneficial to improve the performance of GaN-based devices. In this work, a GaN epi-layer was grown by metal–organic chemical vapor deposition on the monolayer-graphene-coated AlN/sapphire or GaN substrates. The influence of growth temperature, carrier gas, and substrate on the exfoliation of the GaN epi-layer was studied. When the growth temperature is no more than 800 °C and N2 is used as the carrier gas, the monolayer graphene can be retained on the AlN/sapphire substrate during the growth process. Thus, the GaN epi-layer can be exfoliated successfully. However, the monolayer graphene will be destroyed under a growth temperature of 850 °C, and lead to the failure of exfoliation. Besides, the monolayer graphene can also be damaged when the H2 carrier gas or GaN substrate is employed with a growth temperature of 800 °C. This causes the GaN epi-layer to be exfoliated not as well. The experimental results illustrate that suitable growth conditions and substrate are important for realizing the exfoliation of a GaN epi-layer.

KeyWords AITranslate

GaN exfoliation MOCVD graphene remote epitaxy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00997

Chinese Library Classification Number:

Citation Information:

The remote epitaxy of GaN via graphene has attracted much attention due to the potential of easy mechanical exfoliation, and the exfoliated layers can be transferred onto foreign substrates according to the application needs, which is beneficial to improve the performance of GaN-based devices. In this work, a GaN epi-layer was grown by metal–organic chemical vapor deposition on the monolayer-graphene-coated AlN/sapphire or GaN substrates. The influence of growth temperature, carrier gas, and substrate on the exfoliation of the GaN epi-layer was studied. When the growth temperature is no more than 800 °C and N2 is used as the carrier gas, the monolayer graphene can be retained on the AlN/sapphire substrate during the growth process. Thus, the GaN epi-layer can be exfoliated successfully. However, the monolayer graphene will be destroyed under a growth temperature of 850 °C, and lead to the failure of exfoliation. Besides, the monolayer graphene can also be damaged when the H2 carrier gas or GaN substrate is employed with a growth temperature of 800 °C. This causes the GaN epi-layer to be exfoliated not as well. The experimental results illustrate that suitable growth conditions and substrate are important for realizing the exfoliation of a GaN epi-layer.

quote

GB/T 7714-2015 [1] Xu Han, Jiadong Yu, Zhenhao Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00997.
MLA [1] Xu Han, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00997.
APA [1] Xu Han, Jiadong Yu, Zhenhao Li, Xun Wang, Zhibiao Hao, Yi Luo, Changzheng Sun, Yanjun Han, Bing Xiong, Jian Wang, Hongtao Li, Yuantao Zhang, Bin Duan, Jing Ning, Haidi Wu, & Lai Wang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00997
IEEE [1] Xu Han, Jiadong Yu, Zhenhao Li, Xun Wang, Zhibiao Hao, Yi Luo, Changzheng Sun, Yanjun Han, Bing Xiong, Jian Wang, Hongtao Li, Yuantao Zhang, Bin Duan, Jing Ning, Haidi Wu, and Lai Wang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00997. keywords: {GaN exfoliation MOCVD graphene remote epitaxy}