Research and Development of High-density W-Ni-Fe Alloy AITranslate

National Key Laboratory of Powder Metallurgy of Central South China University of Technology;National Key Laboratory of Powder Metallurgy of Central South China University of Technology;National Key Laboratory of Powder Metallurgy of Central South China University of Technology;National Key Laboratory of Powder Metallurgy of Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High density alloy used as penetrater is an attracting topic. In this paper, the latest development and research on this kind of enhancing alloy are reviewed in respect of properties,low temperature sintering by lowering temperature, and near net shape, and some problems arealso pointed out.

KeyWords AITranslate

high density alloy research development

1刘志国,张宝生,庄育智.新型W-Ni-Fe-TiB_2合金[J].中国有色金属学报,1995,5(4):107-111. 被引量:14

2白淑珍,张宝生.合金元素钴和锰对W-Ni-Fe合金性能的影响[J].稀有金属,1995,19(5):357-361. 被引量:12

3刘志国,张宝生,庄育智.高比重钨合金的低温烧结[J].稀有金属,1995,19(3):168-172. 被引量:13

4范景莲,赵慕岳,徐国富.钼对钨基合金砧块性能的影响[J].粉末冶金技术,1993,11(2):119-124. 被引量:6

5马康竹,彭丹,雷正平.镍、钴协同活化钨的烧结[J]稀有金属,1987(04).

6Preston B. Kemp,Randall M. German. Mechanical properties of molybdenum alloyed liquid phase-sintered tungsten-based composites[J] 1995,Metallurgical and Materials Transactions A(8):2187~2189

1罗述东,唐新文,易健宏.添加Ta元素对钨基高密度合金性能的影响[J].粉末冶金材料科学与工程,2003,8(4):333-339. 被引量:2

2王松,谢明.高密度钨合金的研究现状与发展趋势[J].稀有金属材料与工程,2012,41(S2):145-148. 被引量:22

3张守全,黄继华,李荣华,张建纲,殷声.高NiFe比W-Ni-Fe系重合金预应变时效研究[J].材料热处理学报,2005,26(5):1-4. 被引量:1

4李小强,辛红伟,胡可,陈维平,李元元.高密度W-Ni-Fe合金的研究进展[J].材料导报,2009,23(15):66-69. 被引量:9

5冯建,张静,李邦怿,伍方,何欣,朱训奇,邵嘉骏,朱玉斌.FDM用93W-Ni-Cu/ABS复合丝材的制备及表征[J].稀有金属与硬质合金,2019,47(5):19-24. 被引量:3

6张中武,冉广,周敬恩.钨基高密度合金的研究进展[J].金属热处理,2003,28(2):9-13. 被引量:5

1黄晓云.SPS循环次数对车曲轴用86W-12.5Ni-1.2Al-5.5Fe-1.5Al2O3钨合金组织及性能的影响[J].粉末冶金工业,2020,0(1):51-55.

2刘涛,范景莲.W-Ni-Fe系钨合金的形变强化与动态力学性能研究进展[J].中国钨业,2005,20(4):18-23. 被引量:11

3左可胜,席生岐,周敬恩,刘国元,朱蕊花.铜锌粉末低温机械合金化[J].中国有色金属学报,2005,15(10):1577-1582. 被引量:2

4范景莲,祁美贵,刘涛,成会朝.细晶钨合金动态力学性能与组织结构[J].稀有金属材料与工程,2007,36(4):633-635. 被引量:10

5郎利辉,张东星,布国亮,姚松.钨基合金的预强化和后期强化技术[J].锻压技术,2012,37(4):1-7. 被引量:5

6向道平,丁雷.合金元素或氧化物强化W-Ni-Fe高密度合金的研究进展[J].中国有色金属学报,2013,23(6):1549-1559. 被引量:7

7罗来马,卢泽龙,李浩,罗广南,昝祥,吴玉程.稀土改性钨合金的研究现状与发展趋势[J].稀有金属,2013,37(6):993-1003. 被引量:17

8孙文,章晓波.高密度钨合金烧结新工艺研究现状[J].稀有金属与硬质合金,2014,42(2):36-40. 被引量:3

9齐艳飞,李运刚,田薇.合金元素对W-Ni-Fe合金性能的影响[J].材料导报,2014,28(9):79-82.

10徐芳,邹东利,何立峰,肖大武,邱志聪.W-Ni-Fe合金微观组织与冲击性能研究[J].硬质合金,2014,31(2):72-76. 被引量:1

1周国安,林国标,赖和怡,李家杰.真空热处理对95W-3.5Ni-1.5Fe高密度合金组织和性能的影响[J].金属热处理,1995,20(5):13-15. 被引量:6

2封方东.W-Ni-Fe高密度合金的力学性能与显微组织研究[J].稀有金属与硬质合金,2006,34(4):25-27.

3姚兰,常哲.钨基高密度合金热处理力学性能的研究[J].中小企业管理与科技,2013(18):230-231. 被引量:1

4金子武,吴乐贤.应变速率对W-Ni-Fe系烧结合金机械性能的影响[J].兵器材料科学与工程,1991(1):64-70.

5谢明,王松,张吉明,杨有才,陈永泰,刘满门.放电等离子烧结温度对W-30Re合金组织性能的影响[J].稀有金属材料与工程,2012,41(12):2195-2198. 被引量:1

6黄继华,曹智威,周国安,陈浩.高密度钨合金性能的计算机数值模拟研究──钨含量对合金性能的影响[J].稀有金属材料与工程,1998,27(6):344-347. 被引量:5

7常哲,姚兰.钨基高密度合金烧结力学性能的研究[J].中小企业管理与科技,2013(18):311-312.

8罗述东,易健宏,王太宏,唐新文.80W-10Ta-7Ni-3Fe高密度合金研究[J].稀有金属材料与工程,2005,34(2):226-230. 被引量:3

9王博,曹顺华,赵晶,林俊峰,韩超.梯度结构W(Mo)-Ni-Fe高密度合金的组织与结构[J].粉末冶金材料科学与工程,2011,16(2):201-205. 被引量:5

10范景莲,曲选辉,李益民,刘绍军,黄伯云.高能球磨钨基高密度合金超细粉末的烧结[J].中南工业大学学报,1998,29(5):450-453. 被引量:22

Basic Information:

DOI:

Chinese Library Classification Number:TG139[一般工业技术—材料科学与工程]

Citation Information:

High density alloy used as penetrater is an attracting topic. In this paper, the latest development and research on this kind of enhancing alloy are reviewed in respect of properties,low temperature sintering by lowering temperature, and near net shape, and some problems arealso pointed out.

quote

GB/T 7714-2015 [1] FAN Jing-lian, HUANG Bo-yun, QU Xuan-hui, et al. Research and Development of High-density W-Ni-Fe Alloy[J]. Rare Metals and Cemented Carbides, 1998(4): 47-51.
MLA [1] FAN Jing-lian, et al., "Research and Development of High-density W-Ni-Fe Alloy." Rare Metals and Cemented Carbides, no. 4, 1998, pp. 47-51.
APA [1] FAN Jing-lian, HUANG Bo-yun, QU Xuan-hui, & LI Yi-min. (1998). Research and Development of High-density W-Ni-Fe Alloy. Rare Metals and Cemented Carbides(4), 47-51.
IEEE [1] FAN Jing-lian, HUANG Bo-yun, QU Xuan-hui, and LI Yi-min, "Research and Development of High-density W-Ni-Fe Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 47-51, 1998. keywords: {high density alloy,research,development}